Titebond on teak siding

12/15/21       
Kim Thich Member

I am managing a job on Kauai where we are installing teak siding . The siding is 9/16” x 5” face t&g from Indoteak. It is an engineered product that uses solid teak as the crossband sub layers. It is prefinished with Rubio monocoat on the face and back sealed with a water base sealer . It is going on top of sheathing that has 3/16” furring strips every 8”.
We are mitering corners and miter returning into window and door jambs. We have a floating 1/8” spline in jamb edges to connect to slotted mitered returns that are 3/4” to 1-1/2” wide.
We are using West System, fast cure with microfiber. We are wiping glue surfaces with Acetone prior to gluing. We are blue taping glued miters and also pin tacking with 23g ss headless pin nails.
We are removing blue tape on miters within 1 hour to wipe off any glue residue with acetone and changing to clean rags frequently.

WONDERING IF WE CAN USE TITEBOND III instead of epoxy. Concidering all install location factors like: 9’ tall walls, deep overhangs, weather that can be sweltering hot to windy/wet and any factors above. West System is bomb proof but it is so time consuming and we need to be careful with not getting glue residue on exposed surfaces.
If we went with TBIII we would still wipe glue surfaces with acetone.
Like to get some solid feedback.


View higher quality, full size image (4032 X 3024)


View higher quality, full size image (4032 X 3024)


View higher quality, full size image (4032 X 3024)

12/15/21       #2: Titebond on teak siding ...
Matt Calnen

I too love the West System 105 epoxy. As a Michigander, it’s better brand than a Ford anyday. I have been using the G5, which is their 5 minute epoxy. Don’t be fooled by the 5 minute label, it’s strong $hit. In reading the literature on the product, it may not fair well in overly wet environments. Not sure how much moisture your joints will see, but titty bond 3 never impressed me in an application that needed strong holding power. I believe another woodweber states that it loses substantial strength after it gets above 130 degrees. My front door, which is a mahogany, gets very hot on the outside during the late afternoon when it get full exposure the sun. Never would have thought it would get as hot as it does, and I’m in northern Michigan. Good thing I used the 105 west system.

12/16/21       #3: Titebond on teak siding ...
Tom Gardiner

David Sochar has commented that TB III adhesion strength degrades with heat. Another problem that I have seen is PVA will swell when coated with oil finish. You end up with a small ridge at the glue line. I am not sure if that would happen with Rubio but it does with tung oil and other true oils.
Could you make test joints and run them through cycles of heat and wet?

12/16/21       #4: Titebond on teak siding ...
David R Sochar Member

Website: https://www.acornwoodworks.com

What I learned about TBIII is that is loses its strength - its grip - as temperatures increase. At 180 degrees, it loses about half it strength. We have had very dark doors register a surface temp of 200 degrees just from solar exposure. We had about 12 projects out in the world with panels glued for width that came apart or threatened same.

If you wish to use TBIII, I would call the tech department at Franklin glue and use the temps you think this siding may experience. They were very candid with me.

As for using the epoxy, I once had a boss that would at the precise moment say "This is why we call it work, and this is why we pay you to do it!" I have been known to repeat that rough bit of managerial wisdom. I think I'd stick with the epoxy.

12/16/21       #5: Titebond on teak siding ...
Kim Thich Member

Yes, it’s is work. I don’t want any call backs ,so probably staying with epoxy.

12/25/21       #6: Titebond on teak siding ...
Adam

You are doing everything as good as it can be done. Why do you want to switch to TB3. Epoxy is the standard for glueing teak. Over the decades we settled on TB1 for interior and epoxy for exterior. Every other product that's exterior rated negatives.

There are usually 3 reasons why people don't use/like epoxy. Cost, lack of experience, time to mix/waste.

The wood cost alone means that cost should not be an issue. You've got the experience and time to mix is irrelevant in almost every project.

You can improve your epoxy usage by using vinegar for general cleanup. Iso alcohol(rubbing) is the best solvent for epoxy. Not denatured alcohol or acetone.

I would encourage you to try MAS epoxy. They have a product called FLAG resin. It's thick enough that you don't have to thicken it for woodworking. It's also a modern 2:1 non-blushing system that doesn't cause contamination issues.

West System is good stuff(I've used 100's of gallons) but the viscosity is always a problem. 5:1 mixing is a bit annoying as well. It's available everywhere so that's a plus.

12/25/21       #7: Titebond on teak siding ...
Kim Thich Member

Yes, We are sticking with epoxy . Just thought to ask if there were other options.
We had a learning curve at the start . Guys were not careful with epoxy residue from joints and handling material . So they have to use fine wire brush to rid epoxy from miter joints and surface areas. I will try the green scotch brite attachments for dremel drill.
I will use iso alcohol , acetone is what we been using.

12/27/21       #8: Titebond on teak siding ...
Fred Frehner

Website: http://www.rivercity.ca

Hi Kim,

We started to use a product by Loctite.https://www.richelieu.com/ca/en/category/glues-silicones-and-caulking/cons
truction-glues-and-adhesives/polyurethane-glues/loctite-glue-ur-series/1209594
Mostly on exterior door components and arch laminations including Accoya, so far we have no failures. The attached web page does not list, but it but it is available in 5 gal, with 60 and 70 min. open times.
Its messy to work with and hard to clean. It stands up to heat well and is water proof.
Not sure if it is better than the west system epoxy. One plus is you don't have to mix it.

12/27/21       #9: Titebond on teak siding ...
Fred Frehner

https://www.richelieu.com/documents/docsGr/120/959/4/1209594/1466670.pd
Not sure if the link works in the original email. hope this works better.

1/23/22       #10: Titebond on teak siding ...
Kevin Dunphy

Website: http://www.kdunphy.com/

TITEBOND III seen it first hand it gets soft in the heat.

In the second picture, those are all miters? did you biscuit or spline that looks like something that could open up

Those small mitres wouldn't take much to hold the mitres. I used one years ago a two gun cartridge with no mixing especially on site

Expoxy is epoxy you are well covered no much pounding rain.

Just curious do you put a clear coat after and do you caulk the seams

https://www.amazon.ca/Manual-Epoxy-Applicator-Gun-6-75/dp/B07Q8FVTXZ?th=1

2/6/22       #11: Titebond on teak siding ...
Kevin Dunphy

Website: http://www.kdunphy.com/

Curious why you don't answer the question I asked

2/6/22       #12: Titebond on teak siding ...
Kim Thich Member

Kevin,
We are staying the course with west system epoxy. All siding is prefinished with Rubio Monocoat from supplier. We backsealed with water based sealer from HD. All walls are furred out 3/16” every 8” for airflow . T&G is glued in with Titebond 3 ( probably switch over to water based clear caulking ) epoxied miters at corners and short returns to doors/windows are pinned with 23g ss to hold position . Stretched blue tape is used as ‘clamp’ at miters.
The most important part through out is wiping, wiping , wiping ….all epoxy residue on visible surfaces with acetone as solvent. Always using clean rags , otherwise dissolved epoxy residue gets spread around more.
No need for mechanical joints like splines etc at miters , boards are nailed off to wall in close proximity to glued miters. We are busting original budget for siding , but I convinced client how it will look awesome when entire house is sided… added another 100k plus . Don’t need to sweat it out so much now. Apologies for not replying ,hope this suffices.

2/6/22       #13: Titebond on teak siding ...
Kim Thich Member

Also, we will soften sharp miters and tough up with more Rubio Monocoat

2/8/22       #14: Titebond on teak siding ...
Kevin Dunphy

Website: http://www.kdunphy.com/

Thanks for the update, looks easy at first glance it looks easy but it's tricky.It looks, killer


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)