Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: door wood

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

door wood

1/4/16       
doug mclaren  Member

has anyone experience with red grandis or sipo? how consistent is color ,grain, weight?

1/4/16       #2: door wood ...
Geoff

Our bread and butter is making custom interior doors. Since I have working here we have used pattern mahogany, okume, red maranti (luan), sipo and sapele.

The mahogany was the best all around but too expensive. The okume was brutal on the cutters, it dulled everything. The luan we had a drastic down slide in the quality. The ribbon sipo was good but too hard to find. We are now with sapele and are satisfied. It is easy to get, machines well, and we have not had an issue with movement.

Our shop has humidity control and we can keep the shop between 45% in winter and 55% summer, so we are around 9% EMC. Machined wood is either stored on edge or covered with 1/2" mdf.

1/4/16       #3: door wood ...
B.H. Davis  Member

Website: http://www.curvedmouldings.com

I'll second the suggestion of Sapele. It's our go to wood for exterior projects and we're see more and more requests for in on interior work as well.

Another good choice is Utile. It is similar in color and workability to Sapele but hs a grain pattern a little closer to SA Mahogany.

BH Davis

1/5/16       #4: door wood ...
doug mclaren  Member

the quartered darker sapele doesn't work for many of my customers.

1/5/16       #5: door wood ...
B.H. Davis  Member

Website: http://www.curvedmouldings.com

Quartered Sapele tends to have heavy ribbon stripping. While being quarter sawn it is more stable it is an appearance that many do not like. We specify "plain sawn" when ordering Sapele for this reason unless we have a specific order for a ribbon Sapele project.

BH Davis

1/5/16       #6: door wood ...
Geoff

I would like to point out a couple things. One, utile and sipo are the same wood. Two, I have worked with sipo/utile and sapele (both quarter/ribbon sawn) and it is really hard to tel them apart in appearance.

1/7/16       #7: door wood ...
Leo G  Member

Website: http://www.lrgwood.com

I've had many problems with flat sawn Sapele moving on me. I won't trust it for doors. Quarter sawn is much more stable. It paints well too. For exterior doors I tend to use Spanish Cedar. I hate working with it because of the oils in the wood. Smell and taste terrible. Get on your hands and your face and you need to wipe them down with alcohol to get rid of the oils.

But it makes a very stable door that is very rot resistant. A bit soft.

1/12/16       #8: door wood ...
bill steinkampf  Member

Speaking of door wood....

For several years I've been sitting on some 8/4 x ~16" palo chino/Mexican ebony/Pithecellobium mexicanum planks that I had envisioned for a front door while living in Tucson. Has anyone out there worked with this wood? I've moved it to New Orleans and will ultimately put it into a to-be-built shop. Hope to use it for something other than a casket!

1/21/16       #9: door wood ...
John K Barnes Member

Well, I don't have much idea about it. if anyone has the picture of it, please posted here. It will be of great help.

1/21/16       #10: door wood ...
bill steinkampf  Member

I find that two different species are listed as palo chino: Bursera simaruba and Havardia mexicanum [formerly Pithecellobium mexicanum]. I am familiar with the Bursera from having had garden specimens and observations in Baja California Sur. It's an interesting genus, but I cannot imagine using the wood...similar to cotton wood, but, in my obervation, less usable. It shows up for sale at several sites. The second is what I have. The attached photos are of PC bowls, one unfinished, the other spar varnished. The link is to an informative short article. The planks I have are heavy and the wood, based on a few passes with a hand plane, is fairly hard, similar to mesquite. Unplaned it has a brickish red look.


View higher quality, full size image (2500 X 1875)


View higher quality, full size image (2500 X 1875)

https://www.desertmuseum.org/programs/alamos_trees_havmex.php

2/23/22       #11: door wood ...
Edward Isaac

I hate working with it because of the oils in the wood. Smell and taste terrible. Get on your hands and your face and you need to wipe them down with alcohol to get rid of the oils.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!