Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Holding pre-hung man doors closed

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Holding pre-hung man doors closed

9/15/14       
cabmaker

I have to solve a problem that I have never been up against before. We are building cabinets for a mudroom. Part of the project utilizes a pair of 30 x 80 pre-hung closet doors. A washer & dryer will live behind these doors.

My challenge is to figure out how to keep the doors closed at where they meet. We want to be able to open the doors like they were cabinets, just a simple knob on the stile where doors meet.

Ordinarily I would expect that one of the doors to be fixed in position and the second door latched to the first one. In this case we want to be able to open either door first without un-fixing the other door.

Does anybody know of a hardware system that is designed to do this? Are rare earth magnets my only choice?

Click the link below to download the file included with this post.

laundry_closet.pdf

9/15/14       #2: Holding pre-hung man doors closed ...
B.H. Davis Member

Top door edge ball springs are the typical solution to this. One in the top of each door at the meeting edge.

The problem with ball spring catches though is that with seasonal wood movement the latch moves up and down since it is attached to the head jamb. I've resolved this issue by using a dual latch system.

After the doors are hung and the ball spring catches installed insert a 5/8" to 3/4" disk magnet into the top edge of the door. This is best located on center in the edge of the door and between the ball catch and the meeting edge of the door. At only 3/4" wide there is usually plenty of room to do this.

Then in the door jamb install an opposite pole magnet as close as possible to the stop. It needs to be in line with the magnet in the door but further back towards the stop.

When the door closes the ball spring catch will do most of the work. However if there is a little play in the ball catch sitting in the strike bowl the magnets take over and suck the door back to the stops.

I've used this solution to get rid of rattling double doors. A magnet alone will allow the door to swing open too easily. The magnet combined with the ball spring catch though holds door edges in place.

BH Davis

9/15/14       #3: Holding pre-hung man doors closed ...
Jim Herron

You could use an automatic flush bolt (bottom/top or both) on the secondary door and ball catch on the primary.

9/16/14       #4: Holding pre-hung man doors closed ...
Scott

Try these.
http://www.betterbuildinghardware.com/products/the-ultimate-push-latch

9/16/14       #5: Holding pre-hung man doors closed ...
cabmaker

BH,

Thanks for the detailed explanation.
I've been staring at google pics of this hardware till my eyes are bleeding. I like the idea of rare earth magnet backup.

The automatic flush bolt that Jim recommends is pretty interesting. As I understand it the bolt on inactive door latches it into position as the swinging door is closed and disengages inactive door when swinging door is opened. That is very clever. I hope I can find something on youtube to better explain this.

I also like Scott's $95 solution. This is a little pricey for a magnet but way less expensive than a call back.

Thanks a lot guys!

9/17/14       #6: Holding pre-hung man doors closed ...
David R Sochar Member

For many years, the standard for us was the same as elsewhere - the Ives type roller catch, ball projection/height and spring pressure were both adjustable, though most installers were unaware of the adjustments, and probable no homeowner was ever made aware of them.

Then along came roller catches with adjustability, and the roller helped break the friction.

Both of the above benefited from accurate jigging/installation, so the divot in the catch plate would hold the door back tight to the stop.

As the doors get larger and heavier, the latches seemed deficient. So on our larger doors we went with rare earth magnets just like Bernie suggests. We would double up the magnets and do without the mechanical catch. Now we are looking for a way to set one half of each magnet set on an adjuster so that can be set as needed.

The touch latch suggested is the best of the lot, and works well. However, they can get out of cycle and confuse some users (it doesn't take much...) so we prefer other solutions.

Active/Passive pairs are a nice way to go, and a t-astragal can be used to blind the gap. They can still utilize the magnetic catches, but do not give the choice of opening one door or the other. I think edge bolts or extension bolts would be clumsy and inconvenient.

I have used some modified casement window latches that have sliding bars - internal cremone type latches - that engage the only head, similar to exterior multipoint latches. These are really nice, but add a lot of expense and install labor. Also if they get out of cycle, they can damage casings/jambs.

The hardest part is explaining all these to the owner/builder/designer whose job it is to select and specify.

9/17/14       #7: Holding pre-hung man doors closed ...
B.H. Davis  Member

Website: http://www.curvedmouldings.com

David,

What is nice about the system I came up with is you get the feel of the door latching as the spring ball enters the strike plate. This gives a traditional feel to closing the door.

Then the magnets just give a rearward pull to the door, hugging it back to the stop. The magnets never touch so there is no need for adjustment. The magnet on the top of the door is offset outwards from the one inserted into the jamb. The two magnets pulling towards each other draw the door into the stop.

I personally don't like touch latch systems on full size doors. One can get used to the idea of pressing on a cabinet door to open it. But a full size door is traditionally grabbed by the handle and pulled open. Having to push on the door to get it to swing out seems counter intuitive.

BH Davis

9/17/14       #8: Holding pre-hung man doors closed ...
cabmaker

This is an interesting discussion. There are some things here I never considered.

I agree with BH about the tactile experience. Our lizard brains tell us the door is closed because it closed properly. The dynamics of how to make this happen, however, still elude me. The really sad part is that I am probably not going to be able to amortize all these training costs.

BH, what do you mean by "opposite pole magnet"? I usually work with rare earth magnets that I get from Lee Valley hardware. The magnets themselves install in a metal cup that is screwed to the wood. The other side is just a metal disk

If anybody has any pictures of how this hardware looks installed I would love to see them. As David points most of the work is building the comprehension.

9/17/14       #9: Holding pre-hung man doors closed ...
B.H. Davis  Member

Website: http://www.curvedmouldings.com

The magnets are the Neodymium Rare Earth type. The ones I used are about 1/8" thick x 5/8" diameter with a chamfered center hole for a flat head screw.

I drilled a 5/8" dia x 1/8" deep hole in the top edge of the door and in the face of the jamb just in front of the stop lined up with the door magnet location......but again.....recessed rearward. The 1/8" deep hole allows the disc magnets to be flush with the surface.

The magnet recessed into the overhead jamb is chamfered hole down so the visible flat head screw is flush. The one in the top of the door is also chamfered hole down so this one has a pan head screw. This is the orientation for the 2 magnets to attract to one another as vs. repel apart.

The magnets don't really hold the door closed. The spring ball catch does that. The magnets pull the door to the stop with enough force to gently hold it there. This keeps the doors from rattling around due to the slop in the spring ball catch design. I came up with this solution to solve the issue of the doors rattling in the breeze so to speak.

The magnet system alone won't do the job. If you push a magnetic catch door closed with enough force it just bounces back open. That is why the combination of spring ball catch and magnetic pull works better than one or the other alone.

BH Davis

Disc magnets

9/17/14       #10: Holding pre-hung man doors closed ...
cabmaker

Thanks for the description BH.
I just ordered a set of magnets.

If somebody could gently guide me to the roller catch I need to order our work here would be done.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory