Company Name: specialty designthe island and all the trim were built from solid white oak in my shop as well as the columns(which each weighed in at 35 pounds)the only ply is in the drawers which are finger joined 3/4 oak. the top is a crystal finished lam. with our custom oak trim. this is one of many pieces to this kitchen.