Adhesives

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Need to find non-UF Glue for bent laminations

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Need to find non-UF Glue for bent laminations

10/16/15       
Jim Ialeggio  Member

Website: grandpianosolutions.com/

I've been using Unibond 800 for years on bent laminations...most are gentle curves, min radius 6 - 15 meter.

-piano soundboard ribs, 8 to10 x 1/8" laminations in sitka
-piano bridges, 10 to 12 x 1/8" lams in hard maple

The UF glues have always bothered my breathing....its gotten worse, so I need to jump ship on the UF's entirely.

So, in reading through the knowledge based info, it seems low creep options might be Titebond Extend or Extend II. Any experience with spring back and length of time needed in the press on these glues?

Other options?...I use epoxy, but for this its way overkill. Readily available small shop Polyurethanes like Gorilla, have worked for me well on face laminations. Easy machining, no spring back at these radii...but spreading many laminations without the advantages of a spreader of some sort makes the gorilla type polys too hard/slow to apply. Any ways to roll gorilla type glues on face lams

10/17/15       #2: Need to find non-UF Glue for bent l ...
Tom Gardiner

My understanding is that springback is determined by number and thickness of laminations and the tensile strength of the material as well as the radius of bend. Short of glue line failure, your choice of adhesive is not a factor. I have glued many bent lams with Titebond 2 and haven't had issues. In the summer I would have preferred to have longer open time but I overcame skinning of the glue by spreading more. Messy insurance. Springback was predictable and small. I would recommend full 12-24 hour cure on the form or drying fixture but you would be doing this with any glue.
I am happy not to be breathing in the UF fumes anymore and the easy clean up of PVA is a bonus.

10/17/15       #3: Need to find non-UF Glue for bent l ...
Jim Ialeggio  Member

Website: grandpianosolutions.com/

talked to both Titebond tech,and Daryl @ vacupress re Unibond 1. Titebond extend has the hardest glue line of the Titebond line, and Unibond 1 was formulated to that same hard(relatively speaking) Extend PVA glue line + a blocker for veneering.

I decided to try the Unibond 1as it has the extend glue line and also can be tinted as per the wood color.

Bent lamination clamp times have been at least 12 hr with the UF. I will give the PVA a full 24 hour, and/or set up a resting caul, where laminations can be taken out of the form after 24 hrs, and clamped very minimally (just to hold the existing shape) in the form as they cure for a few days.

12/10/15       #4: Need to find non-UF Glue for bent l ...
Gene Wengert-WoodDoc

You mention Unibond. Are you thinking about Unibond 800? This is a UF adhesive...urea formaldehyde. Actually Unbind makes a whole lot of adhesives, so some additional specification would be helpful.

When using any adhesive with "F", you probably want to use very good ventilation, due to the carcinogenic effect.

When you mention gorilla glue, that is one specific type of polyurethane adhesive. There are many different ones with different spread requirements, curing times, and so on. You should explore these adhesives because they are excellent and have no "F".

Even some PVA adhesives have "F" in order to help curing. Check the on-line Consumer Info Sheets and you may be surprised...a small amount of "F" but it is there.

12/10/15       #5: Need to find non-UF Glue for bent l ...
Jim Ialeggio  Member

Website: grandpianosolutions.com/

Are there Polyurethanes available in small shop quantities...ie a couple of quarts or a gallon at a time? Last time I tried to research this, commercial Polyurethanes seem to only be available in rather large quantities.For this reason, I haven't looked too far into the other PU formulations and mostly stick with Gorilla PU glue...Gorilla PU is available in small shop, small run quantities.

Am I missing out on other small quantity PU supply options?

12/10/15       #6: Need to find non-UF Glue for bent l ...
Gene Wengert -WoodDoc

PUR also does not have any moisture, which be a help sometimes. However some PUR adhesives are not as rigid, which can be an issue.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)