Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Does wood thickness matter?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Does wood thickness matter?

3/15/16       
Mitch Suber  Member

Website: subercustomshutters.com

After 25 years of building exterior shutters, my question is, is a 3/8" x 2 1/4" shutter louver any less likely to bow than one that is 5/16" thick? Lengths range from 12" to 30" on average. I am talking about exterior fixed louver shutters, and the wood type may be cypress, red grandis or cedar. I am also asking in regards to a louver that has already passed inspection during the cutting and assembly process. These are all woods we typically use, or will be using. Stress relief and uneven moisture has already been dealt with, as much as possible. For years my biased thinking has been that the thicker wood would somehow be more stable, but many of the things I read here on Woodweb lead me to believe that 5/16" is just as good as the 3/8". Yes a small difference in thickness, but a huge difference (to me) in the cost of making the thicker louver. It also seems like the length is not a huge factor either.

3/15/16       #2: Does wood thickness matter? ...
rich c.

My opinion is that the thicker stock looks better in the bigger shutters. Not going to add any stability, just appearance and proportion. The cut of the wood will make the difference in bowing. Quarter sawn would my cut of choice for real stability.

3/16/16       #3: Does wood thickness matter? ...
Adam

I've only made one house set of shutters in my career.

Who decided that 3/8" was superior? If it has been the "standard" for the last 100 years, it still doesn't really mean anything.

Often the dimensions of such things was determined by ease of fabrication, not the physical properties of the material.

Its kind of like making a structural beam larger than it needs to be out of convenience. The math says it could be smaller, but you would have to cut it down.

Based upon my experience, I would not expect those woods to have stability problems that would be helped by keeping the material a wee bit thicker. If you are having a problem the thickness is not going to be the reason.

3/16/16       #4: Does wood thickness matter? ...
TimG

In short lengths ,no. Longer I'd say yes as it's easier to flex, therefore it takes less force to bend it.

3/16/16       #5: Does wood thickness matter? ...
Mitch Suber  Member

Website: subercustomshutters.com

Tim has made a point that the thicker material has more resistance to force, and I think that is probably the main reason why I always believed the thicker material was better. While a few of my customers believe that closing their shutters can add a level of storm protection, we certainly do not sell them with this in mind. Sure they can deflect a few small limbs, but nothing serious. So with that in mind, for the most part, these louvers basically are made just to sit there year after year, with no force being introduced. So for the most part, I think this is a minimal factor in my deciding which is better, with the exception of orders where a thicker louver is specified.
I agree that quarter sawn lumber would be more stable, but seldom do my suppliers have it available in the wood types I use. Thicker does look better at times, in proportion to the type and size of the panel. I can resaw 4/4 lumber to get 2 blanks for making 5/16" louvers, but not 2 of the 3/8" blanks. Around here, 5/4 lumber is getting harder to find, which I use to resaw, to get the thicker louvers, even up to 1/2". But when I have to plane down a 4/4 board to get a 3/8" louver, that is a lot of waste. Too much labor, too much time and too much waste and all for too little gain. Other factors like moisture or defects will cause problems and bowing in even 1/2" louvers, so that is now not a strong factor in deciding.
Thanks for your thoughts and input, 5/16" it is.

3/17/16       #6: Does wood thickness matter? ...
David R Sochar Member

I would say that thickness doesn't matter. Now, our esteemed Presidential candidates will have no trouble debating the merits of thickness, since "we all know what that means...." But we know better.

If the wood is going to move in response to changes in the environment/MC, then it will do it if it is 1/4" or 2" thick.

Another cause is internal stress caused by the tree's growth or by improper drying. In this case, if the piece if left in the size/shape it was when dried, it may stay that way. But once it is cut, the stress will come into play and the wood will move at the saw. Jointing flat will work until it is planed, when its internal stress overrides that flat imposed on it, and it moves.

Generally, thicker means better quality, and in woodwork, it can mean stronger shadow lines and better mass. We all have seen products where the accountants have thinned the stock and flattened and shrunk moldings to where the product looks nothing like what it should, but it does hit a certain price point.

I don't know that I could detect a 1/16" in slats, so I have no real answer. I do think wood quality and proper drying are the key factors that will affect the flatness of your slat stock.

3/17/16       #7: Does wood thickness matter? ...
socharsux

So you have no real answer but pipe up only to throw in politics.

Nice.

3/17/16       #8: Does wood thickness matter? ...
Mitch Suber  Member

Website: subercustomshutters.com

So isn't the one liner making a comment against David piping in?
Anyway, thank you David for your informative response, which contained good information which confirms much of what I was thinking. Rich, Adam and Tim I thank you as well. I find this forum to be very helpful and I for one really appreciate that. Even when we have to separate and step thru the petty crap. Some people.

3/18/16       #9: Does wood thickness matter? ...
D Brown


Mitch , besides woodworking we have also

been in the window coverings business

for about 25 years . We don't fabricate our own shutters but we do sell them .

Thinking about say a 2 or 2 1/2" blind slats

They are rather thin even maybe about an 1/8" give or take some are thinner.

The most stable wood slats are made of Basswood . So the thickness may not be as important as the properties and stability of whatever material used or the slats would be thicker if stability came with thickness.

3/18/16       #10: Does wood thickness matter? ...
Mitch Suber  Member

Website: subercustomshutters.com

D, interior window treatments played a big part in my thinking prior to my posting the question about the thickness of louver slats. While I also build interior shutters, I have been carrying a few lines of interior blinds for quite a few years. I have always been amazed how stable those thin blind slats are. Ours too are mostly Basswood. Just as interesting to me, is the fact that I have observed about the same % of defective parts in exterior and interior products. Totally different environments, or so it seems. The side of a closed blind in an uninsulated window gets exposure to some very high temperatures during the day, plus I see some higher than expected humidity in some poorly sealed windows. But overall, I would bet maybe 1 or 2 slats per 1000 end up bowing to a degree that is not acceptable, about the same with exterior shutters. I often laugh when customers start telling me how stable plastic faux wood slats are. They may not bow, but I find they sure do expand and droop, even worse than real wood.

4/7/16       #11: Does wood thickness matter? ...
Homee App Member

Website: http://www.homeeapp.com

From the structural point of view you don't have any need of extra thickness, but if you just want to add to its thickness for change in the look or some other design need, then that is your choice.

4/8/16       #12: Does wood thickness matter? ...
Gene Wengert-WoodDoc

Wood warps because of grain angle. Wood warps because of uneven MC, face to face. Wood warps because of juvenile wood, tension wood, and compression wood.

So, straight grain (like we use in high value pool cues) with a finish to slow moisture changes, and with avoidance of special wood will behave excellently. From a resource point of view, basswood meets all these criteria, so is the preferred species.

Note that thickness is not an issue, but if things are not perfect, thin pieces will warp more easily than thick. The reason is that a small MC change or other issue requires more force to warp than in a thin piece.

5/7/16       #13: Does wood thickness matter? ...
David Waldmann  Member

Website: vermonthardwoods.com

Have you considered using a thin kerf multi blade frame saw and 10/4 material?

That way you would essentially have quartersawn material and the least waste possible. Yes, I know 10/4 is more than 4/4 per BF, but I bet the reduction in waste makes up for it, and you get the additional stability of quartersawn for "free".

It would also give you the ability to change thickness as required and still use the same material.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory