Tally Your Lumber!!!!

8/7/14       
JT

This is more a rant than anything but as I prepare to call upper management of a large hardwood distribution company I want to just warn/remind you all to tally inbound lumber. Doesn't matter if it's a large or small order, be sure you are receiving what you are paying for. I have been doing this for well over twenty years and I can count on one hand how many times a tally has gone in our favor, yet we at least once a week contest a tally on a delivery ticket of inbound lumber. Granted must of the time it's not huge but when raw materials make up such a large portion of job cost it can be significant by years end.

The latest phone call to unnamed company was prompted by the fact we noticed grinding marks on what are clearly mill banded units. First thought was they were trying to hide the source of material but soon discovered someone had been removing the mill tally painted on the units....with a grinder!. Of course their tally did not match what we had received, and we busted them again as we just received a unit that had the mill tally poorly painted over and we can read the original numbers. Just so happen to be a unit of walnut so that little twenty five board foot adjustment is fairly significant! Years ago we had another supplier who decided to arbitrarily add 15% to all their tallys for straight line and plane, even if it was in the rough. Needless to say that didn't work for us but think of how many shops probably didn't even know because they don't check.

I am not saying all lumber companies are evil and most discrepancies are probably attributed to sloppy block tallying, You still need to make sure you keep them on the straight and narrow and at the same time help your bottom line.

8/7/14       #2: Tally Your Lumber!!!! ...
red oaks lumber

why haven't you switched suppliers? if they did it more than once on you,shame on you for still buying from them.

8/7/14       #3: Tally Your Lumber!!!! ...
Mark Elliott Member

JT,

Without naming them, although we all wish you would, at least what state do you liven?

Mark

8/8/14       #4: Tally Your Lumber!!!! ...
D Brown

I usually do a quick block tally depending on the quantity and almost always come up very close , the few time there was a real shortage I called my sales rep and let him know he makes the adjustment and issues a credit .
We all have to make sure we understand the rules our suppliers go by as far as net tally , block tally minus 7% for SLR or whatever .

8/8/14       #6: Tally Your Lumber!!!! ...
door shop guy

I wont stand for the shortages they try to get by on me every week!! They usually short me 3-4% and every single time i call and get my credit! It gets old. I even try to short myself by rounding up when i tally and still come up short on footage. All my lumber comes to me in rough so no straitlining. Im in Kansas.

8/9/14       #7: Tally Your Lumber!!!! ...
D Brown

Door shop guy ,

Maybe you should ask them to show you how or who comes up with any given tally.
If this happened to me on a weekly basis I would talk directly to the owners or general manager and ask them why this keeps happening .Usually what happens is they send a bit more than I order and charge accordingly .

8/9/14       #8: Tally Your Lumber!!!! ...
Larry

One of the problems is few shops understand the tally rules so can't do an accurate one. It makes it easy for some "adjustments." Mill tallies tend to be better because the distribution yards keep better track. We do block tally which gives the benefit of doubt to the yard. Not really accurate but ball park.

How many of you do a tally?

8/9/14       #9: Tally Your Lumber!!!! ...
Mark Elliott Member

One of the mills I deal with sends a tally listing the number of boards and the width distribution within each individual unit. I have found it to be accurate. These do come un-opened from the mill.

Of the others I deal with, I've never really had a problem. Knock on wood.

I'm in MI and deal with ITL, Banks Hardwoods and Devereaux primarily.

Mark

8/10/14       #10: Tally Your Lumber!!!! ...
door shop guy

D Brown...I have asked them and got two diffirent answers from the salesman and the rep...Basically they always round up and they might or might not measure each board. But i said i dont pay for air. So its a matter of do they want my business or not?

The more i think about the OP and what is happening to him...I find it very disturbing that a supplier would grind off the tally marks from the mill!! Thats just sick.

Im sort of a large guy...you dont mess with a fat guys lunch.

8/12/14       #11: Tally Your Lumber!!!! ...
D Brown

Door guy , do you have other sources ?
I not a huge guy but I'd make an appointment face to face with them and bring a few boards in and ask them to tally them .

Rounding up is not unusual as long as they are fair about it .

The sales rep will not have a clue of what happens in the warehouse even though he knows in general .

the individual who pulls our order and tallies it is the one to be concerned with the office gets a ticket with a number on it.
We tell our inside salesman what we want and if he does a good job of communicating we get what we ordered .

8/12/14       #12: Tally Your Lumber!!!! ...
JT

Interesting comments. Probably like "door guy", we buy from a lot of suppliers and the one thing I have learned is you need them all at one time or another no matter how bad they are. I can say however, we definitely take the path of least resistance, if my guys have to constantly call and complain about tallys that supplier is headed to the bottom of the call list.

8/28/14       #13: Tally Your Lumber!!!! ...
Verdis Upton  Member

Website: uptonsmillwork.com

Wholesaler dirty little secrets
Gross or net tally how do you buy? To many years in this business I see wholesaler play the game. Quote you a price that seems too good to believe, you buy it. It was sold on a gross tally (12% higher than net). When it comes in you don’t tally it, think you just found you’re new best friend and they give you great deal (not). Bottom line I never in 25 years of planning and milling had a container load short by mill (tally). Before mills started scans tallying they would be long never short on BF. Now dead on.

Most buyers can’t even grade lumber, let alone tally. If it’s not NHLA graded, which are based on the percentage of clear-defect free wood on a board. The measurements of this percentage are referred to as clear-cuttings. Don’t buy it!!!!! Made up grades like northwest hardwood are good for their bottom line not yours. And you have no recourse http://www.nhla.com/assets/1603/rules_card9.pdf. When your material comes in, and has different color ends on it, grade it you may find a blend (FAS 1 face and one common.)

Back to the tallying never trust anyone one. If it is an un-open unit from a mill (still in its 1 ¾” steel bands I would block tally it not hard. Anything less than a full unit by rules needs to be stick not blocked tally. If you buy your lumber in the rough it graded different then surfaced. One more thing if it’s not over the foot mark it’s measured down to the next foot (8’11” is 8 foot not 9 foot). I had a local wholesaler warehouseman try to measure to the inch of length on thick lumber (12/4) then argue with me about it. Just think of all their customers that over paid for their lumber since lumber comes over length by at least an inch.

Your best friend is yourself, teach your employees to not just sign for things. We would write subject to tally and grade inspection.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory