Subject: Re: Backer Board for Church Parts

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Backer Board for Church Parts

4/26/14       
Chad

We made some rosette parts from mahogany to be placed on a church steeple. We glued up the parts in a way (Octagon) so the grain should not split along the grain.

The contractor has come back to us saying the surface he will install the pieces to is not flat and wants us to build a backboard to attach the rosettes to and then he will attach to the steeple.

Our question is - would you glue up the boards in a regular straight line fashion or in a octagon manner so they won't split. Maybe we are overthinking this as well.

Looking for some suggestions.


View higher quality, full size image (2000 X 1332)


View higher quality, full size image (2000 X 1332)


View higher quality, full size image (2000 X 1332)

4/26/14       #2: Backer Board for Church Parts ...
ZachF

Website: http://lyndandesigns.com

Azek or Extira for the backer.

4/26/14       #3: Backer Board for Church Parts ...
Chad

I suggested both to them - they want to keep it wood.

Thanks for the suggestion

4/26/14       #4: Backer Board for Church Parts ...
Adam

Hi Chad,

I would be inclined to bond the new parts on with a gap filling poly adhesive/sealant like 3m 5200 or PL white poly instead of the backer board.

The original parts were probably old growth Eastern White Pine. It survived up there forever with a few rusted finish nails to hold it on there.

Your parts look really good. I would do a really good prime job before handing them over to the contractor.

Cheers, Adam

4/28/14       #5: Backer Board for Church Parts ...
David R Sochar Member

I assume the octagons are assembled with reinforced joints - splines, fingerjoints, mechanical fasteners or just staggered layers. That is the first step to longevity.

Secondly, the assemblies can be fastened to H Mahogany boards/panels with screws and washers from the back, set up to allow some movement. I am unsure of the sizes involved, but H Mahogany moves very little. The one photo shows multiple boards, probably T+G, where each is allowed to move a bit.

It would be beneficial to prime/paint the parts before assembly considering the location.

If the joints are not reinforced, then you must rely upon the backer for structural strength, and then expect the joints to open in time.

4/30/14       #7: Backer Board for Church Parts ...
Steve Member

Your parts do look fine but I will add just a few thoughts for consideration.

Is the contractor going to do any prep work in the area the parts are going on? I can't imagine putting up those nice replacements on top of the disaster that the picture indicates. A combination of wood replacement and epoxy consolidation and filling of lesser voids should be included in the overall scheme.

Another issue to consider is relative to your product and that is the fact that mahogany is a tannin containing wood and it would have been ideal to glue everything together with an epoxy adhesive or saturate the piece in an epoxy sealer to prevent tannin bleed. The bleed will most likely occur where the paint film eventually breaks at the joints and water gets to the end grain and eventually creates a red/brown staining on the finish coat.

Don't be fooled into thinking the coat of primer and finish paint is enough to prevent the bleeding from happening in the no so distant future. Remember, this trim is EXPOSED to the elements and will take considerable wetting.

If the contractor can get the subsurface reasonable well prepared you can use a bedding compound as is used in the attachment of fittings to a wood boat deck.
One such product is "Dolfinite".

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory