Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Solid cherry tops

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Solid cherry tops

3/1/23       
Al

I’m making some some cherry tops to replace existing on some bedroom furniture. The current tops are oak veneer plywood with 1-1/2 bullnose on 3 sides. Instead of matching the 40 year old finish the new tops will be cherry and have a two tone look. Customer likes the idea. The bullnose will be eliminated on new tops and will have a square edge.
I can either go cherry ply with solid edge on 3 sides or solid. To get 1-1/2” I need to bring in cherry and would rather not. I have 1” cherry on hand. 2 tops 22x42 and 1 top 22x84. Can you build up end grain to 1-1/2” by glueing an end grain piece to each side and then mitre fold the front piece? I’m thinking the end grain pieces would be 21-1/4 wide by 4 inches in length. Sometimes looking for trouble isn’t worth it but thought I would ask.
Thanks,
Al

3/1/23       #2: Solid cherry tops ...
Dave Edgerton  Member

Hi Al, we tried to build up an edhe as you are saying and we found it did not look nice. I think thick solid would be great but its a bit wasteful. If it were me i would probably go with the cherry ply (on a particleboard or mdf core not plywood) and then add a 3/16 solid band all the way around. My two cents

3/1/23       #3: Solid cherry tops ...
Al

I was thinking gluing top 8” longer and fall offs would be the build up pieces. So the color on edge would be close. But I know the growth rings won’t line up.

3/1/23       #4: Solid cherry tops ...
duster

Website: http://sunvalleywoodworks.com

Al - I've done quite a few solid wood tops with built up edges in the manner you suggest. I start by gluing up a panel at least 4" wider and longer than the finish size. I try to use the straightest grain boards for the 2 outer edges. After planing and sanding, I rip an equal amount off of both long edges, leaving the panel about 1/4" oversize in width. Then, cut an equal amount off the ends, again about 1/4" oversize. Fold the offcuts against the edge they came from and glue into place. Once the glue is dry, rip an 1/8" off each side and end to clean up the glue line.

I've lots of these in alder, african mahogany, and walnut. The one pictured started out with 5/4 walnut, after all the work I ended up with a 2.25" thick top.


View higher quality, full size image (640 X 480)

3/1/23       #5: Solid cherry tops ...
Al

Duster,
If I understand correctly the front edge is miter folded and then you rip an 1/8” off. So now you don’t have the sharp edge of the miter.

3/1/23       #6: Solid cherry tops ...
duster

Al - I do not do a miter fold. I simply turn the cut off pieces under the edges of the panel, so the both of the sawn edges match. If you use fairly straight grain boards for the edge, this will create the illusion of a panel that's double the thickness. I've shown these to other experienced woodworkers and they couldn't tell.
The end grain is the only giveaway, but you'd have to know what you're looking for.

I've done a lot of dining, console, and end tables with this method. With a lot of the premium wood species going for over $12 a board foot, this is a good way to build up thick tops without breaking the budget.

3/4/23       #7: Solid cherry tops ...
Al

Thanks for the good info. Your tops look great.

3/4/23       #8: Solid cherry tops ...
duster

Thanks Al - here's another one I did in african mahogany with the same method.
I started with 4/4 rough material, I was able to get 1.5" thick for finish.


View higher quality, full size image (640 X 617)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!