Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Woven Wood Doors, Part V Success!

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Woven Wood Doors, Part V Success!

4/13/18       
David R Sochar Member

Part Five - Success!

We set a straight edge (door stile) and a rail at a good 90 degrees to each other to hold things straight as we glued all the blocks together. We used spacers as place holders where there was no block edge. Buttered them up with epoxy, and laid tile for a while. The fit was just right to allow things sliding together with a tap every now and then.

No clamping required since this is epoxy.

The hardest part was keeping the alternating grain correct. We watched each other and avoided a calamity. A panel was built on each bench and allowed to cure overnight. Our benches are carefully leveled and have no twist, curve, bow or defect that can be transferred to the work they build.

The next day, the panels were rigid, though we left them in place on the benches since there was no need to tour them around the shop. No sense tempting fate, eh? The track saw was set up to rip off the protruding blocks on all four sides. A router with a long baseplate was then used to mill a new dado into the edges with allotting cutter, on all four sides. This would accept a spline - the same size as the ones on the blocks - that would also fit a plow in the rails and stiles.

The panels look a lot like a solid wood panel, with all the grain going in one direction. The splines were cross grained and would limit some movement. But in my experience, I have not seen Honduras Mahogany move. I have 13” wide panels on a west facing, small overhang exterior door in the house, and after 12 years, they finally almost crack the paint. Almost.

So - how much room for expansion? This is critical because half the blocks are cut off square and will stop short of landing on or touching the rails/stiles. We opted for a slight 1/8” all four sides - .100”. Top and bottom do not need any clearance, but we thought it best for continuity.

The tenons were milled and mortises made, and we added the stiles and rails to the panels right on the bench. A few clamps, and they were assembled. All familiar ground. Remarkably easy, especially compared to the path we had already trod.

We have about 18 blocks left over. Enough for a 4x4 sample panel that we will oil up and try to keep in the shop.

The next day we sanded the frames, eased edges, cleaned up a little glue. Justin machined for hinges and extension bolts. We loaded them up and took them to the finish shop. We did spend a bit of time congratulating each other and smiling a bit more than usual. Satisfaction is the norm around here, but these took it somewhat higher.

The pair are going into a high visibility restaurant as entrance doors. While I may not frequent the restaurant, I should be able to catch a happy hour and admire our work. No one else will ever know, or be able to appreciate what we go through. Nor will they know the pleasure we take from the work.

Once they are in place, I will post photos in an epilogue.


View higher quality, full size image (1800 X 1350)


View higher quality, full size image (1800 X 1350)


View higher quality, full size image (1800 X 1350)

4/13/18       #2: Woven Wood Doors, Part V Success! ...
Kevin Jenness

David, thanks for the documentary. Your workmanship is admirable. In the end, do you feel you made the right choice in aligning the grain in the blocks given that if the material were actually woven as in a splint chair seat the grain of the warp and woof would be opposite?

4/14/18       #3: Woven Wood Doors, Part V Success! ...
Joe Calhoon

Nice looking and very unique door Dave!
I finally get how it all goes together seeing these pictures.
Joe

4/14/18       #4: Woven Wood Doors, Part V Success! ...
pat s gilbert

Website: http://e

Nice work Dave I think you're starting to get the hang of this woodworking thing.

You finish before install?

4/17/18       #5: Woven Wood Doors, Part V Success! ...
David R Sochar Member

Kevin - I would certainly change the grain directions in the future to reflect the design heritage that would have pieces at 90 degrees to each other, warp and weft-wise.

I looked at the original image (with all grain running vertically) and thought of it as a large panel on a CNC bed - maybe. Since that grain ran the same way, I guess I just picked it up and ran with it.

That is the one thing I would change. I am not sure how it got out from under me. I think I was taken up by all the other niggling things that I missed the forest for the trees.

The effect is still very strong and came out better than I hoped. Sometimes, I beat myself (ourselves) up with these missed opportunities, but most observers will never see the level of detail that we all operator on. I try not to become callous in these judgements in fear of accepting a product that is less than it can be. If something is a bad miss, we will scrap and start over. But that is very rare, and has only happened at the start of the project.

Thanks for all the comments.

Installed photos coming next week or so.

4/17/18       #6: Woven Wood Doors, Part V Success! ...
Russ

Dave
I always been impressed at all your comments on the forums over the years. Always a response that would help someone be successful.

This is by far your best post, this is exactly what the forums were created for, to help other craftsmen and to tease our brains into to thinking that anything is possible.

Thanks for sharing, you have some amazing craftsmen working with you. I realize you absolutely love what your doing, it sure makes it easier when you approach life with that mindset.

Kudos to you and your shop employees, a job well done, can't wait to see the installed pics.

Russ @ Mirror Reflections

4/29/18       #7: Woven Wood Doors, Part V Success! ...
Kevin Dunphy

Website: http://kdunphy.com

Thanks for your time . The doors looks amazing

6/9/18       #8: Woven Wood Doors, Part V Success! ...
Alexander I Hendrick

How is the finish coming? I can't wait to see these installed.

6/11/18       #9: Woven Wood Doors, Part V Success! ...
David R Sochar  Member

They are going in this week. Commercial work. They had to have the doors by end of March. when they could not decide, they moved it to the end of April. When we wanted to deliver them at the end of April, they said they would call us. That happened a week ago.....

Once in, I have to get a clear shot for photos. I think the grand opening is in 2-3 weeks.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory