Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Windows

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Windows

8/2/15       
Kevin Member

Hello, I am looking for advice on making wood windows for my 1850 Victorian. I am looking to make replacement units without having to use the existing pulley system. I have been looking at various jamb systems and am looking for feed back. I have a large cabinet shop but have never done windows before. Any thoughts?

8/3/15       #3: Windows ...
Farno

We just tried to do this and couldn't find a
balance that could be adapted to made-up wood windows nor could we find any neighbor who had successfully hung such windows other by using the weights, replacing the parting beads, etc. Available balances were incompatible with the weight and we feared problems in the long term.
PS: If you're in a historic district, regs on the color and type of balances may apply to you (as well as the type of glass; EX: UV reflective, true divided lights, double panes, etc.)

8/3/15       #4: Windows ...
Rob Scaffe

I have built a lot of double hung reproduction windows. Sash weights are simple, effective and an elegant solution-smooth as silk. Perhaps you need to replace the cord but you apparently have all the other parts. Stick with what you have, you won't regret it.

Best regards
Rob

8/3/15       #5: Windows ...
Kevin

Thanks for the responses. I have restored multiple old homes and gone through the pain staking process of restoring old windows. Our typical method includes steaming the sashes and carefully removing the glass. If a piece breaks we then install old salvage glass to maintain the look of the origanol window. We then sand, prime, glaze and so on.
When it come to the jambs we remove any old paint sand and then install new parting beads. I have always had the best luck using fir beads that we mass produce in the shop and then fit on site. My biggest problem has been getting a good fit in windows that have moved as the house as settled over the years. The other problem we encounter is were the sashes meet. I have milled new stock and applied them on site after the we have installed the sashes and that seams to work good. My biggest issue is time. To fully restore a window it takes one man about 8-15 hours depending on the unit size and condition. If I were to make these in the shop I figured we could produce two windows in a 8 hour shift in production mode easily per man. Again that with two shapers set up for my cope and stick, pre milled jamb stock, sills , glass stock pre ordered to size ect. My biggest problem is finding a counter weight system. I have thought of using the existing pockets and weights to match the new units. I think my next step is to take two days and make a test window and see how it goes. Thanks again for the ideas and feedback and look forward to hearing more. Kevin

8/4/15       #6: Windows ...
Rich

Website: http://www.hausmann.com

I have not ordered from this company but they should have what you are looking for.

www.blainewindow.com

8/4/15       #7: Windows ...
Joe Calhoon

Here is how we build DH. The pine section sample is not how we laminate. It was built from scraps.
Weights are expensive but you can make your own from bar or round stock. Save the old ones.
I prefer weighted but the one disadvantage to weight pockets is the heat loss. If you have enough room a foam insulation can be added to the outside lining. Usually not enough room in old 2X4 walls though.
Joe


View higher quality, full size image (1280 X 960)


View higher quality, full size image (1280 X 960)


View higher quality, full size image (960 X 1280)

8/4/15       #8: Windows ...
Joe Calhoon

More pictures.
The frame is the labor intensive part of building double hung but a good system of S4S and moulded parts will cut down on time.


View higher quality, full size image (960 X 1280)


View higher quality, full size image (960 X 1280)


View higher quality, full size image (960 X 1280)

8/4/15       #9: Windows ...
gary

I agree with Joe that the traditional weight system is the way to go. I would completely remove the old windows and replace entirely with new units. Using solid 1-1/2" steel dowels with threaded holes at the top for eyelets makes an easy to adjust/shorten weight. A traditional double hung window properly weatherstripped with waxed jambs ( no paint) is simply the best working window ergonomically and in regards to adjustable air flow.

8/25/15       #10: Windows ...
E. F. Pionkowski Member

Website: http://islandfurnitureltd.net

We do a lot of sash windows and have used a supplier out of England for about 25 years - really high quality fittings and weights - www.reddiseals.com. have a look.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory