nailing 1 3/8 Jatoba flooring directly to joists

10/26/15       
bruce long Member

building my home in the US Virgin Islands. We've milled Jatoba flooring (1 3/8"x4" & 6") which we'll install over 4x10 Andiroba mahogany joists, no subfloor as the joists & underside are visible beneath in the bedrooms.
Any experience/recommendations for what flooring nailer to use for this species & thickness? As we are preparing all materials here in my Granada, Nicaragua shop we could consider pre boring holes for screws & shipping up a zillion pre cut bungs. Looking for suggestions.

10/30/15       #2: nailing 1 3/8 Jatoba flooring direc ...
gary

Hi Bruce,
Is the material tongue and groove or just butt joint ?

10/30/15       #4: nailing 1 3/8 Jatoba flooring direc ...
bruce long Member

t&g. Best suggestion received so far is to pre bore through tongue then use SS trim screws. Unless I see a better method, think this will be my route. 3M 5200 on top of 4x10 joists to assure adhesion & to reduce noise.

10/30/15       #5: nailing 1 3/8 Jatoba flooring direc ...
gary

I would lean towards a normal head screw for more holding power. 5200 is amazing stuff and also quite expensive in Calif. I have used Sika 1A with same results for half the price. Would love to see some photos of your shop and house; sounds great.

10/31/15       #6: nailing 1 3/8 Jatoba flooring direc ...
Gene Wengert - Wood Doc

No question that pre-boring is essential for jatoba wood. It is very dense and will either bend the fasteners or split if you do not pre-bore, or the fastener will break.

The hole, however, should not just be a vertical hole, but needs to slant inward so that the the screw holds through the tongue and through the bottom of the piece. The hole must be large enough at this point as the strength is based on the head that is in the tongue (actually the screw is at the tongue joint with the main piece of flooring and not really "in the tongue") and the screw that is in the andiroba. You do not want any resistance in the jatoba...if there is, then you will not have the floor held tightly against the andiroba and so it will squeak.

You do not need to pre-bore the andiroba.

No question that screws are "better" than nails, but installation is intensive. If you opt for nails, which is what most floors use, a power nailer is essential and then you need to inspect each nail to make sure it penetrated far enough so the head is not sticking out. Of course, nails also should not penetrate too deeply either. It is likely that nails also must be purebred or else you will get some humps in the finished floor where the nail wedged the wood apart.

A special note...the dust from sawing the ends of the flooring off and the dust from pre-boring needs to be captured and removed from the dwelling as this species does have allergy issues, especially from the dust. You do not want the dust floating around, getting into the bedrooms, etc., or getting into the air while installing the floor.

10/31/15       #7: nailing 1 3/8 Jatoba flooring direc ...
Bruce long Member

Thank you Gene. Had already made the decision to go with screws into pre bored holes. Your advice coincided with how we'd decided to work & again, thank you. We've nailed with 16 gauge nail guns about 1500 sq ft of Jatoba flooring in my home here in Nicaragua with fair to good success. About 10% of the nails needed to be set with a punch, which obviously slows down the installation. But that was all 7/8" flooring not the 1 3/8" that is for this next project.
Regarding Jatoba dust & irritation from it, we've encountered no issues with myself or our workers. However Ipe & Cocobolo Rosewood are another issue, especially Ipe. My best craftsman, & shop foreman, has severe skin reaction to it, whether from dust or just touching the surface of a board. Has to leave shop when milling it. Cocobolo is more of a respiratory issue & one we pay attention to.

11/12/15       #8: nailing 1 3/8 Jatoba flooring direc ...
Jay

my Bostotch flooring nailer drives 'em home through "Brazilian Cherry" tongues as does my Paslode15ga DA nailer. But as they say: "YMMV"

now 5200 is amazing stuff, but gluing flooring to joists is not always a good idea... Id investigate carefully before proceeding with that.
have you considered half lap joints? for the situation youre describing, half-lap (as opposed to T&G) might be a better choice.

Sounds like you're "living the dresm"! Good for you! & best wishes on your project
btw, Waterlox creates a STELLAR finish on Jatoba (actually, I haven't come across a species that doesn't turn out splendidly, with the stuff, and the application is as simple & foolproof as it gets. try a test panel on your flooring, & I'll bet you'll never look back ;)
I'm fab'ing some more wood countertop samples the 1st of next week, & a 8/4 Jatoba (with 14mm Festool Domino joinery) -Im sitting on a rough 7ft "slab" of the stuff as I type this!
Its finish will be Waterlox Original on one side & one edge/end, and SW F3 Kemvar on the opposite (side, edge & end)
if you'd like to see finish process pics, just lmk,

no doubt Jatoba is quite hard -but not THAT hard.. if you run up the pressure & dial in your gun, you'll be properly setting your fasteners.
EB-Tie (EB-Tye?) biscuits can be used on flooring (with a slight modification). Id probably use one (with a SS trim screw ) every 3rd or 4th joist & nail the rest


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory