Subject: Re: How to clamp 4' x 8' sheets evenly

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

How to clamp 4' x 8' sheets evenly

5/21/25       
John S

I am looking for a way to clamp material to 4x8 sheets of plywood. The problem is trying to get even pressure across the sheets so it adheres evenly and doesn't bend during the dry times. I am planning to do up to 50 sheets at a time, finishing at 3/4". My current idea is to use ratchet straps over some angle iron or something similar to keep it flat. Any suggestions on equipment or ideas you may have would be helpful, thanks in advance.

5/21/25       #2: How to clamp 4' x 8' sheets evenly ...
Ken Member

Are you talking about gluing 4x8s to 4x8s or dimensional stock to the 4x8?

5/21/25       #3: How to clamp 4' x 8' sheets evenly ...
John S

Ken
We will be gluing 3"x48" pieces to the plywood. Maple to maple plywood.

5/23/25       #4: How to clamp 4' x 8' sheets evenly ...
David R Sochar Member

Will a vacuum bag worK?

5/25/25       #5: How to clamp 4' x 8' sheets evenly ...
Tom Gardiner

If this is a money making venture and not just a one off then you will need to invest in an hydraulic press.
You will have significant adhesive and wood movement issues to overcome as well as working out how to accurately place 36 pieces of maple on each sheet and get it into the press without shifting.
What you are trying to do is similar to hardwood flooring. To manage wood movement, flooring is fixed on one edge and the other is free to move in the tongue and groove. Engineered flooring is essentially plywood and can be glued down with a flexible adhesive - flooring mastik. You might consider that technique.
Do not glue down solid wood to the ply and expect it to stay flat. Read up on wood movement from moisture cycling. I recommend "Understanding Wood" by Bruce Hoadley or just read through the numerous threads here on woodweb.
I strongly recommend making a sample and running it through simulated environmental cycles to test the feasibility of the product.
You do not want to end up with fifty epensive maple potato chips on your hands.

5/27/25       #6: How to clamp 4' x 8' sheets evenly ...
John S

Tom
A press or something similar is what I am looking for recommendations on. Placement, glue, and wood are all things I understand well. What I don't know is what type of press or clamps are available for a project of this size

5/27/25       #7: How to clamp 4' x 8' sheets evenly ...
John S

David
I had not considered a vacuum bag, will look into that

5/28/25       #8: How to clamp 4' x 8' sheets evenly ...
Acctek  Member

Website: acctekcnc.com

A vacuum bagging system may be suitable for this project. The vacuum creates uniform atmospheric pressure across the entire surface. You can laminate multiple panels at once.

5/28/25       #9: How to clamp 4' x 8' sheets evenly ...
Tom Gardiner

I do not think a vacuum press will be sufficient to ensure a flat pressing. I would look for a 4 X 8 hydraulic cold press. If you use a slow setting adhesive you could load multiple sheets at a time.
Here is a typical pod press with a large daylight that could handle your job.

https://woodweb.com/exchanges/machinery/posts/551587.html

5/29/25       #10: How to clamp 4' x 8' sheets evenly ...
Will Williamson  Member

Website: http://www.willmade.com

I use the vacuum Table on my CNC to clamp 4 x8 sheets pulling 22 inches of Vacuum Works very well

6/8/25       #11: How to clamp 4' x 8' sheets evenly ...
BH Davis  Member

Website: http://www.bhdavis.net
A 4x8 vacuum frame table is about as good a method as you can get for this. It will give you even pressure over the entire surface while keeping the plywood flat. You just have to have a way to make sure the parts applied to the plywood don't move during the pull down process.

This will give you 13 lbs of pressure per square inch at full vacuum pull down. I once put a piece of 3/4" particle board on top of the open end of a joint compound bucket as a base for a pressing operation and placed the assembly on our vac frame table. The vac pressure punched a 6" round hole in the center of the particle board.

https://veneersystems.com/product/flip-top-frame-49-inch-by-121-inch/

BH Davis

6/27/25       #12: How to clamp 4' x 8' sheets evenly ...
Poor Bunny Member

Using a vacuum bagging system may be an effective approach for this project. It ensures even pressure distribution across the surface and enables the lamination of multiple panels at once.

5/4/26       #13: How to clamp 4' x 8' sheets evenly ...
Quint Member

Vacuum frame table is the right answer for this kind of volume work and the pressure math backs it up. The main challenge with strips rather than a single sheet is keeping all 36 pieces from shifting when you pull down vacuum, so some kind of registration system or slow-set glue that gives you time to verify placement before committing is worth sorting out before you scale up. A cold press with multiple daylight openings would let you batch more efficiently but the capital cost is significantly higher than a vacuum setup.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • Excel Dowel and Wood Products Inc.
      Plain and Pre-glued Dowel Pins, and Wood Parts - Servicing Small Hobby Shops to Large OEM's
    • Vacuum Pressing Systems, Inc.
      Vacuum Pressing Equipment - Including Bag and Frame Systems

    Become a Sponsor today!