Strippable booth coating, over already-nasty booth walls -- 2 -- 
10/18

Hey guys, our shop never has bothered to use the strippable booth coatings to keep overspray to a minimum. The booth we have was bought used, and was neglected from the outset. We were told that the overspray already on it would make it nearly impossible to strip off the waxy coating.
I'm sorta curious though, there has to be a way other than a full 100% chemical strip, that we can surface these walls and make for a strippable surface. Some sort of glossy hard coating like an epoxy.
Thoughts?
10/18 #2: Strippable booth coating, over alre ...

I would think if you sanded them down really well and applied a gloss epoxy floor coating it should work. It will take a lot of time and money however. You could always do a test on piece of scrap before you dove in all the way. Maybe applying a skin of cheap metal over the existing walls with self tapping screws would be cheaper?
10/18 #3: Strippable booth coating, over alre ...

Would formica be cheaper skin than sheet metal? I'm also thinking about how razor sharp the edge of sheet metal is (meaning that you should dress the exposed edges just so no one slices themselves should they walk into it or grip it the wrong way.
10/19 #4: Strippable booth coating, over alre ...

Rick Mosher, I can always count on a good response from you, thanks! We did think about veneering it with some sheetmetal, it's on our list of options. Not being a sheetmetal guy, I'm not sure what I'd buy, or where to get it, or what's a reasonable cost. But that's something we can find out.
Dan Shafner, I had not thought about using formica, that's probably a great idea. I'd just need to buy a gallon of the coating and spray it on some P-lam and see how easily it peels.
I know that I can buy sheet aluminum from one of my P-lam vendors, it's a popular veneer in this area for accents here-n-there. I think I even have a spare roll of it over in our offcut purgatory.
10/19 #5: Strippable booth coating, over alre ...

Matt,
I would think adding a layer of metal liner panel (similar to corrugated roof panel but cheaper) would be an easy fix. It has a smooth painted surface, comes in 3' widths, and can be ordered cut to exact lengths. It's available through big box stores or lumberyards and is pretty cheap, much cheaper than plam. I have it in my shop for ceilings and plan on using it in my new spray room for walls and ceilings.
Fabral is one brand. It screws on with hex head screws or could be drilled and riveted if you wanted a smoother face. Hard to beat the price.
10/19 #6: Strippable booth coating, over alre ...

When our booth was new, the first thing we did was spray several coats of the strippable coating all over it. In time, it would start to flake and big chunks would come off. We were not happy. May have just been the particular brand we used, but we dont use it any more. Now, we simply just broom the walls as we sweep out the booth and periodically scrape with a putty knife.
10/19 #7: Strippable booth coating, over alre ...

JM, that's basically what we do, but our booth is smaller than most shops of our volume, because of various constraints. If we were fortunate enough to have the larger 20ft wide booths, this wouldn't be nearly the issue.
I do appreciate you sharing your experience though, thanks!
10/19 #8: Strippable booth coating, over alre ...

Another option would be to deftly sand blast the walls using a medium such as crushed Walnut shells. Once your down to the a bare and clean surface, the Binks booth coating is a good product. Comes in a clear or a White. Can be brushed/rolled.
As with any coating your applying , the prep work is the most important step.
10/19 #9: Strippable booth coating, over alre ...

we use Sherwin Williams strippable booth coating and peel down the walls once a year and the celings once every 2 - 3 years... the trick is once you have a clean surface to work with is to degrease them and then spray the coating in multiple passes up to the correct thickness.... if you don't get it thick enough it makes it ten times harder to peel off cleanly without tearing constantly... We typically use about 10-15 gallons per 20ft wide 12 ft. high 10 ft. deep booths we have....
10/20 #10: Strippable booth coating, over alre ...

I believe galvanized steel sheet should be available locally and not too expensive. We used to make the tops of our mixing tables out of it. It cleans up really easy.
10/21 #11: Strippable booth coating, over alre ...

this is how we get that stuff off the walls
View larger image
1/4 #12: Strippable booth coating, over alre ...

This response may be too late but might help someone else in the future.
I am just putting up a used booth and I removed some of the overspray with a pressure washer. You probably can't do that if the booth is already up in your shop. The remainder of paint will come off pretty easily with a blow torch, heat gun, or one of those radiant heat devices people use on houses and furniture. use a 6" drywall knife or one of those wide scrapers with a disposable blade from the paint store.
Once clean, put adequate booth coat on so it will hang together when you peel it in the future.
2 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|