Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Front door

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Front door

2/17/18       
Mike

Greetings all,

I’m heading to a customer’s home to discuss a new front door or full replacement, jamb snd all.....

I’m debating between Douglas Fir and African Mah. Preference and why?

It’s a half circle and she wants a price a few different ways....

1. Right now the door skin is plywood and it’s delaminating. She wants to find out what it would cost to modify the door and cut in a half circle top glass or full circle.
1a. My challenge is to determine how to make the mullions and muttion bars (fixed on exterior and removable on interior. I’d have to devise a way to properly insulate around the cut out. Also, could I “get away” with using a 3 ho router, vs buying a shaper (which I would rarely use

2. I do not have a CNC, so I’d have to do it the old fashioned way with a router.

2a. Since udding a router may be my only way of making the arched top, my thought is to glue a few boards together and route the arched top out of that and join the segments together via biscuits, dominos, spline or mortise and tenon.

3. Where could i ger weather stripping that will press into a groove.

4. Regarding measuring for the radius, my thought is as follows:

5. Put a piece of masking tape in a centralized location, so I have the length of chord (width of the door) mark my center at a point where arc starts, then measure to the center of the furthest (highest) point of the chord) lay it out in autocad, then offset my lines

6. Measurements for opening, the opening, I cannot think of any other way, than to pull the casing on the interior

7. The exterior is stone

Anything I’m missing?

Thx!

2/19/18       #2: Front door ...
David R Sochar Member

I will stake out the negative opinion and state my personal advice is to sub this out to a person that knows all about building doors.

Everything comes together in a main entry door: Security, appearance, function, hardware, finish, durability, timing, and more.

It is basic to have a working knowledge of finishes, hardware, weatherstrip, IGU, muntins and their joinery, sealants, glues, exterior jambs, sills or thresholds, wood species and door construction details and methods.

You seem to have given the geometry some good thought, but that is the least of your worries.

Where is your previous experience and at what level?

Just because someone asks you does not mean you have to do it.


View higher quality, full size image (1401 X 2226)

2/19/18       #3: Front door ...
Mike

I have over 20 years as a custom cabinetmaker/furniture builder, but front doors are a new ballgame for me and a challenge I’m definitely up for, especially since this is now the third request in just the past year. What makes this one uniquely different and difficult for me is the arched top like your pic and then to add the mutton bars to boot (on the radius)

I’m looking for advice from those such as yourself, to help “guide” me through the best practices on making these types of doors....not sub it out.

We all didn’t become good at what we do over night, nor by not asking questions.....hence the reason i’m asking for guidance.

Thx!

2/19/18       #4: Front door ...
David R Sochar Member

My answer may not be much different than earlier. I don't mean any disrespect. I appreciate the jump in and swim method - it is one of my favorites. But it is not for everyone, and at some point it's too deep or the current too strong and you find things going out of control.....

If this came to me, I would encourage a completley new door and frame. Re-use the hinges, latch, and interior trim if possible. Patching onto an existing door means that if something pops 3' from your new work, you get the call, and you get to explain why it is going to cost more money - and time. There is not a clean way to join stile butts together if it is rail and stile (or frame and panel) or flush (as it sounds like).

That, and the cost will be about the same for the repair over new. I can spend days and days piddling around on historic doors, whereas a new unit gets run thru the shop on its normal pace.

One big advantage to a new unit is that it can arrive on site 100% ready to go in. Finished if you like. Tear out the old and set the new in one day, go home done, happy all around. Yes, it costs more (but you sell more!). I have sent out door slabs to nice older houses where the carpenter wants to fit and hang, and after 3 days of cutting, it is too small, and we get a call to cut down the jamb, or shim hinges, or worse, the owner calls and says they don't think he did a good job.....

Now curved muntins - that will be chapters 146 thru 182 in my How To Build A Door Book. It would take a half day of explaining with you in the shop, and it is distinctly tooling driven. More than a few router bits. That and every shop doing it is doing it differently. CNC is not required, by the way. We also only do divided light glass, and never tacky tacky muntins.

A shaper is fundamental to door making, even if it is the upper half only. And a curve head door, frame and perhaps trim? Start shopping. We have two shapers for a two man shop, and over $16K in tooling.

Some people get offended when others that think complex knowledge can be handed over in a few minutes of typing. I once had a woodworker ask me to teach him to build curved stairs - he had an afternoon free and could pay me for two hours work. I spent two hours talking about the good ol' days and petting his dog, and invoiced him. I spent years learning it. I still take huge risks building them. I'll learn something new on the next one. While I do not mind sharing my knowledge when it is well received, it is not simple stuff. Curved muntins? I learn that every time I do it. And will again.

Since we cannot do the door book here today, I can back out a bit and say the two most important things you need are a good mechanical mind, and aggressive, multi faceted problem solving. You may well have both since you have long experience. If you are nearby, come on by one Saturday, bring some good beer, and I'll tell you all about curved muntins and answer your questions. I'll also talk about them good ol' days a bit.

2/19/18       #5: Front door ...
Adam

Doug Fir has no rot resistance. The common African Mahogany other than Sapele is difficult to work. Very hard, squirrely grain that typically tears out. Spanish cedar or SA mahogany is a better choice.

Door is made of plywood. Stop wasting everyone's time and build a new one properly.

Door is delaminating. glue it back together with epoxy. No warranty.

Door is delaminating. Glue it back together with epoxy. Modify it with complicated glass work. No warranty.

You could spray some of the blue foam that we use around windows and door jambs. If you choose to go down that rabbit hole.

Build a new door.There are plenty of cutters available for routers that will allow you to make such a door. In order to be accurate and safe we use shapers with power feeds.

Making these type of doors is a risky proposition. They either work well for a decade or for 6 months. Then you start trying to fix them.

We've all taken on projects that are sink or swim. Be prepared to lose a bit of time and money on this first door. Then decide whether its worth it to make another one. That's how we all learn.

2/21/18       #6: Front door ...
dConti

First off you will need a good 8ft jointer, you can't build a straight door without straight material. You maybe be able to get 1 3/4 " door out of 8/4 in the rough but I would figure on 10/4 to be sure. The radius is going to be time consuming but can always be made up as shown (in two peices, joined top center. most likely doweled) . So lets get our list started:
1 Jointer
1 Commercial shaper ( 5 hp min)
1 dowel machine
1 Commercial band saw (to rough cut radius peices)
1 set door knives for shaper
1 42 inch wide belt to sand that door nice and flat
wish list: CNC router to cut those header peices just right

This is just my opinion but I think that any millworker that truely makes his money from this sort of custom woodworking and has been successful at it will tell you the same thing. Making custom doors is an expensive time consuming practice and you need to have a customer that knows that and is willing to PAY for your services.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory