2010 Clock Commission

Listing #3399 Listed on: 07/29/2011 Company Name: Edward Jorgensen, Master Cabinetmaker
Name: Edward Jorgensen Member

This clock case was fitted with a huge custom made clock movement and sent to India.

1 Photos
Social Media:
Viewer Comments:
Posted By:steve
For the Taj Mahal?
Posted By:Ed
No actually it was bought by an individual.
Posted By:Anthony
That's a beautiful case. I like the mirror finish. What kind of wood is that? Is it veneer, or solid?
Posted By:Ed
Crotch Mahogony veneer on solid mahogony body
there is black ebony inlay where you see the black lines. The molding was gold leafed by people in Santa Barbara. Then we did a varnish finish.
Posted By:Howard
Wow that's really amazing!