Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Table legs glue up for turning.

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Table legs glue up for turning.

4/29/20       
Scott

I am building some table legs for some tables, the legs are going to end up about 8” diameter once finished on the lathe.

My plan is to glue up maple stock to create the blanks. I am planning on using some stock that I have laying around, most is 4/4, some 6/4. Some of the stock are narrower boards, only 5 inches wide so I am planning to have a few ljoints that will be in the center or close to the center.

I have though this through in my head and I don’t see any issues, however I am not an expert at wood turning so was wondering if anyone else sees any issues.

Thanks and I hope everyone is staying safe out there.

4/29/20       #2: Table legs glue up for turning. ...
David R Sochar Member

Solid? If so, they are likely to develop cracks. You would do better if they were hollow, hexagonal or octagonal. They will also be lighter.

The 6/4 may work if your cuts /design is not too deep.

Draw in section longitudinally to see what thickness is needed.

4/30/20       #3: Table legs glue up for turning. ...
Scott

David,
I will try upload a picture of my end goal.
Thanks for the info.

4/30/20       #4: Table legs glue up for turning. ...
David R Sochar Member

Most certainly build hollow, or else it may crack. You could break the turning into 3 components - top, middle and bottom. The top and bottom (8/4 x 8.5" x 8.5"?) would be turned on the faceplate, and the vase shape would be tapered hollow hexagonal, spindle turned.

If you just want to gang up lumber and glue, it will split in time. Of course, turning will be slow since it will be off center no matter what you do. The splits will happen, probably in several places and fairly soon. Solid is not viable, just not done. Your experience could be different than everyone else's.

4/30/20       #5: Table legs glue up for turning. ...
Tom Gardiner

I was just asked to quote the same table in weathered grey. I would think that a solid glue up of basswood would be more stable and less likely to crack. Turning it wouldn't be as crisp though.

4/30/20       #6: Table legs glue up for turning. ...
rich c.

Lay it up like barrel staves. If you are worried about getting good joints all the way around, glue it up in two halves. Joint each half and do one final glue.

4/30/20       #7: Table legs glue up for turning. ...
TonyF

Basswood may not be as "crisp" as maple in turning, but there is no detail in that leg that calls for "crispness". Possibly the bead, but I think sharp tools would overcome any deficiencies that basswood may present. David makes a good point about assembling three components, you would do well to consider that.

Basswood is available in large thicknesses, is both inexpensive and light in weight, and you will find very few wood species that have less seasonal movement.

Unless you are building a project with a natural clear finish on maple, I would consider using basswood. Glue it, turn it, and go.

Hope this helps.
TonyF

5/2/20       #8: Table legs glue up for turning. ...
Russ

Website: http://www.mr-moulding-knives.com

Here are just a few of the many options we have to support David's reply. Maybe they can give you a few ideas to help you.

All the best
Russ @ MR

https://www.mr-moulding-knives.com/mould

5/2/20       #9: Table legs glue up for turning. ...
Scott

Thanks for the help. I guess the pieces would have to be quite thick if glued up like barrel staves??
David,
Quite often my experiences are different than everyone else’s, but hey, in due time I get over it.

5/2/20       #10: Table legs glue up for turning. ...
rich c.

No the stock would not have to be quite thick. You could taper 1/2" thick stock if you wanted to, it would just take a lot of them!

5/2/20       #11: Table legs glue up for turning. ...
rich c.

Just to clarify. When I said barrel staves, I meant with the grain running vertically. Like using a 2x6 with the width running from the center to the outside diameter.

5/4/20       #12: Table legs glue up for turning. ...
David R Sochar Member

Draw the part in full size, section thru the center. Also, draw the top of the 'cylinder' and the bottom.

I see tapered staves, probably 8/4, six of them. The cap and base are separate, faceplate turned. That is the easy part.

8/9/20       #13: Table legs glue up for turning. ...
Ian

I've done many jobs just like the one you are doing from solid stock. If you have adequate clamping surface are/ pressure it should not be a problem. Titebond 2 works well as long as it's inside


View higher quality, full size image (596 X 794)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!