Resorcinol for Sapele

2/15/20       
Harold Pomeroy  Member

I need to make some wide panels for exterior doors, in Sapele. The panels are 58" x20" x 22", double thickness. The door faces north, will be painted, is set back from the porch drip line 8', and the sill is 5' above grade.

I used to use Resocinol to make structural exposed beams, and am used to it. Would it work well on Sapele panels?

I am looking at using Aerodux Resorcinol Resin Kit.

2/16/20       #2: Resorcinol for Sapele ...
Leo G Member

You might end up with the dark line. It should work fine. Probably overkill though. Polyurethane glue is waterproof and more than strong enough to keep panels together.

Personally I would just use Tite Bond II as I have on many exterior doors.

2/16/20       #3: Resorcinol for Sapele ...
Jeff Pitcher

Website: http://www.cpadhesives.com

I would suggest using a reactive polyurethane. It will give you higher water resistance than a Type II PVA but will be simpler to use than a resorcinol.

2/17/20       #4: Resorcinol for Sapele ...
David R Sochar Member

Okay Jeff, what is a reactive polyurethane? I imagine it is the glue that gives you a black hand if you get any on you. Correct?

I know CPA has it, with a less glamorous name.

I used resorcinol in the 70's for exterior work. It came in little cans taped together for catalyst and resin. From Elmer's. It required pressure and heat, but it bonded better than other glues. I still have post caps that look good after 40 years. The wood is nearly gone, but the resorcinol glue line is still there.

I am thinking of going back to it, replacing epoxy in my glue pantheon.

2/17/20       #5: Resorcinol for Sapele ...
Jeff Pitcher

Right you are! It will give you the dreaded black hand. CP carries both the PUR (CP-0701) and the resorcinol (Aerodux 185). The resorcinol will certainly give you the highest degree of water resistance but some people find it a little difficult to use because it's a two part adhesive. If you're already comfortable working with epoxy you won't have any issue with resorcinol.

2/17/20       #6: Resorcinol for Sapele ...
Jeff Pitcher

Website: http://www.cpadhesives.com

Here’s a blast from the past 😁


View higher quality, full size image (4032 X 3024)

2/17/20       #7: Resorcinol for Sapele ...
Harold Pomeroy  Member

Thank you for the replies.

Sapele seems to have a lot of oil in it.
When I burn rippings, the oil actually comes out as a flammable liquid.

I think I will give Resourcinol a try.

2/17/20       #8: Resorcinol for Sapele ...
Harold Pomeroy  Member

No one said anything, but the panels are 5/8" thick, not 58" thick.

2/19/20       #9: Resorcinol for Sapele ...
David R Sochar Member

It has been a while for me, but heat and pressure are what I remember about using Resorcinol.

Heat like over 70 degrees for overnight, with wood, glue, clamps all warm - no chilling along the way. I recall a time whne the boss came in from outside on a cold day while we were gluing up. He left the door open and the temp in the room dropped 20 degrees while it was open. We got him in and unloaded, and closed the door and slammed the heater back on. But that 5-10 minutes that the glue got cold was enough to 'kill' it. Most everything we glued up came apart the next day.

And 5/8" thick? I'll ask the question elsewhere....

2/19/20       #10: Resorcinol for Sapele ...
Jeff Pitcher

Hi David,
With some formulas / brands or Resorcinol the temp was critical. It still is, but with the Aerodux product it's not quite so bad. At 65F he'll get a good cure in 5 hours or so. At 55F it will still cure but take more like 12-16 hours.

2/19/20       #11: Resorcinol for Sapele ...
Harold Pomeroy  Member

Thank you, Jeff. It's good to know about the temperature.

David, the 5/8" thick panels are to match existing in a 90 year old door. The panels are double thickness. The construction is frame and panel, through mortise and tenon, square edged, with panel molding on blocking set in a plough. If the panels do fail, they are replaceable.

When I worked in a shop making laminated beams, the owner would turn the glue room heat up at night to over 100 degrees. The glue would dry hard, but all the wood moved a lot.

2/19/20       #12: Resorcinol for Sapele ...
Adam

Epoxy???????

We have 3 glues on the shelf. Titebond 1, marine type epoxy, and good super glue.

Every once in awhile I used to buy a small bottle of poly for bonding dissimilar materials. It would get used once then end up in the garbage can either because it went bad or because I hate the stuff.

As a side note:

We’ve been using West System G-Flex epoxy for about 10 years for the odd stuff. You guys should get a small kit. It’s the only one that will bond plastics.

2/25/20       #13: Resorcinol for Sapele ...
Zach D Member

Hi all,

So I decided to call CP Adhesives to get some more info on their resorcinol. First, I have to say, they have great customer service. I would not hesitate to call them if I have any questions.
Second, for anyone interested in working with their resorcinol. The open time is 5-7 minutes. Definitely a handy piece of info.

Zach

9/28/20       #14: Resorcinol for Sapele ...
Eric Burke Member

The 5-7 minutes of open assembly time is correct. However, If you can put the resorcinol down and then stack your pieces immediately to minimize air exposure, you can achieve 12-15 minutes of closed assembly time before you have to have it under pressure.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors
    • Vacuum Pressing Systems, Inc.
      Vacuum Pressing Equipment - Including Bag and Frame Systems
    • Veneer Systems Inc.
      Specializing in Veneer Equipment and Veneer Supplies
    • Seam Mate
      Perfectly Aligned Countertop Seams with no Gaps
    • Rangate
      Woodworking Machinery, Supplies and Knowledge
    • ULTI-BOARD
      The Ultimate Spoilboard - ULTI-BOARD - Specifically Engineered and Formulated for the Ultimate in Spoilboard Performance - Not Your Ordinary Sheet of MDF.
    • Excel Dowel and Wood Products Inc.
      Plain and Pre-glued Dowel Pins, and Wood Parts - Servicing Small Hobby Shops to Large OEM's

    Become a Sponsor today!