Should whole-tree chips for fuel be dried before storage?

      Whole-tree chips deteriorate more rapidly than do clean, debarked chips and present a greater hazard for spontaneous ignition when stored in outdoor piles. To prevent ignition, the chips can be stored for only short periods of time and the frequent rotation of the storage piles results in high handling costs. Drying the chips prior to storage will prevent deterioration and heating, provided the chips are stored under cover. In many cases, the costs of drying can be recovered when the chips are burned for fuel. In these instances, drying and covered storage is the least expensive method for maintaining an inventory of whole-tree chips to be used as fuel.
This article is in PDF format (file size: 100 kb). To download this article, right click on the link immediately below and choose "save target as". To view the article, left click the link immediately below.
(Download the latest Acrobat Reader if required.)

Should whole-tree chips for fuel be dried before storage?   ( )

Whole-tree chips deteriorate more rapidly than do clean, debarked chips and present a greater hazard for spontaneous ignition when stored in outdoor piles. To prevent ignition, the chips can be stored for only short periods of time and the frequent rotation of the storage piles results in high handling costs. Drying the chips prior to storage will prevent deterioration and heating, provided the chips are stored under cover. In many cases, the costs of drying can be recovered when the chips are burned for fuel. In these instances, drying and covered storage is the least expensive method for maintaining an inventory of whole-tree chips to be used as fuel.

Author: Springer, E. L.


Source: (Research note FPL ; 0241):5 p. ; 27 cm.

Citation: Springer, E. L.  .  Should whole-tree chips for fuel be dried before storage?   (Research note FPL ; 0241):5 p. ; 27 cm..

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: FPL (Forest Products Laboratory)

  • KnowledgeBase: Forestry

  • KnowledgeBase: FPL (Forest Products Laboratory)


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2021 - Woodweb.com
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review Woodweb.com's Copyright Policy.

    The editors, writers, and staff at Woodweb.com try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at Woodweb.com after considerate evaluation, and at their own risk.

    Woodweb.com
    865 Troxel Road
    Lansdale, PA 19446

    Contact Us











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article