Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: tips on machining birch

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

tips on machining birch

5/19/14       
Jeff Guild

I'm using a W&H to make birch base and casing. About 150 feet worth. When I run the relief cut and the face profile the knives brake out pieces of wood across the grain. Does anyone why this happens with birch or how to stop it.
Thanks

5/20/14       #2: tips on machining birch ...
Adam

Birch is notorious for large chips and big splinters. Sometimes its impossible to run a board thru a planer.

It just seems to be a very brittle wood lacking in adhesion between the fibers.

The only thing you can do is lighter passes. However, its not much help on the Hussey.

Basically its the nature of the beast. Personally I dislike birch in appearance and machining.

5/20/14       #3: tips on machining birch ...
ken

If you have the ability to climb cut it first it works pretty good. Basically run it backwards first. With shapers and power feeders it works, but with your molder, I don't know if you can do that.

5/20/14       #4: tips on machining birch ...
Jeff Guild

reverse cutting works well to rough in the cut on a router or shaper without a fixed feed direction. With the W&H there is a fixed feed direction and fixed motor direction. I've tried to take multiple passes, I've tried spraying water on the face. That helped on the small back out cut. But I run the deeper face it breaks chunks out and splits.

5/21/14       #5: tips on machining birch ...
Will Williamson

What is the moisture content of your stock ? Sounds like you are running air dried material.

5/23/14       #6: tips on machining birch ...
Larry

Normally when birch is run on a molder a cutter head with a very shallow hook is used. It reduces the tendency to pull chunks out. We run with a 10 degree hook angle on a real molder. It takes more power because it is pushing/plowing the wood out rather than slicing. You will need really good hold down & constant feed as any vibration increases the risk of blow out. It is possible to modify a set of knives to make them act like a shallower hook than what the head is. We can do that on our profile grinder, not sure if it is possible to get a good job by hand. You are probably best off taking it to a shop with a 5 or 6 head molder. Machines with two tops can do a better job.

5/23/14       #7: tips on machining birch ...
Jeff Guild

The local mill I use assured me that the birch is kiln dried to 10 to 12%. I bought it about 2 years ago and it sat on a shelf until I got this job to run the trim. I bought W&H about 3 months ago before that I used a Grizzly. I bought the model 206, 230v, viable speed. It leaves a really nice finish on oak and poplar

5/24/14       #8: tips on machining birch ...
David Martin Member

You can choose stuffs as per your budget and expectations. However, before making a final decision, you must go through every aspect associated with the stuff. Further, if you want to get it done in a professional manner, then taking help from a professional could be a wise decision.

5/24/14       #9: tips on machining birch ...
Will Williamson  Member

Website: http://www.willmade.com

Kiln dried in my book means 7 % moisture content. I would expect your same results with that MC.
In my experience Kiln dried stock breaks up into small chunks as it comes off the knife.
As compared to Air Dried 12 % MC.
As the cutter comes around, the knife edge lifts the fiber instead of cutting it and it starts to split ahead of the cutter
Your cutters dull 3 times as fast cutting 12 % MC.
So your knifes are dull also. Will they shave your thumb nail?
And in addition to that your little W& H does not have a chip breaker.

5/24/14       #10: tips on machining birch ...
Jeff Guild

Sounds like that's the nature of the beast with birch it just chunks out with a small molder. I have install trim for 15 years. Learned from the best in the business on high end homes. I still cut my miters with a jig on the table saw. Over the last 5 years I've ran 20,000 feet on the grizzly and W&H mostly red oak and poplar, the grizzly was a good machine because it had 3 knives and it didn't pull up chuchs like the W&H. But I was constantly fixing it. I bought the W&H to make higher quality products. I'm trying to grow my customer base and services offered.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory