Company Name: PhitrabaCherry canopy bed.
Construction notes:
Pierced carving floats in headboard.
End rails and side rails are of torsion box design, giving a 6/4 look, with similar stiffness, but half the weight.
Style leans on 19th century Dutch, French and English influence.