Modern "flush" door construction

12/6/22       
Jack Member

First time posing here. I am used to building historically appropriate rail and stile entry doors. That is my bread and butter... but more recently I have had inquiries on more modern designs, which more or less require vac-press lay ups on exterior grade sheet substrates. I am thinking either extira or marine grade fir with the edges and ends capped in hardwood before the lamination.
One that I am going to do involves a sort of "ship-lap" look to it on each face. I plan on laminating 3/8 thick hardwood (white oak) to each face with west system epoxy in my vac-press, widebelt sanding the face flat, then routing the 3/16 deep grooves into the face at the joints to create the ship-lap look. Has anyone had any experience on this type of door construction? Will there be problems with the boards splitting since it wont be allowed to float like it would in a rail and stile door?
It will essentially be like a piece of veneered plywood, but the veneers are 3/8 thick... instincts tell me that may be a problem. I know big-time door manufacturers do this with some of their engineered raised panels where the "cores" are 1/2" mdf with 3/8"+ solid wood material laminated on each face... open to tips and suggestions. Thanks!


View higher quality, full size image (540 X 676)

12/6/22       #3: Modern "flush" door const ...
Mark B

Me thinks your 3/8" skins will get some pushback.

12/6/22       #4: Modern "flush" door const ...
Tom Gardiner

Yup, not loving the 3/8" skins. Look for 1/16" veneer from certainlywood.com or other suppliers. The sequence match of the thinner veneer will be better, the quality of the wood tends to be superior with veneer and you won't have the stress issues.

12/7/22       #5: Modern "flush" door const ...
RichC

You could have a chance if you use quarter sawn white oak, but it goes against a law of nature of gluing hardwood to mdf. I"m no fan of mdf anywhere in an exterior door. Get water in around the lockset, or the bottom of the door and you are in for a call back. What is your experience with exterior mdf usage? What is the success rate of those "big time" manufacturers? Just doing it doesn't count unless you know how long it lasts!

12/7/22       #7: Modern "flush" door const ...
Jack Member

Tom,
Yes I agree with the 1/16" veneers. I resaw them myself for all of my stave core stiles for my rail and stile doors. The issue is that the design calls for grooves to be routed into the face of the door. I would route right through the veneers into the substrate... that wouldn't be a great look.

Rich
The specs call for flatsawn... as far as exterior mdf, it seems to hold up very well and obviously much more stable than solid wood or even plywood. I soaked a raw piece in a 5 gal bucket of water for 3 months and measured absolutely zero change in edge thickness, i.e. zero swelling due to moisture... It definitely has applications where I wouldnt use it, like in cases were screw retention is needed. But it seems to be a great product.

Anyone on here that has real world experience building these particular styles of doors that can weigh in? Any advice would be much appreciated.

12/7/22       #8: Modern "flush" door const ...
Tom Gardiner

You could prepare your core with routed grooves filled with solid oak. Veneer then rout through into the oak filled grooves.

12/7/22       #9: Modern "flush" door const ...
aj

You may consider inletting small strips of oak into the substrate so you can route "through" the face veneer essentially breaking them up from pushing on the next piece, yes it's a pain. Even at that I wouldn't exceed 1/8" in thickness for the faces.

Another work around is instead of a v-groove a narrow 1/8" square groove that is straight into the substrate but looks more like a shadow line and would be impossible to see what the core is. Key once again it is breaking up that solid wood from pushing on the next piece.

You would have to do something similar for veneer I'm guessing.

12/8/22       #10: Modern "flush" door const ...
Fred Frehner Member

Website: http://www.rivercity.ca

Hi Jack,
We have build doors like this by routing and inserting solid strips into the core first. We then glued boards to the surface. It is essential to give booth sides of the door the same treatment. Obviously narrower board and vertical grain material are a better choice. Often we add the final vertical edge banding after the horizontals are installed mostly do to weather stripping needs. We have also build doors with added boards on the exterior only. In that case we use T & G or ship lap products ( often matching the siding)and there is no glue or grooving of the core. A lot of it really depends on the location and protection that's provided. We refuse to build doors like this for the wrong location.
Personal I prefer veneer especially if wider boards are requested.

12/8/22       #11: Modern "flush" door const ...
Mark B

What is your approach to weather sealing the horizontal gaps in the door face in the exterior?

12/8/22       #12: Modern "flush" door const ...
Fred Frehner

Hi Mark,
It depend on type of gap we have need. We do prefer to prefinished the inset if we can. That way if we have a bit of movement with the seasons it does not show. Sometimes we have metal insets in the core. Attached is a picture of a door I was worried about wide 3/8 thick boards boards are overlapping the inserts. The boards are way wider than we are comfortable with and flat sawn material as well. This door was build 9 years ago and we had on problems with it.


View higher quality, full size image (3456 X 5184)

12/9/22       #13: Modern "flush" door const ...
Joe Calhoon Member

If V grooves are allowed I usually use solid wood for this type door with the cladding over a ladder frame. The walnut door is 5/8” T&G over a ladder frame both sides. Cladding is glued to the frame but they are not glued to each other so each board can move. Most of our doors are euro rebated so no issue with air leaking through the v grooves. For a conventional door I would make a small rebate around the door edges to allow the gaskets to sit to a flush surface.
The fir door in the picture is a outhouse door I built for my son’s yurt. It is one side clad over a ladder frame. No worries about air leaks on that one. It has held up well for 3 years at 11,000 feet.

I would never use MDF for a door core. I would like to try Tricoa for a moder door core but difficult to source here,


View higher quality, full size image (2266 X 3022)


View higher quality, full size image (960 X 1280)


View higher quality, full size image (1280 X 960)

12/9/22       #14: Modern "flush" door const ...
Adam

About 15 years ago I was hired to build a pair of french slab exterior doors. The builder liked to think he "knew" what he was doing. They speced a ladder frame with pink foam. 3/8" quatersawn white oak "veneer". Stained jet black on the exterior, clear on the interior. Contemporary house with (2) big 7' tall black slab doors. Not my house...

I told them that I wasn't excited about the 3/8" thickness, they thought the thicker the better. We had done 1/4" then run the doors thru the wide belt in the past. The doors were built to finish at 2 1/4" thick. Several days after layup with epoxy, the boards started to cup. There was no debonding, but you could feel the boards. We ended up grinding the doors down 1/8" per side. They ended up as 2" thick door slabs. The final thickness didn't matter as far as hinges. They were speced to have some weird ugly super expensive pivot hinges top & bot and a matching handle.

Thick "veneer" can be vary sketchy. Personally I think 3/16" is about right. Cut them 1/4" glue up your door then grind it down.
I believe the t&g doors appear fine because each board is separated. If you put a straight edge on it there will be discrepancies between each board.

12/13/22       #15: Modern "flush" door const ...
David R Sochar Member

We first build an egg crate core, then skin it both sides with 1/4" exterior rated MDF or ply. We add blocking for latches, and edge band the vertical sides.

The cedar face parts were all shiplapped, and laid with a strong 1/32" gap between pcs. The were not nailed, but glued in place. Identical on both sided. These doors were about 10' tall, and 3" thick. Hung on Tectus hinges for the bit of adjustment they provide. We aded two lines of bulb type weather strip to the vertical sides and top, with bronze interlock at the sill.


View higher quality, full size image (4032 X 2268)


View higher quality, full size image (4032 X 2268)


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)