Subject: Re: Hardwood floor thickness for loft...

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Hardwood floor thickness for loft...

3/9/20       
Derek Krzanowski Member

I've been asked to make a custom hardwood floor out of white ash and as close to 6/4 finished thickness as possible as it is for a loft area where they want the underside to look like traditional tonque and groove as it will be visible from below. The reason for the thickness is that the beams are 4' on center and the unsupported distance between beams is roughly 3' 6". I'd love to hear opinions or even better would be an engineers opinion on if that is realistic or not. I've found a ton of formulas for calculating the maximum load however I'd have to go back to school to figure them out.. Lol. My basic test of taking an 18" wide by 4' long by 1-3/8" thick slab and sticking it on 4x4s and jumping on it showed almost no deflection but that is far from a definitive answer... Does anyone have experience or knowledge on this that they'd be willing to share?

3/10/20       #2: Hardwood floor thickness for loft.. ...
james e mcgrew  Member

Website: mcgrewwoodwork.com

I am not an Engineer and never profess to be one, That said get an email from the drawings Engineer to sign off on it directing you to Install as drawn, if something were to go wrong the liability is gonna fall on the responsible party

3/10/20       #3: Hardwood floor thickness for loft.. ...
David R Sochar Member

Use the Sagulator to help predict what will work.

6/4 Ash should dress to 1-1/4", maybe a little thicker. According to my run thru the Sagulator, you will be fine. Assuming a live load of 450 lbs on a 42" x 42" floor....

The Sagulator

3/10/20       #4: Hardwood floor thickness for loft.. ...
Sam

I've built numerous post and beam houses
where we used 1-1/2 native pine T&G for
loft flooring on 4X10 joists 4 foot OC and
never had any owner complain about
springy behavior. 8/4 ash would be way
way stronger - I wouldn't hesitate at all
to use it as you describe.

The complaints I did get had to do with sound and dirt -
every step is heard perfectly
from the floor below, and eventually, dust/dirt
works its way into the T&G joints and when
the low humidity in winter has the flooring
shrunk to its narrowest width, the dirt finds
its way through and onto whatever's below

hope this helps

3/10/20       #5: Hardwood floor thickness for loft.. ...
Rich  Member

Website: http://www.hausmann.com

Are the Beams rated to support living space?

3/10/20       #6: Hardwood floor thickness for loft.. ...
Peter Gagliardi

1 1/4"-1 1/2" is well more than enough. Don't overthink it. 2x6" t&g #2 spruce is used for this all the time at 1 1/2" finish.The Ash is considerably stiffer.
The dirt working thru is a real problem, though the Ash being kiln dried should stay much tighter.

3/11/20       #7: Hardwood floor thickness for loft.. ...
BH Davis  Member

Website: http://www.bhdavis.net

How about a sub-floor first? That could be 4/4 or 5/4 T&G material. Then a layer of the typical laminate flooring 1/16" thick sheet cushioning material and finally a 5/4 or 6/4 top layer of ash flooring. If you ran the ash at 45 degrees to the sub-floor it would be even stronger.

The whole system would look good from below, have plenty of strength, solve the dirt drop issue and be quieter due to the sheet of cushioning material.

BH Davis

3/12/20       #8: Hardwood floor thickness for loft.. ...
Derek Krzanowski Member

Wow, thanks to everyone for all the awesome information! The sagulator is exactly what I needed! I also like the idea of making a subfloor from the same material and running it at a 45 degree angle, I'll mention that to the homeowners and see what they think. Thanks again, much appreciated!

3/12/20       #9: Hardwood floor thickness for loft.. ...
BH Davis  Member

Website: http://www.bhdavis.net

If you are going to run the sub-floor at 45° then take another look at the Sagulator. Your spans are going to be greater so thicker material will likely be in order for the sub-floor.

BH Davis

3/13/20       #10: Hardwood floor thickness for loft.. ...
Derek Krzanowski Member

BH Davis, good point, thanks!

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!