Circular Sawmills - and Their Efficient Operation

      A primer from the USDA Forest Service. February 16, 2004

by Stanford J. Lunstrum
US Department of Agriculture
Forest Service
State & Private Forestry

This manual was written for circular sawmill operators who recognize the need for producing the maximum yield of well manufactured lumber in the shortest possible time.. It does not attempt to cover all aspects of sawmill operation; it is concerned only with the first and most important step - primary sawing - and all the mechanical components that affect the primary sawing function.

To view the file, left click the link below. To download the file, right click and choose "save target as". The document is in Acrobat PDF format. Download latest Acrobat Reader if required.

Circular Sawmills and Their Efficient Operation (PDF 1.73 MB)



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Forestry

  • KnowledgeBase: Forestry: Timber Harvesting

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Sawmilling


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2021 - Woodweb.com
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review Woodweb.com's Copyright Policy.

    The editors, writers, and staff at Woodweb.com try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at Woodweb.com after considerate evaluation, and at their own risk.

    Woodweb.com
    865 Troxel Road
    Lansdale, PA 19446

    Contact Us











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article