Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Warped material frustration?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Warped material frustration?

9/1/15       
Keith Newton

I posted this over on the Veneer forum, but don't know how many people regularly follow that forum.

I'm needing to get started on building a 12' long kitchen island which will be veneered with some very nice figured Bubinga.

The builder has specified that I use Extira for the substrate, which would be fine with me, since there is a sink in it. When I went to pick up materials, the bundle that my supplier had pulled for me was so warped that I wouldn't accept it.

Then we went back to get a new bundle, and cut the bands on it. It had been sitting on a level floor, and showed no reason for the whole bundle also being warped. Every sheet had 1.25" bow down the long side, and 7/16" across the short axis, creating a bulge.

I'm wondering if I should expect the face veneers to hold this amount of bulge out?
I don't have any extra veneer to do the project over, if it just comes out curved again.

I always thought one of the wonderful things about mdf products were that we could always expect them to be flat.
My local supplier says he hasn't had any complaints, and that he even has one shop using it for exterior doors.

Seems like life is hard enough without having to fight problems like this. Not to mention that with a price over $50 per sheet, flatness would be nice.

What do you think? Are any of you regular users of Extira, and is it always warped when you get it?

9/2/15       #2: Warped material frustration? ...
door shop guy

NO!!! Dont use Extira for cabinets! Every single time i used it for anything it was warped really bad. Flat doors, anything you need flat this is the worst choice.

Of course the supplier says they have never had a problem.

9/2/15       #3: Warped material frustration? ...
Gene Wengert-WoodDoc

The product specified is for exterior use. It is also treated with zinc borate as a wood preservative. I do believe it is not the correct product for a countertop substrate. Note that if it were dried to 6% MC it would not warp, so we know it is at a higher MC, which would typically be ok for exterior use. It also uses phenol adhesive...I have always seen that this adhesive uses formaldehyde as a catalyst. Their ads say "no added formaldehyde" but does this include the PF adhesive?

9/2/15       #4: Warped material frustration? ...
David R Sochar Member

I think it is wise to not let customers specify materials or methods beyond generalities. It is also best if the woodworker uses materials and methods he/she is familiar with to produce the best product for the job.

It would be good for you to gently explain this to the builder/customer. No doubt, as a result of marketing, he envisions the Extira as fending off waves of water over the years, whereas the core stock you might use would fall apart with the first bit of dampness. Your job is to convince him that you are a professional and he can trust you to execute the work in a professional manner.

Beyond finding another vendor, you can easily photograph the panels you have seen and rejected, and ask him if he is sure he wants you to use this marginal material.

9/2/15       #5: Warped material frustration? ...
Alan F.

If you are going to use customer specified materials then use the specified adhesives and finishes so if it fails you did everything to "spec"

Using Extira Panels

9/3/15       #6: Warped material frustration? ...
JeffD

I haven't used Extira, (my main supplier doesn't carry it), so I use a "water resistant" mdf product for my bath cabinetry instead. Unfortunately I don't know the name off the top of my head. Anyway it's about as flat as normal mdf and for my needs, usually veneered vanities and such, it works well. I always sand the face before veneering, 120 grit on the ROS. Using TB Cold Press in a vac bag with paper backed veneers I haven't had any problems with it…..but will admit I've only used it the last few years.

I honestly don't know if the face veneers will hold the panel flat? I would probably consider design changes that would allow for structural support behind the panel.

good luck,
JeffD

9/4/15       #7: Warped material frustration? ...
kevin

Jeff,

Would you be referring to Medex Moisture Resistant MDF?

9/13/15       #8: Warped material frustration? ...
Mitch Suber

Website: http://subercustomshutters.com

I have not noticed any of my Extira sheets coming in warped, always seemed pretty flat. I do use 2 different thicknesses, both 3/4" and 1 1/4". It appears that this product is not as rigid as regular mdf. I would also be concerned about gluing anything to it, as the material has an oily feel to it. This is addressed in the paint recommendations.

9/14/15       #9: Warped material frustration? ...
mark

Moisture content! Extira is an exterior panel, manufactured for average exterior moisture content 10-12%. Good thing you're supplier has had this lot inside for a bit, as it's already starting to warp while reaching indoor moisture content unevenly. It will get 6-7% eventually. Expect buckled veneer if you don't somehow manage to dry it evenly before veneering.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory