Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Painted White Oak

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Painted White Oak

7/22/18       
Patrick

I have an upcoming door that is frame and panel that the client wants to be painted flat sawn White oak on the outside and Rift W/O on the inside. Does anyone see any problems when it comes to the panels and how they are laminated ( 4" wide Flat grain outside/4" wide Rift inside glued back to back and then edge glued together). Or should they float seperate from each other and only edge glued together ?
Thank you

7/22/18       #2: Painted White Oak ...
BH Davis  Member

The whole point of quartered and rift oak is to minimize wood movement and shrinkage.

I suspect you know the answer to the question and are hoping some responses here will prove you are wrong !

Unfortunately you are not.....they will move differently enough to cause a problem if glued together back to back.

That is of course if you are referring to the panels. The rails and stiles will be narrow enough that it should be a problem.

You could resaw the plain sawn down to about 1/16" and use it as a face veneer on the rift rear. That would give you a stable panel

If these are going to be painted then what would be the difference in using rift or quartered? I can't see any effect one way or the other. Plus to be honest I don't know if anyone could tell the difference between paint rift and painted plain sawn. The grain will be completely covered and only the pores will protrude through the paint coating.

By the way painting oak is often referred to as pickling......at least one way of painting it. Is that what you are planning? If so then "maybe" you might see a grain difference through the rubbed off paint surfaces.

BH Davis

7/22/18       #3: Painted White Oak ...
Patrick

Thank you BH,
I have had experience with painting only Plain Sawn; I wasn't sure if Rift Sawn is suitable for exterior use. (?)

7/22/18       #4: Painted White Oak ...
BH Davis  Member

Patrick,

White oak is the "original" New England area pressure treated wood so to speak. It is the most rot resistant species around here and in the olden days was used for fence posts and anything else that needed to be in contact with the ground.

The use of kiln dried white oak for an exterior project though could be subject to problems. Your ambient moisture content is going to go back up to around 13% which is a good hike up from a kiln dried content of 7% to 8%. Quartered or rift is going to be relatively stable in movement over typical interior seasonal changes but even that might move too much on its way back up to 13% if used outdoors.

If you go this route don't skimp on the paint quality.......especially the primer coat. Also if you make your own 1/16" veneer cut plain sawn use exterior glues to bond it to the rift layer. Veneer cements don't even do that great indoors.....IMHO.

BH Davis

7/22/18       #5: Painted White Oak ...
rich c.

Are you talking about laminating veneer, or laminating solid wood back to back?

7/22/18       #6: Painted White Oak ...
Patrick

For the panel: solid wood back to back

7/23/18       #7: Painted White Oak ...
rich c.

Flat sawn glued to rift is going to cause trouble.

7/23/18       #8: Painted White Oak ...
Adam

I would tell them that qtr sawn white oak is just about the nicest looking wood on the shelf. It would build the best door aesthetically and structurally.

7/23/18       #9: Painted White Oak ...
Keith Newton

I agree with Adam, plus if it is going to be stained, W Oak can be stained to match any color that R Oak can, plus some. If the color doesn't have any red tone, you don't have to take extra steps to kill the red.

Not to mention White Oak has built in decay and insect resistance missing from R Oak.

7/24/18       #10: Painted White Oak ...
Leo G Member

If the panel is just flat, then glue the center of the two panels with the grain. Then both can move the way they want and be captured at the center. Not sure if you pin panels or space ball them. I pin them with 23ga in the top and bottom center.

7/24/18       #11: Painted White Oak ...
Adam

Leo,

That is is very interesting idea. Never thought of that one. In theory you could do that with any different panels. As long as you only run a vertical bead of glue in the center.

7/24/18       #12: Painted White Oak ...
Leo G Member

Same as I treat a breadboard end on a wide counter. I pin it about 6-8" apart in the center with holes the same size as the pins. Then the rest of the pin holes on the tongue get elongated so they can let the countertop move with the climate.

That way it stays locked to center.

7/24/18       #13: Painted White Oak ...
Adam

I typically use the 23 gauge pinner as well for cabinet doors. Space balls are an annoying time wasting invention. I was referring to actually bonding along the centerline of two seperate panels. They act as one panel but expand independently. It would work well in one of these weird two sided panel interior doors.

7/25/18       #14: Painted White Oak ...
Larry

I used to make exterior doors and used two panels back to back with a sheet of stiff plastic between to isolate the movement differences and the humidity transfer. Also pinned at CL. Recently looked at a door I did over 20 years ago. No cracked panels.

7/26/18       #15: Painted White Oak ...
SteelieMark

What needs to be recognized is that rift and flat sawn sort of move in different directions- flat sawn shrinks and swells mostly in width, rift and quartered shrinks and swells mostly in thickness. Gluing them
back to back may not allow the wood to move as it wants and cupping may be the result.
If the exterior will be painted solid, just make the whole thing from rift sawn, you'll have a seriously good door. But if the exterior will be translucent or 'pickled' (ugh), you'll have to veneer the flatsawn onto the stiles and rails like has been mentioned

8/4/18       #16: Painted White Oak ...
Jay

Patrick, you began this thread with "painted, flat sawn Wht. Oak (ext.) & Clear finished Rift sawn (int.)"

"painted" can mean a lot of different things, and I would like to know more...

if Exterior side is to be solid opaque finish, Id suggest you build this (back to back construction) door entirely of rift sawn Wht Oak.
I suggest Exterior "painted" gets a "full fill" 3k Polyester finish, then switch to an appropriate clear 2k urethane on all surfaces (this is your clear finish for the ibterior, and also a top coat for the polyestervfinished surfaces.

8/4/18       #17: Painted White Oak ...
Jay

For 3k polyesters & 2k urethanes; I've had excellent results with Sherwin products & especially with Sayerlac (which is now carried (owned by?) Sherwin Williams

however there are plenty of other sources as well

good luck with this project, & please post some photos as you build it.

by the way, if your client insists on flat sawn ext. & rift sawn int. you may want to consider a different construction method.
for example:
-full M&T, or Domino joined Stave core (built entirely of the face species). & with minimum 7/16" thickness "skins"
use urea resin (brown glue) or resorcinol throughout & you'd have one helluva door&#128682;

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory