All Listings
Gallery Guidelines
Hydraulic laminating press
Listing #202 Listed on: 03/07/2020

Company Name: Go-Tools

Contact Name: Gabe O
|
Hydraulic press built from four 20 ton harbor freight press frames. The manual jacks are replaced with air actuated jacks. A 5x22 gluelam for the bottom platen. Two separate top platen. 22”x11’x3’ capacity. The jacks don’t bleed off and loose pressure if the bleed valves are tight
(No images available for this Shopbuilt Equipment listing.)
|
|
|
|
Viewer Comments:
Posted By:
ALEX J Gonzalez [11/08/2020]
Interesting, ive been wanting to make a press for some time now. Are you blowing air into the hydraulic cylinder?
Posted By:
Gabe O [11/09/2020]
Alex, yes they are air over hydraulic jacks. Also I added a automotive jack to the bottom to raise and lower the bottom platen.
Posted By:
Al [01/28/2021]
Nice press. Do the springs pull up the top platen? Also when using air jacks, do they receive air all at once? If so you must have 4 port air manifold. Thanks, Al3924
|
|