Hi there, I am having trouble finding a better way to fill voids, cracks, knots quicker and easier. Currently we are filling with 5 minute quick cure epoxy mixing in sawdust to aid in the sinking that always occurs. Because they yellow in time is another reason we add sawdust and sometimes black dye. When we do clear we use Art Resin but the problem with it is stays soaking wet for over 16 hours which doesn't always work for timelines and it's super thin causing us to fill several times. We are often doing multiple pours when it comes to reclaimed wood or live edge slabs regardless of different things we have tried. Is there anyone out there that can suggest a better product name, way of applying, and any other advice?

11/22/17       #2: Epoxy problems ...
Pete Anderson  Member

Website: petesfloors.wordpress.com

Have you tried wood flour for the thickener?It doesn't seem to shrink when I use it. I use 100 grit sanding dust collected from the edger which has a 7 inch disc. Add the flour before you start to mix everything. Along with the 5 min. epoxy I use general purpose 1:1 mix that hardens in 7 hours cause it fits the budget.

11/22/17       #3: Epoxy problems ...
David R Sochar Member

Contact Rangate, a Woodweb advertiser. They have a knot filler that is much quicker than epoxy. I am unsure about the clear, though.

Knot Filler

11/23/17       #4: Epoxy problems ...
ALEX Gonzalez

Website: http://FINISHINGTOUCHCARPENTRY.COM

We gravitated away from 5 min epoxy long ago. Now using west systems epoxy for higher end applications. We mix with sawdust to add color along with other fibers and color agents if need be. Its a 2 part mix that can be adjusted to go off fast or slow. We build it up over the problem area so when it settles and dries it is still above finished surface and sands out beautifully with just one application. Expensive...but worth it my opinion.

11/27/17       #5: Epoxy problems ...
Alex Sponsor - Rangate

Website: https://rangate.com

Hi Holly,

I work for Rangate, the company David mentioned earlier. We do indeed have an epoxy alternative that's picking up some steam in popularity of late, especially for live edge producers.

It's applied through a heating gun- you apply the hot material into the void, cool it down with an aluminum heat sink, and then chisel off any excess. The whole process takes less than 5 minutes. It doesn't sink after being applied, either. We have about 13 different colors, but the black is the most popular.

If you want to talk to some other producers who are using the material, I'd be happy to put you in contact with some people. I hear from a couple people every week who are very satisfied about not having to do epoxy pours any more. If you're curious to see it work, I attached a video.

I put together a FAQ last week that might be helpful as well. You can check it out under the link.

If you are seeing this message, your version of flash needs to be upgraded to view this video.
Click here to get the latest version of the Flash player.

Knot Filler FAQ

1/9/18       #6: Epoxy problems ...
Matt

On darker colored woods, I have used fiberglass resin with good success, even stain grade, so long as it's dark wood or at least that the fiberglass resin's color blends in.

You can get polyester resin with fast hardeners that should work a lot faster, are basically non-yellowing, and the world is your oyster for coloring.

West System 105 with fast hardener will probably also work well for you,.

For paint grade items, any of the "bond-o" type products work and cure very quickly.

2/10/18       #7: Epoxy problems ...
GeneWengert-WoodDoc

The reason you have difficulty with epoxy is that, as you know, it generates the heat needed for it to cure. However, when you apply it in a very thin coating, there is not enough epoxy to generate enough heat...it needs to be thick. You could apply a thicker coating and then sand off the excess after it hardens. Without the heat required, it will not cure properly and so will seem too soft or sticky.

Note that a soft coating will not work well at times, as when the moisture increases in the wood, the materially can be pushed out slightly; when the moisture drops, a depression can be created. So, a very hard coating is often the best.

2/11/18       #8: Epoxy problems ...
Carlos Levine  Member

I'm not sure what are you doing, if your are pouring epoxy resin as a finish, you can try use polyester resin, is faster, then you can sanded, and pour epoxy resin without problem, if you are using other type of finish, you can try any type of acrylic filler with saw dust, depends on what type of wood your using & what type of finish, you can even use plaster with saw dust!

3/9/18       #9: Epoxy problems ...
Bruce H

I use polyester resin. I tinted some black but that extended the cure time. Using clear, it still takes over night to cure. The items covered with a tarp and a small heater do make a difference. I put mine on a drying rack and cover.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)