Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Reclaimed Slab Doors

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Reclaimed Slab Doors

4/7/16       
Richard

Hello All,

I am designing a utility room cabinet for a customer who would like to have slab doors made from reclaimed wood that she is supplying. She has given me the attached pictures as a guideline of what look she wants.

My concern is that the doors will be quite large, in particular there is a broom closet with a door that is approx 17"W x 102" H. How would you prevent a door like that from warping?

Any thoughts are welcomed.

Thanks

Richard


View higher quality, full size image (410 X 539)


View higher quality, full size image (596 X 370)


View higher quality, full size image (413 X 508)

4/7/16       #2: Reclaimed Slab Doors ...
Edi Silva  Member

Website: silvawoodworking.com

Richard

We just finished a project that we use some reclaimed wood for the back of the island and for a Barn door between kitchen and mudroom. The material we used it was 3/4" thick so we end up making the the door 1 1/2" thick by gluing two layers with the Vacuum bag. Works perfect, they door came out nice and strait.

Edi

http://www.houzz.com/photos/48205427/NEW-CANAAN-CT-contemporary-
kitchen

4/7/16       #3: Reclaimed Slab Doors ...
Dennis Bean  Member

Website: http://www.saliceamerica.com

Hafele offers a product called "Planofit" especially for the purpose of stabilizing large cabinet doors. The stabilizer is installed to the inside surface of the door to add rigidity and to prevent warping. here is the link to Planofit.

Hafele Planofit

4/7/16       #4: Reclaimed Slab Doors ...
JOHN Member

Richard,
In my experience, the moisture content is key to making sure that door stays straight. Get it to 8% and seal it right away. and at 102" tall, you would need perfect conditions for reclaimed wood to stay straight. Ive made over 2000 tables from reclaimed cedar, pine, doug fir, and white oak, and I've come to realize that you cant fight mother nature when it comes to old growth wood. It does what it wants, and doesn't care about your project.

4/7/16       #5: Reclaimed Slab Doors ...
David R Sochar Member

Why will the wood warp?

Wood warps in response to changes in moisture content. If you are the responsible party, then it is your job to insure that the wood purchased is at the proper MC, or you will have to do what is needed to get it to the proper MC. 2 weeks on the job acclimating will not give the assurance I think you will need. Meter each and every board in several places before you start the project. One board that is not at your target MC can cause problems. Proper MC and EMC can be determined by charts as found in Bruce Hoadley's book Understanding Wood.

Solid wood doors as in the photo usually have horizontal battens on the backs that are fastened to allow wood lateral movement. Surface mounted or inlaid, dovetailed or decorative, they should be considered essential. The doors will still move with the unavoidable seasonal variations in relative humidity, so you will need to know that range so as to plan gaps and clearances correctly.

4/7/16       #6: Reclaimed Slab Doors ...
rich c.

Make sure they kiln dry the reclaimed wood to kill bugs before you get it. If they don't, you may get a call in a few months asking about the little piles of sawdust on the floor under the doors. Powder post beetle eggs love to hatch out in the nice warmth of a home.

4/8/16       #7: Reclaimed Slab Doors ...
pat gilbert

Rip and Flip others will discount this, just saying technically it has to alleviate warp.

4/18/16       #8: Reclaimed Slab Doors ...
Richard

Thanks All.

David, I like the idea of doing some kind of decorative inlaid battens do you have any more details or thoughts on how this might be achieved?

Thanks

Richard

4/26/16       #9: Reclaimed Slab Doors ...
David R Sochar

Rip and flip was a strategy that came about as a way to deal with boards cupping across their width as they responded to changes in environmental humidity. The rest of the story also mandated that no piece of wood be wider than 3". This was during a time when most wood was air dried or in the early dries of kiln usage.

The 'rule' was extensively promoted by Jerry Metz as a keystone of "Metz Rules" that he offered in 25 years as a columnist for a woodworking journal.

I feel that current thought is that the two steps mentioned in the old saw are no longer needed, since cupping across width is not a problem with solid wood that is used inside and dried properly.

As asked above - Why will the wood warp? Understanding this will help a woodworker concentrate their energies and resources where needed instead of blindly adhering to uneccessary and outdated rules.

4/28/16       #10: Reclaimed Slab Doors ...
rc

did a run of doors like that recently
resawed the weathered surface off old pine boards------> sanded to 1/8" in ----->layed up on perimeter internally banded3/4" mdf cores, doors came out of press @ 1" thick, very flat , the freshly milled perimeter wood(edgebanding) was finished as a weathered grey

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory