My parents are having a house built, and if I take the trees before the lot is cleared they are mine. I have access to a 20-by-20-by-26 barn for air drying, and believe I can make a crude sawmill setup for limited use. Many trees are 6-inch diameter oaks and maples, and there's also 12-inch pines, along with a few much larger trees.

My question: Will I encounter any special problems because of the small size of the logs? I will be using the materials to build a 20-foot catamaran. Most of the oak will be made into 2-by-2s. Any tips, ideas, opinions?



Twelve-inch pine can be used to produce common construction lumber. The small oak and maple will probably be of little utility for any application requiring high grade, stable wood.

Six-inch logs will yield little material larger than 2-by-2, and only then if they're straight; but 2-by-2s sawn out of small trees like these will probably be difficult to dry straight. The tight grain arc and juvenile wood will make them unstable.

None of the species you mention are typically used in boat construction; further, boatbuilding is usually done with very high grade lumber, often vertical grain, neither of which can be expected from small trees. From what you've said, I don't think harvesting this wood for boatbuilding is worth your time. The pine in particular, though, may be useful for other things.



I always hate to see good trees go to waste, but if the trees are that small, let the bulldozer clear them out and don't mess with them. I wouldn't try working with a tree less than 16 inches in diameter.


I would cut the pine up to use to make a shed for your boat or whatever. The small trees can be cut into firewood and you will not be letting as much of the wood go to waste.


From the original questioner:

So if I were to cut, say, four 2-by-2s out of the center of the oak (in this boat oak is a very good material for several specific parts) and dry them slowly, would they be strong, and resist any-post drying splitting? (I don't think warp is a big deal in these pieces, because they will be steam-bent anyway.)


"...would they be strong, and resist any post-drying spliting?"

That's just the problem: When dealing with juvenile wood, it's a crap shoot. It may do OK, it may not, but most likely not.

If you're dead-set on using these to get the 2-by-2s you need, you might try getting some pieces off the sides instead of from the heart. You might be able to squeak out two pieces from the outside of the logs rather than four from the heart.



The last poster is right, if you're going to try it at all, you have to stay away from the heart. Any piece with the heart boxed will split; walnut is about the only hardwood I've seen that can hang together when the heart is boxed.

If you want to go ahead with it, by all means do it; if nothing else, you'll learn a lot. I still think there's a better-than-even chance it won't work out. If you're steam-bending, you still need a piece of straight-grained, uniform wood to get a good bend. And remember that even if the lower trunk is clear of limbs now, it wasn't at one time and those knots are buried down in the center of the log.

To get a clear 2-by-2 out of a 6-inch diameter log (assuming it's absolutely dead straight), the tree would have had to be clear of limbs at that height when it was 1 inch in diameter, and this is not likely. In addition, when trees are small they often waver as they grow, so the pith isn't dead straight -- this will make it even more difficult to get clear blanks that avoid the pith.

There are issues in the bending end of this also. You can't take a warped blank and bend a fair curve (since you're bending these 2-by-2s, I assume you're making ribs). The same irregularities and stresses in the grain that cause the warp are likely to cause irregularities in the bent piece. Any knots, or irregular grain covering old knots, will cause spots that won't bend fair with the rest of the piece.

Think of it this way: Take a straight-grained 2-by-2, then put a 1/4-inch-deep nick in one face, then bend it. You'll wind up with a sharp spot in the bend where the wood is weak.

Consider this: Though you say you've got 6 inches in diameter, probably two of those six inches is sapwood, which is not decay resistant like the heartwood of white oak is (I assume this must be white oak if you're going to use it in a boat), and is therefore not suitable for boatbuilding.

Consider too the impact of having poor-quality material in the construction of your boat. Think of the time you'll have invested in getting set up to saw, drying and milling the blanks, then bending each one. If you have a failure rate of one-third because of poor-quality material, your time was poorly spent compared to buying high-grade material that's well suited to your purpose. Chop the 6-inch oak into firewood and sell that; use the proceeds to pay for better material.

Sawing your own wood for a project can be a really rewarding thing, but not if you jeopardize your project by working with stock that isn't up to the task.



If your mind is set on milling your own lumber for this boat, then I would suggest that you do like the last posting suggested and sell the logs for firewood, then take that money and buy some nicer logs to mill yourself. Logs are cheap compared to milled lumber. You could still mill yourself, I just think you're using the wrong logs.


I have a much clearer idea of what I am dealing with now. I think that I will start with the pine (good for temporary jigs, at the very least).

Then I will pick the biggest, straightest oak and see how it goes. With everything that is obviously unsuitable, I'll do as you suggest: Sell the BTUs.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Primary Processing: Sawmilling

  • KnowledgeBase: Wood Engineering: Wood Properties

  • KnowledgeBase: Knowledge Base


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2021 - Woodweb.com
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review Woodweb.com's Copyright Policy.

    The editors, writers, and staff at Woodweb.com try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at Woodweb.com after considerate evaluation, and at their own risk.

    Woodweb.com
    865 Troxel Road
    Lansdale, PA 19446

    Contact Us











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article