Olive ash burl ent. ctr.

Listing #135 Listed on: 07/07/2004 Name: Joe LaRock

Company Name: Joseph LaRock & Co. Inc.This ent. ctr is primarily olive ash burl. It has african ribbon stripe "corners" and canopy. The curved decorative pieces are zebrawood. Unit has 3 concave surfaces and one flat which is a pullout cd/dvd storage.
speakercloth covers on the speaker openings and
"smoked"glass on the component compartments.
hidden touchswitch for halogens on backside of z-wood.

(No images available for this project.)
0 Photos
Social Media:
Viewer Comments:
Posted By:Curtis

That is one Bad A$$ entertainment center!! Looks great and very time consuming. I am curious on what you made and sold it for.
Curtis

Posted By:M&M

Joe do you do your designs in house or is it from outside designers? Either way beautiful design and execution.

Posted By:Joe LaRock

Thank you both for your kind words. I did not design the piece myself. A friend of mine and former furniture maker who lives close by did by the name of Roy Allen.

Joe LaRock