Question
Does anyone have info regarding the decay resistance qualities or other pros and cons of European larch (Larix decidua)?

Forum Responses
(Sawing and Drying Forum)
From Professor Gene Wengert, forum technical advisor:
The heartwood of this species has very high natural resistance to decay.



From the original questioner:
Very encouraging since I'm buying 20-30 mbf from a plantation in Woodstock, VT.


From Professor Gene Wengert, forum technical advisor:
Plantations tend to have more sapwood, so be careful. Is the plantation in VT? It is interesting that they would choose this non-native species. I wonder why.


From the original questioner:
The sapwood ranges from 1/2 to 1" generally. The plantation is on land that is now the Marsh-Billings-Rockefeller National Historical Park. Frank Billings chose larch as well as several other species after a trip to Europe in the early 1880's. He was interested in forest stewardship and replanting the Vermont countryside after devastating clear-cutting for sheep farming left the landscape barren.


From contributor K:
I live in the UK. We use larch for fencing posts. A 4x4 will last 20 years untreated. Also good for exterior cladding. It is regarded as good timber in the trade and fetches good money in the round.


From the original questioner:
Very helpful. I'm planning to use it for porch decking and clapboards. It air dries incredibly fast. After 2 weeks on sticks its reading 12-14 %!

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Forestry

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Air Drying Lumber

  • KnowledgeBase: Primary Processing: Sawmilling


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2021 - Woodweb.com
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review Woodweb.com's Copyright Policy.

    The editors, writers, and staff at Woodweb.com try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at Woodweb.com after considerate evaluation, and at their own risk.

    Woodweb.com
    865 Troxel Road
    Lansdale, PA 19446

    Contact Us











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article