Q.
I recently put up some red oak to dry and I notice I`m getting some stains. Can someone tell me the reason it`s doing this and what to do about it.

How deep will the stain go? Will it plane out? Thanks for any help, I didn't realize there is so much involved in properly drying wood.

A.
How did you notice the stains? It is hard to identify the stains on the Internet -- looking at them firsthand is the best way. They can go quite deep. Most stains are a result of drying too slowly.
Gene Wengert, forum moderator



From the original questioner:
I used some of the scraps for stickers. Would this be from those bleeding out? I noticed it when I took the pile apart to see how it was doing. Maybe the stickers themselves were too wet?

A.
It certainly could be the result of using wet scrap pieces for stickers.
Gene



Thank you Gene, I certainly have a lot to learn, but it really is a fun thing to do!


It might be a good idea to unpile the stack and restack with dry stickers. When I use old stickers that are not perfectly clean, I soak them in diluted bleach, then re-dry them.


Sticker stains are caused by fungus. Using the same species which might have the same fungus, especially old stickers, is not recommended.

It is recommended to use stickers of a different species, which will not support the same fungus as that which will stain your lumber. Also, keep your stickers as narrow as possible. Using the short boards for stickers is a sure way of getting sticker stains. Many kiln operators now use profile stickers which are hollowed out in the middle and only make contact with the outer edges.

Exploding that myth, Gene replies:
Sticker stain is NOT caused by a fungus. It is the result of chemical enzymatic oxidation within the wood.

Stickers do NOT become infected with sticker stain and transfer it to another load. Even if it were fungus-caused, 130 degrees F in the kiln kills all fungi, so the wood and stickers are sterilized.
Gene



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Primary Processing: Kiln Operation

  • KnowledgeBase: Wood Engineering: Wood Properties

  • KnowledgeBase: Knowledge Base


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2021 - Woodweb.com
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review Woodweb.com's Copyright Policy.

    The editors, writers, and staff at Woodweb.com try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at Woodweb.com after considerate evaluation, and at their own risk.

    Woodweb.com
    865 Troxel Road
    Lansdale, PA 19446

    Contact Us











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article