Wood identification

8/28/14       
B.H. Davis  Member

Website: http://www.curvedmouldings.com

In the attached photo the darker/red tone trim board in the rear is what my customer is trying to match. My take was that it was Southern Yellow Pine (I also correctly or incorrectly refer to this as hard pine).

The shorter sample in front is the hard pine cut off I sent him as a sample.

He is of course concerned about the color difference. I do not know if he put any color or finish on the sample I sent but even if he did not it could be hard to get a decent match.

Any thoughts on the original being something other than Southern Yellow Pine?

Thanks,
BH Davis

8/28/14       #2: Wood identification ...
Chris

Website: http://www.trickettwoodoworks.com

B.H. I think you have it right. Does the customers sample have finish on it? If so it might have ambered over time You could stain or tone your work
Good luck Chris

8/28/14       #3: Wood identification ...
B.H. Davis  Member

Website: http://www.curvedmouldings.com

I took a look at an installation of this material from 4 or 5 years ago. It is an interior staircase and it has aged to a more red tone than the sample I sent.

I've suggested the customer put my sample out in the sun and see what happens.

Thanks,
BH Davis

8/28/14       #4: Wood identification ...
David R Sochar Member

Heart Pine. Also called Longleaf Pine. It has the look of SYPine, but is redder and the latewood is very resinous. Think turpentine.

This wood is rare commercially since it was overcut up until the late 30's, but is available reclaimed. Very hard, and good rot resistance. But expensive.

I have used SYPine as a substitute for Longleaf/Heart Pine and it works, but is not as hard (especially the earlywood) and not the same color.

Heart Pine Story

8/28/14       #5: Wood identification ...
SteveG

Hi, this is B.H's customer. The doorway sample is not treated at this time, I took off old paint with a heat gun then an old layer of varnish/stain under that with ZipStrip. By the third ZS pass it scrapped off clean, so that's as pure as the original wood can look.

I'm impressed at how close the lighter part of the old wood is to the darker part of the sample. I'm going to play with some staining options this weekend. For the final treatment of the original stuff I've been using natural stain, which makes the color richer without really darkening, then gloss poly over that.

8/28/14       #6: Wood identification ...
Chris Meyer

Im leaning towards longleaf as well. If you cant get you hands on any a nice piece of doug fir with good heart content could work out for you.

8/28/14       #7: Wood identification ...
Adam

I believe it is SYPine. I layed a 1000 sqft floor 3 years ago. It has a penetrating oil finish on it. The old sample provided is pretty much an exact match.

Its totally normal for the early/late wood to have such a massive contrast in SYPine.

Your sample is not virgin even after you stripped it. The wood could have been layed then UV aged then finished. The stripper takes off the film. The varnish penetrated into the wood which is highlighting the early/late wood.

I really like the look of SYpine. I regard it as the ideal wood shop floor. Cheap, hard and comes in 1x8 flooring.

8/28/14       #8: Wood identification ...
Adam

BH,

I was taught by my wise old woodworking master that:

Its costs an extra 10% if the customer wants to watch, and an extra 50% if they want to help.

Now that we are in this new age of social media. How much do we charge our customers to read and make comments on The Woodweb!

8/28/14       #9: Wood identification ...
B.H. Davis Member

Adam,

I usually want my customers as involved in the project as possible. Since I rarely see any of them face to face this sort of interaction helps develop a trusting relationship.

BH Davis

8/28/14       #10: Wood identification ...
Adam

BH,

I was joking.

However, I have had to use the old line a couple of times when installing some crazy expensive thing and the customer wants to watch for the fun of it.

8/28/14       #11: Wood identification ...
SteveG

I promise to stay away during production! Really though, the impact of having a vendor who invites engagement is huge. What I am looking for is not really reasonable under the circumstances. I need an obsolete pattern cut from a wood that no longer exists in its original form. I think the only chance I had to move ahead was finding someone who loves the craft enough to bulldoze over the obstacles. Its appreciated!

8/29/14       #12: Wood identification ...
Rob

The color looks like Longleaf, awful large growth rings though as compared to to the typical reclaimed old growth.

There are sources for new cut longleaf however. A number of plantations in southwest Ga are harvesting trees, it is surprisingly plentiful. Might be a good happy medium. Here is one supplier I have dealt with:
http://www.redhillslumber.com
Good Luck
Rob

8/31/14       #13: Wood identification ...
Bill Richardson  Member

Website: http://www.awwtx.com

That is definitely longleaf pine.

9/2/14       #14: Wood identification ...
TomO Member

Adam,

You forgot the 3rd part of the equation. It costs the customer 75% more if they already started the project and gave up!

9/2/14       #15: Wood identification ...
mark

Another 100% for longleaf pine. And, as already mentioned, this is second growth material: not old-growth.
In my experience, the term "hard pine" is a muddling of "heart pine", which itself is a muddling of "longleaf pine". I live and work in GA.

9/2/14       #16: Wood identification ...
B.H. Davis  Member

Website: http://www.curvedmouldings.com

Thanks everyone. Project is all set.
BH


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory