Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Reinforced Miters

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Reinforced Miters

8/10/15       
David R Sochar Member

There was a good question about reinforcing miters as mentioned in my post "Ten Years After" in the Galleries: Project Forum in Woodweb.

The drawing below shows that we plow the inside edges of the stiles and rails. After assembling the door frame, we add an accurately S4S'd "molding land". In the case of a 2-1/4" door, this is usually 3/4" thick and wide enough to fit into a 3/4" x 3/4" plow, and will protrude enough to give a solid back to the panel molds, and create a rabbet/plow for the panel or glass. The molding land is butted snugly at the corners - not mitered. It is made tightly enough to need to be tapped into place once glue is applied, and then self-clamped. This will make it align correctly and be dead parallel to the frame faces.

The panel mold is accurately mitered and assembled with Ulmia spring clamps. It is then quickly plowed across the miter - in the rabbeted area - with a 1/4" groover, deep enough to cross the bulk of the joint but not enough to come out into the profile. We do this on a small shaper with a push jig holding the mitered frame at 45 degrees to the fence/travel. It can also be done with a saw blade, standing up on the table saw, for smaller molds and frames. Splines are made and glued into the plows so as to not protrude out into the rabbet of the panel mold. The grain of the splines runs 90 degrees to the joint, 45 degrees to the miter faces and bridges the joint with long grain.

The splined frame is then glued into the molding lands in the assembled and rough sanded door frame. No nails in most cases, just clamps and glue on all contact surfaces. Turn the door over, lay in the panel, and glue and clamp the second side.

This reinforces the miter since the bottom of the panel mold is glued directly to the molding land, and since the molding land is butted, the miter/panel mold is on solid footing. Then the spline also reinforces the miter in a more conventional manner.

This may be seen as overkill, but we obviously have absolutely no problems over time, and fully expect the doors to last as long as they are maintained. The customer is usually bored if I try to explain these things to them (as a means to understand the pricing....). But they have no problems and often say the doors are a favorite part of their project.

Historically, we would see older doors with nice moldings where the miter opened up over time, and the nailed moldings were merely rabbeted onto a square edge door frame, and held the panel in place. Once the miter opened, the integrity of the corner was gone, and it is possible to see daylight thru some of these doors.

Interior doors get the panel land, or a splined miter, but no need for both since the threats are minor in comparison to an exterior door. Couple the methods above with pattern grade Honduras Mahogany and good craft throughout the door, and it is something that takes the product out of the the realm of disposable.

I'm trying to upload a couple of photos......


View higher quality, full size image (806 X 407)

8/10/15       #2: Reinforced Miters ...
David R Sochar Member

Here is a photo with the molding land exposed before the panel and molding are added. Secondary woods are sometimes used. After all, water is not supposed to be in there anyway, right?


View higher quality, full size image (1000 X 750)

8/10/15       #3: Reinforced Miters ...
Mitch Suber

Website: http://subercustomshutters.com

Very nice article David, thanks for providing such detailed explanations. This is certainly something we can use on some of our work.

8/10/15       #4: Reinforced Miters ...
Joe Calhoon

We had problems with large applied moldings opening up on exterior doors. Even small glass beads sprung into place seem to open up after nailing. A few years ago we started using a Hoffmann dovetailer for this and making all moldings large and small as a preassembled frame. This works well and is quick. The assembled frames are easier to finish than loose moldings.

For years on our Victorian style doors we ran a custom large diameter panel raiser with a flat for the applied moulding and deep enough to go into the door groove. This thing was a bit scary on small panels and we went to a inserted spline similar to what David shows.
Lately we have been doing a reversed cope and stick (tongue on the stile). This works well and less parts involved.


View higher quality, full size image (1280 X 960)


View higher quality, full size image (1280 X 960)


View higher quality, full size image (968 X 1296)

8/11/15       #6: Reinforced Miters ...
The Staff at WOODWEB

Here is a second image from Dave:


View higher quality, full size image (450 X 600)

8/12/15       #7: Reinforced Miters ...
Geoff

David and Joe,

Thank you for sharing your methods on how you keep your miters tight. I am interested to know how you keep moisture from getting between the molding and panel?

A common "look" in my geographic area is a door with glass on top and a v-groove panel on the bottom. Having glass with either TDL or SDL makes it difficult to do an applied molding door, Additionally, the v-grooves act as a channel for water to get behind the molding.

Thanks again for your contributions to this website.

8/13/15       #8: Reinforced Miters ...
Joe Calhoon

Geoff,
By nature applied moldings are not the best design to face bad exposure situations. The plank panel complicates this.
Plank panel with square edge detail is easy to weatherproof. The first picture shows a barnwood veneered bottom door rail. Instead of a groove put a tongue on the bottom rail narrower than the stile groove. The exposed edge has a bevel to drain the water off. The plank panel is saddled over this. I have a door we just made with this in the shop and will get a picture tomorrow

When applied moulding is used in combination with a plank panel we make sort of a raised panel out of the planks so the groove does not drain into the moulding. In addition we put a caulk notch in the applied moulding and caulk after finish. The moulding is held like the pictures in my above post. Picture 2 shows this on a normal profiled door. We have venting channels in our doors to drain moisture if it gets in also. With the best efforts applied mouldings are going to get moisture behind at some point in bad exposures. Our Victorian Mountain mining town has a lot of historic store fronts with appled moulding doors to the weather. The old doors did not do well in this situation either.

We have done doors like you describe with applied mouldings below and SDL above. I don’t have pictures of the finish door but we make the upper grills same profile as the raised moulding below. Not as wide and profile both sides of the bars and cope them into the vertical and horizontal mouldings. Picture 3 is a bar being shaped


View higher quality, full size image (968 X 1296)


View higher quality, full size image (1280 X 960)


View higher quality, full size image (1280 X 960)

8/13/15       #9: Reinforced Miters ...
Joe Calhoon

Here are some door pictures from a shop in Belgium. This door is plank bottom and glass top. You will almost never see Euro shops putting panel doors to the weather. They overlay the planks. Sometimes leaving the inside frame and panel.
The doors are thick which makes this easier to do.


View higher quality, full size image (960 X 1280)


View higher quality, full size image (1280 X 960)


View higher quality, full size image (1280 X 960)

8/15/15       #10: Reinforced Miters ...
Geoff

Joe,

Some great information, thanks for sharing. I really like your idea of reversed cope and stick.

Have a good weekend.

8/20/15       #11: Reinforced Miters ...
Jim Lewis

Nice work. Question: Do the splined corners make it more difficult to remove the moldings should it be necessary to replace the glass?

8/20/15       #12: Reinforced Miters ...
David R Sochar Member

If we have art glass piggy-backed over insulated glass, we fasten the assembled frame to the door with oval head screws. This allows for easy removal for cleaning or repairs.

If just stopping insulated glass, we usually only nail the stops in place, with no assembled miters. We also do it with assembled miters - we have no standard on this..... The nails are few, since we use sealant on the interior side as well, and it does more to hold the stops in place than nails will, long term. So far, we have not had to remove the stops for glass replacement. It may not be pretty.


View higher quality, full size image (1944 X 2592)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory