Short answer: the residue problem usually comes from using a permanent pressure-sensitive adhesive, not from the label itself. For temporary job-site labeling you want a removable (low-peel, clean-removal) PSA labelstock, which is designed to release cleanly within a defined time window.
When comparing options, separate three variables:
1. Adhesive class - removable vs. semi-permanent vs. permanent. Blue painter's tape is a removable acrylic, but many stock stickers use a permanent hot-melt or acrylic that ages/gels over time, which is why residue builds up.
2. Age and exposure - a removable label is only removable within its rated window. Left on melamine/Formica for months, or in a warm shop, the adhesive can age and split (cohesive failure), leaving residue even though it started as "removable."
3. Substrate surface - melamine and Formica are low-porosity, smooth surfaces. A label that releases cleanly on paper can still leave ghosting on glossy laminate, so test on the actual surface.
A practical check: run a small batch on the real cabinet finish, then peel at 24 hours, 1 week, and 4 weeks, inspecting for both clean removal and residue/ghosting. If labels stay only a few days, a removable PSA on a smooth labelstock usually lifts cleanly with a fingernail or gentle heat; if they stay for weeks, the removal window is what actually matters.