New Startup Shop here with a Biesse 5x12 Rover K and Holzher 1057 XL C Bander .

We are having the new edge bander installed this week and it currently without the nesting shoe .

My initial thought was to have the CNC take care of all the boring and Drilling, but didn't realize that presents a problem for the bander.

Im torn on the decision to have the nesting shoe installed or not. I hear without the shoe, i should have better edge finishes.

I currently do not have any setup for hinge drilling at the moment other than a hinge jig.

What are you guys doing and opinions on it?

8/25/22       #2: Drill for Hinges on CNC / Edgebande ...
Mark

Rich,
Seriously, buy and install the shoe. Likely around a grand? No separate op on the press, or for that matter no press at all, switch at will between Blum, Grass and Salice, etc (but definitely stick with Blum) and switch to the inserta hinge, short money for the better, quicker more versatile job.
I generally pocket the large cups with a router bit, but some have had success with a 35 mm brad point in the drill bank, or so I have heard.
I run a Biesse edgebander with perfect results over the hinge cups, with the appropriate bridging device, slightly different than the HolzHer setup but no matter No edge quality issues at all.

8/26/22       #3: Drill for Hinges on CNC / Edgebande ...
Derrek

Website: http://www .closetdr.com

We had this issue previously. We cut mdf plugs that fit in hinge hole to keep copy wheel running smooth. I believe Fastcap has a product for this as well that is adjustable

8/26/22       #4: Drill for Hinges on CNC / Edgebande ...
Dropout Member

Something new everyday.

I have 4 CNC,s 2 of them Biesse, and have no idea what a nesting shoe is.

Anyone?

8/26/22       #5: Drill for Hinges on CNC / Edgebande ...
Derrek

Each trimmer usually has a large copy wheel that rides on the panel and you adjust trimmer to it. When u have an imperfection on panel wheel will raise up or in case of hinge hole drop into hole and trim to much. To solve this they make a long shoe that slides on panel or like on my Vantedge has multiple copy wheels so the trimmer stays flush with panel in the area of hinge hole.
See attached photo of my glue scraper it has 3 rollers only pic I had on phone

8/26/22       #6: Drill for Hinges on CNC / Edgebande ...
Dropout Member

Thanks.

8/27/22       #7: Drill for Hinges on CNC / Edgebande ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

I do what Derrek does, I just made a pile of plugs .5mm smaller than the cup size and made them the depth of the cup cut.

I use a 35mm bit in the drill block. 8mm for the pin holes. Seems easier/faster than a pocket operation to me.

8/28/22       #8: Drill for Hinges on CNC / Edgebande ...
Quicktrim

Same as Karl here, holzher triathalon without the nested based kit.

8/29/22       #9: Drill for Hinges on CNC / Edgebande ...
Andy Officer Member

We use a 5mm drill bit to mark pilot holes on cnc, edge band and than the guys used the dimple as a center line on regular blum hinge machine. Found its much faster than trying to screw around with plugs at the edge bander.

8/30/22       #10: Drill for Hinges on CNC / Edgebande ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

I don't think the plugs slow anything down.

They get dropped and roll off sometimes, but that's why you make a ton of them.

I try and do the hinges as not the last edge. Run the hinged edge, then on my way back to the feed, I dump them out on top of the bander. Shove it through again. I'm sure it varies bander to bander, but I almost always get back to the in feed before it's ready to accept the next part.

8/30/22       #11: Drill for Hinges on CNC / Edgebande ...
Pdub Member

We used to use the puck method on our old Holzher. Recently got a new Biesse with the "shoe" and love it. The puck works, but the idea is to make it so that the puck is slightly proud of the panel in case 1 door is slightly less thick than others (material inconsistency) , it won't cut into the door. Now you have a small lip of edgebandng to sand/ scrape off.

If instead, you're going to band and then bore afterward, or if you're boring 5 piece doors, I'd suggest figuring out how to run "ops only" program with your CNC as opposed to a hinge boring machine. I suppose it depends on what software you're using.

We pocket with a 1/2" bit. If you use the drill, occasionally the "veneer" (or laminate or whatever) can break loose and spin with the bit so that it doesn't cut at all. Best case is no hole. Worst case is damaging your CNC.

8/30/22       #12: Drill for Hinges on CNC / Edgebande ...
Dropout Member

Regarding drilling the hole, we took the extra time to pocket 0.030 or so under size and use the drill bit just to clean up the hole.

8/30/22       #13: Drill for Hinges on CNC / Edgebande ...
Derrek

Website: http://www.closetsr.com

“We use a 5mm drill bit to mark pilot holes on cnc, edge band and than the guys used the dimple as a center line on regular blum hinge machine. Found its much faster than trying to screw around with plugs at the edge bander.”

I would love to see your time studies on this. I find it very hard to believe that adding an additional step, including the handling and transportation, along with the cycle time of the hing machine is faster than putting a plug in a hole and pushing through a bander?

8/30/22       #14: Drill for Hinges on CNC / Edgebande ...
Andy Officer Member

Derek,

For me personally its faster for a few reasons

We do a ton of shaker and custom doors that don't come off the cnc and therefore we already have a system in place where when you pick a up door and lay it flat to put the hinge cups on it (which you have to do either way even if you have a automatic inserter) you bore it first, put hinge cups on and put the handle on all in motion so we are really not handling it any more than we would to begin with.

Second being majority of the time we have helpers on the edge bander, and the amount of time that they would forgot to put those plugs in and burn through a door is way more expensive than boring it when you put cups and handls on.

Third we do a ton of locks, and its a complete waste of time to switch out our drill block from the lock plug to the 35mm boring plug, yet alone can't do it both at once anyway.

So that's my time study, down the road when we get a new bander will probably bore them out first but at the moment its way more effective to dimple.

8/31/22       #16: Drill for Hinges on CNC / Edgebande ...
Rich Member

Do you guys have a picture of this plug? Does it need to be tight? or Can it be loose?

8/31/22       #17: Drill for Hinges on CNC / Edgebande ...
Derrek

No they don’t have to fit tight 33mm is good
See video of mine 10 years ago

Edgebander plugs

9/2/22       #18: Drill for Hinges on CNC / Edgebande ...
D Conti

I guess I am just old school. I bore and install my hinges on a hinge machine after the door is banded. We don't use inserta hinges just plain old hinges with dowels. I have the software set up to cut a hinge 4" on center from the top and bottom of each door. The hinge plate is cut into the cabinet side accordingly. On large doors with a third hinge it is in the center of the door. Four hinges do become an issue and you have to check the box (hinge plate for location) but we do so few of these that it is not a problem. The only issue we ever have is on ADA sink bases were the hinge is 8" from the top to allow for a 4" skirt board. We have aux stop set there and you must make left and rights. This way if we make 5 piece doors they get bored the same way and if there are MDF doors we do not have to do a flip side to the door. I have been doing this for years without any issues. I think that pressing in a hinge with dowels is about as quick as you are going to get, plus if there is any sort of imperfection in the banding we can always put it on the side that will not be seen. This also eliminates the need for plugs or speciality shoes. This just works for me, and I have been around awhile and am pretty set in my ways. I am sure that the plugs and /or shoe work just fine it is all just another way to skin a cat. I am also not a big fan of inserta hinges and their extra cost.

9/21/22       #20: Drill for Hinges on CNC / Edgebande ...
Rich Member

We have the nesting shoe , but not installed . I can have it installed at part of sales agreement if I wanted it .

We made some 33mm plugs on the cnc and dropped them in . Ran a door through the bander . The dust collector sucked the plug up and we damaged a door from that ran .

We tried another door but this time put blue tape over the plug . Seems to work fine after that .

Is this normal ? Are you guys taping your plugs down ?

9/23/22       #21: Drill for Hinges on CNC / Edgebande ...
Karl E Brogger  Member

Website: http://www.sogncabinets.com

I don't tape them. Try making them a little more snug. Not tight enough they friction fit, add don't fall out, but tighter than you've got them? I'm pretty sure I made mine 34˝ mm, but I'd have to measure one to be sure

And I'm jealous your dust collection is good enough to suck them up.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)