Very hard to find Joos DLP 135 5' x 10' End-Loading Feed-Through Hot Press. PLUS we installed NEW UPPER and LOWER Elkom Okotherm Plus Platens + Insulation Panels with an installed cost of $30,000. Yes, it has never used NEW platens! Pneumatic pop up cross rollers on outfeed. Safety fence included per pictures (under infeed).
Pressing Surface: 1600 x 3150mm (63" x 124")
Height of Pressing Area: 200mm (7.87")
Six Pressing Cylinders
90mm Diameter Cylinders
NEW Elkom Okotherm Plus Platens + Insulation Panels
Twin Tool-Temp Heating Units
Infeed belt conveyor is 130" long by 63" wide
Outfeed roller table is 128" long by 66" wide
This fully functional machine has been fully cleaned, checked, and is ready to work from the time you receive it. This is our guarantee to both you and your company. It is owned by 360 Degree Machinery and located in our inventory in Kingston, TN.
Link to more images and info at 360