I'm thinking of making a 4 x 8 foot dining room table top by gluing together two 9/16" thick layers of solid walnut with a 1/16" cross-grain walnut veneer in between the two 9/16" layers and then putting it in a vacuum bag. By doing this I would hope to minimize or eliminate seasonal expansion and contraction. Has anyone tried this? Is it a good/bad idea?

10/10/22       #2: Laminating a table top ...
Tom Gardiner

I don't think you will find someone who has done this, but who knows? How much stress will be in the table top will depend on the annual RH swings in its location. If this is for a client, I would not do it. Too much risk with an unknown procedure. If it is for yourself, go for it and tell us how it works after a year or two.
I would choose epoxy for this layup or another adhesive with little or no moisture otherwise you will be fighting with curling layers during roll out. I would consider a five ply glue-up instead by adding 1/32" or 1/16' veneers to the top or bottom and having the thick layers as the cross grain. This will balance the glue line stresses to both sides of the thick layers.
As a last thought, this is a lot of added work over a single solid layer of 1 1/8" walnut or a core and veneer. Is the extra effort and risk necessary to the outcome?

10/10/22       #3: Laminating a table top ...
RichC

You will never prevent seasonable movement with wood that is 9/16" thick. My feeling is that the inner veneer layer will be split into pieces when the thick wood expands. 4' is a very wide table and difficult to pass food across. I'd forget the lamination and use quarter sawn walnut that is milled to the thickness you want. It's been done for centuries, no need to feel like solid wood will never behave all of a sudden.

10/11/22       #4: Laminating a table top ...
David R Sochar Member

I disagree with Rich. We regularly make 7 ply panels with two solid layers 5/8" thick. This is done mostly in Mahogany or White Oak. 7 years and no problems yet. Many of these panels replaced solid wood panels made with Titebond III that came apart with exposure to heat - normal environmental conditions.

We have 7 ply samples laying in the downspouts that have been there for 8 years, and they are a little rugged, but are as tight as can be. Each layer is intact, and the layers have not peeled or buckled.

Now, these are door panels, so the perimeter is retained in the frame and movement of about any kind is limited. But the 7 ply system works wonderfully.

I can see it would work well as a table top. In general, the more plies the more stable.

10/24/22       #5: Laminating a table top ...
Dave Edgerton

Bad idea. That table will expolode or warp to heck.
Use solid wood.

10/24/22       #6: Laminating a table top ...
Dave Edgerton

Bad idea. That table will expolode or warp to heck.
Use solid wood.
Sounds like a make work project.

10/24/22       #7: Laminating a table top ...
RichC

Aren't you comparing apples to oranges David? I agree that 7 ply will react much differently than 3 ply.

10/24/22       #8: Laminating a table top ...
David R Sochar Member

Apples and Oranges go together in the nice turned bowl in the center of the table. But seriously.....

Yes, the more plies, the better stability. A 3 ply with 2 - 9/16" thick layers would be pretty dicey. No telling how it would come out. I would do the top as a solid wood table, as long as I knew the lumber and who and how it was dried. Any insecurity, I would go for 7 ply, and the sure thing.

The reason we developed 7 ply panels for our doors was the "Sure Thing". We had to avoid any problems with panels, and we could not do so even with the great wood we buy.

The OP says he wants to do the lamination to minimize or eliminate seasonal expansion and contraction. A reasonable response to a reasonable design issue. But, I would either choose solid wood carefully, or a 7 ply lamination. And yes, that 7-ply lamination would be monster to get into a vacuum bag.


View higher quality, full size image (4000 X 3000)

10/27/22       #9: Laminating a table top ...
John Member

Why has no one mentioned a standard veneer over plywood or MDF approach? Take your wood and slice it into 1/16 to 1/8" veneer. Seam it and glue it to the substrate with UF glue. This is a system with decades of history, all good.

John

12/24/22       #11: Laminating a table top ...
Cherry GTree  Member

Website: https://cherrytreedepot.com/

I think using Solid wood will make your table strong and it also provides good finishing.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)