Listing #5185 Listed on: 06/24/2020 Name: Dennis Fell

with almost 10 years experience in cabinetry, i was given the opportunity to fabricate a solid krion vanity for a NYC apartment. I bent all the krion using heat and male and female templates. solid legs were laminated together using 14 pieces of 1/2" krion. I hope you enjoy the work

4 Photos
Social Media:
Viewer Comments:
Posted By:Dave Sochar
What is Krion?
Posted By:Dennis Fell
It’s a solid surface material made by porcelanosa. It’s very similar to corian made by DuPont
Posted By:JK Interior Finish Inc.
I work with Krion a lot , but mostly jsut countertops so I can appreciate the work that went into this. Well done and well excecuted.