Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Cedar On A Ceiling

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Cedar On A Ceiling

7/1/16       
Ray Member

Website: http://interiorfixtures.weebly.com

I will be installing red cedar on a ceiling 16' X 32' that has 2" of soft sound insulation that is attached to the bottom side on a metal grid system. The boards are 16' long and the sizes are 3/4" X 3/4", 1 1/2" X 1 1/2, and 1 1/2" X 2 1/2" with a 1 1/2" spacing that makes a random but repeating pattern. With no expose fasteners.
I tried rabbiting the top side of lumber 3/8 X 3/8 and use some power grab adhesive that would receive a same size stick but 8" long, with a screw in the middle of it. The pull out test was iffy.
I would like to find metal clips that would work.
Anybody suggestions?
They rejected holes and plugs but could have to live them.

7/2/16       #2: Cedar On A Ceiling ...
james mcgrew Member

I would call Kip Porter at Star Hanger, Man is a genius in Fastening architectural work

http://starhanger.com

7/3/16       #3: Cedar On A Ceiling ...
TonyF

Ray:

Would it be possible to fasten some 1/2" plywood to the ceiling, and then it may be easier to fasten the cedar to the plywood?

16 sheets of plywood could be an inexpensive cure. Does any of this material need to be fire-rated?

TonyF

7/3/16       #4: Cedar On A Ceiling ...
Ray Member

Tony
That is something I haven't considered. The 2" insulation is attached to the grid by
clips. I will ask if the clips would work with
with plywood. Yes this needs to be fire rated blocking.

7/3/16       #5: Cedar On A Ceiling ...
james mcgrew Member

Use fire rated Ply wood adn cut strips where needed, no need to cover entire cieling it is blocking,, or go straight to studs, it is cedar floor plank right ?

7/3/16       #6: Cedar On A Ceiling ...
Ray Member

James
This is lumber of 3 different sizes with spacing between each board. The largest is 1 1/2 X 2 1/2 some are laid flat and some on edge. The 2 1/2" plus the 2" would require a 5" screw. Plywood strips or 2 X 4 blocking might work. Cut sheets attached.
Plugs and screws will be a hard sell.

Click the link below to download the file included with this post.

USG_Drywall_Suspension_System.pdf



Click the link below to download the file included with this post.

USG_Drywall_Suspension_System_2.pdf

7/4/16       #7: Cedar On A Ceiling ...
Adam

The simplest easiest way would be to fasten 1/2" plywood or 1/2" osb to the whole ceiling.

Then you can toe screw any of those pieces of wood to the ply.

I would not consider doing this job on a contract basis. T&M only or they can find somebody else.

7/5/16       #8: Cedar On A Ceiling ...
Pat Gilbert

This is for a ceiling, right? There are no studs in a ceiling.

7/6/16       #9: Cedar On A Ceiling ...
Mark  Member

+1 on screwing ply to the ceiling; use self tapping tek screws w/wafer heads. Since the ceiling is suspended I'd check with the contractor/architect/engineer to be sure the system can carry the weight of fire rated ply.
Then paint the background, adhesive & trim screws to apply.

7/6/16       #10: Cedar On A Ceiling ...
TonyF

Ray:

Mark makes good points about painting the background, for uniformity and possibly for contrast, and determining if the suspended ceiling infrastructure will hold the weight of the plywood. You should also consider the combined weight of the plywood and the cedar.

If the weight capacity allows you to use the plywood, one thing that you might try is to channel or rabbet the cedar, much as you tried before, except now you can pin the glue strips to the plywood.

You could fasten these glue strips prior to securing the plywood to the ceiling, allowing you to register the spacing you need for the cedar pattern with the glue strips, making the installation of the cedar E-Z.

Not sure of the finish requirements, but with glue strips in place, you may be able to pin the cedar in place through the face with a 23 gauge Grex pin nailer, which would almost defy detection from the floor, or through the sides of the cedar with a nail gun if the spacing between the cedar does not allow a full-on view of the cedar sides.

Good luck.
TonyF

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)