Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Treated Toe Kicks (medical)

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Treated Toe Kicks (medical)

9/12/19       
james e mcgrew  Member

Website: mcgrewwoodwork.com

I have a job where ladder back toe kicks are called for spec and drawings show plywood, (medical) the arch came back after quote and showed treated ply toe kicks under certain sinks only.

in a meeting they are trying to tell me to use 2 x treated on all toe kicks. I have done this once before and the toe kicks did "Move" on that job i had a disclaimer at the bid and we removed 12 elevations and replaced them. with VCP.

I am looking for experience or a disclaimer or a blessing if it so be .

Thanks Jim McGrew


View higher quality, full size image (839 X 891)


View higher quality, full size image (1127 X 863)

9/12/19       #2: Treated Toe Kicks (medical) ...
Josh Koschak Member

Could you use marine grade plywood?

9/12/19       #3: Treated Toe Kicks (medical) ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

thanks that is on the list

9/12/19       #4: Treated Toe Kicks (medical) ...
Alan F.

Pressure treated is pretty typical in California medical facility's that are more than just a Dr.'s office / public works where it is attached to slab on grade because of moisture contact with the kick.

We also have attachment details we need to follow and on many jobs kick installation needs to be inspected to verify it confirms with the details.

The site inspectors don't usually allow any deviation from Architectural connection details.

Private work is not as restrictive.

Some of our jobs are Certified seismic installations that require specific screw and casework connection details as well as inspecting and documenting all backing locations.

We see the firms that do the larger medical facilities use the same details whether its required or not.

We rip a pressure treated 2x6 to a 4" kick with the cut edge up to the box.

A-

9/12/19       #5: Treated Toe Kicks (medical) ...
Leo G Member

What about something like Star Board which is essentially plastic.

9/12/19       #6: Treated Toe Kicks (medical) ...
Adam

What about. Azek type pvc flat stock they use for exterior trim?

9/13/19       #7: Treated Toe Kicks (medical) ...
Tom Gafgen  Member

Website: http://www.TPGCABS.com

What about moisture resistant MDF or Extira ?

9/13/19       #8: Treated Toe Kicks (medical) ...
SG

Became aware of this material a couple of years ago, but have not had call to use it. Kiln-dried, treated yellow pine.

YellaWood

9/13/19       #9: Treated Toe Kicks (medical) ...
pat gilbert

Accoya might be useful for this application.

9/14/19       #10: Treated Toe Kicks (medical) ...
Alan F.

I guess the issue is why is PT material being called out. If the Architect or site is in a flood zone it could be to resist damage if some water gets in the facility.

If the facility has certain cleaning methods that use hoses to clean floors (not likely with rubber base) then the kicks need to be moisture resistant

If the facility uses foot pedals at the sinks then it might be for moisture resistance.

PT 2X lumber is used used in seismic zones to resist uplift in a shaker. It's possible that high wind/hurricane zones could use the same logic.

And it's possible that its a detail out of a can that is either what that firm always does or what they do because of a problem on a prior project.

Deciding on what to substitute depends on why the material is being speciifed.

Seismic zone Map

9/14/19       #11: Treated Toe Kicks (medical) ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

None of the Above, Just a urology lab with welded seam floors.

architect knows i am right but makes her claim that the owner is being this diligent, i am working for the same owner on several other areas of the hospital and i am looking for a way for her to save face. technically the wood movement should be the factor, i have used exteria on wet labs (very we labs) and marine grade ply on others ( twice cost of VCP)

thanks to all but i think each of you has made my point ! again thanks

9/14/19       #12: Treated Toe Kicks (medical) ...
Alan F.

I have a few in the office we use for delivery when the building isn't dried in.

If you notify them of concerns in writing with their design detail and note that their detail is known to fail and proceed per plans and specifications at their direction, the future failure rests on them.

We spent a long time in arbitration once and our only failure was failing to notifiy someone at the executive level of the GC who could authorize the risk in writing of the potential future failure so we were responsible for their legal costs per the contract even though our concerns were in the meeting notes with the GC, ARCH and us and documented.

If a meeting says 2x and plans and specs say plywood we would ask them to modify the specs per a formal document.

The waiver would be something like
Per XXX direction we are proceeding with solid lumber kicks at an additive costs. Owner /architect / GC recognize that this material is known to move, shift contract and expand potentially causing future problems that cause may be difficult or costly to determine fault. Owner / Architect / GC agrees to pay all costs and waive all contract clauses that require us to defend and determine the cause.

Future liability shall be limited to the workmanship that does not meet AWI section xxx.

Any movement that causes damage to any connection to the casework shall be the responsibility of the GC/owner/architect.

Call the GC in advance and the owner if you know them and apologize but tell them you need to send a letter waiving liability and blame your insurance company or lawyer.

9/15/19       #13: Treated Toe Kicks (medical) ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

Thanks Alan and All, I am sending an RFC (clarification this AM, this is a fast track Job and I needed some confirm, I also posted on AWI forum and recieved some helpfull calls as well will follow up.

Jim

9/16/19       #14: Treated Toe Kicks (medical) ...
Alan F.

Moisture related waiver is attached

Click the link below to download the file included with this post.

Release_and_Waiver_of_Claims_Sample.pdf

9/16/19       #15: Treated Toe Kicks (medical) ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

Thanks Alan !

9/22/19       #16: Treated Toe Kicks (medical) ...
ed Member

Hello, I have been making ladder kicks with cabinet plywood . then attach 3/4 x 3/4 " plastic trim at bottom at front and back to provide barrier to moist floors. Just get it at Lowes in 1x4 or 1x6 and rip to 3/4.
Ed

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory