I’ve a project I’d appreciate comments/ideas. It’s a prototype; a tree branch 12’ long that will support 930 lbs. It’s essentially an art sculpture that in its final form will be a tree with three branches with ‘leaves’ at the end of the branches.

The core structure is a hollow steel beam 4” x 12” that tapers at 6’ to 4” x 3” the remaining 6’. It is to be covered in wood. Wood choices are Mexican tropical woods, each have interlocked grain.

The environment is in a semi-arid steppe climate, where the temperature during the day can swing from 50 – 105 degrees F, and RH can swing from 32 – 90%.

I’m working from the architect’s specs on the steel beam, the size of which was calculated by a structural engineer. Ultimately, they don’t care for the overall size of the ‘branch’ as they think it’s out of proportion. I’ve played with the ideas of carbon fiber, which I have some limited experience with, and considered a core structure of aluminum constructed with internal ribs as in an airplane wing. For the moment though, the architect wants a prototype on the above steel beam.

My main concern are the swings in temperature and RH. My idea is as follows:
1. Attach 5/8” birch ply to the steel with rivets;
2. Attach 1/4” veneer using West System epoxy. The veneer would have 1/8” gaps.
3. The finish would be a WB impregnated finish as Milesi, Klima or Solrac.

All comments appreciated.

Click the link below to download the file included with this post.

Profile_2.pdf

11/9/14       #2: Wood over steel in a brutal climate ...
Adam

Steel and wood don't mix well. Your current "design" would fail quickly. No movement is allowed because of the rivets.

The steel expands with the heat and the wood shrinks as the heat lowers the moisture.

I would stay away from the steel. What is wrong with making it out of wood? 930 lbs is not that much weight. How is it fastened to the ground? It would be helpful if you gave us a sketch or drawing.

11/9/14       #3: Wood over steel in a brutal climate ...
Craig Caughlan Member

Adam-
Attached is a rendering of the entire tree. I made a mistake on the weight - the total of the hexagonal sections is 2,250 lbs, plus the weight of the two secondary branches. As the architect has it, there would be a steel beam protruding from the trunk that the main branch would slip over.

We've also considered solid wood, laminated, although I'm not sure how the joints would be done. For the moment, the architect wants a prototype of their design.

I've doubts too on the efficacy of how I would cover the steel, which is why I'm throwing it out to WoodWeb. My thinking on the birch ply is that with all the plies it would restrict the movement from the steel heating and expanding. I'd thought of using another type of fastener in an elongated hole, but then I think it would introduce too much 'slop'.

The idea is that this prototype would be placed in the environment for six months to see how it behaves. I'd like to try and get it right the first time. I've told the architect of my doubts.

Click the link below to download the file included with this post.

141009_Mercado.pdf

11/10/14       #4: Wood over steel in a brutal climate ...
Larry

Seems like doing it in just steel would be the best bet. If wood is really required how about making it obvious that it is applied over a steel frame by allowing the steel to show @ the corners (1"+-) and allowing lots of room for the wood to move. Provide large headed stainless steel, through fasteners in slots. This solution makes the construction an integral part of the design. If he doesn't want to stoop to the level of us woodworker's! design ideas, tell him it came from an architect, which I am. But I'm mainly a woodworking business man these days.

11/10/14       #5: Wood over steel in a brutal climate ...
Adam

"My thinking on the birch ply is that with all the plies it would restrict the movement from the steel heating and expanding."

This line of thinking is fatally flawed. The steel may move a bit which you will never be able to control. The bigger problem is the steel is more or less stable and the wood grows and shrinks.

If they are hell bent on making a fake tree out of wood, then its time to forget about the steel. Start thinking of carbon reinforced wood beams. Build up box beams out of western red cedar and skin them with biaxial carbon fiber(45/45 fabric) and epoxy. Apply the 1/4" veneers on top of the carbon. We use cedar as core under glass & carbon in boatbuilding all the time.

Anyone(your engineer) who says their modulus of elasticity(flexibility) are too different fails to understand that the carbon is so stiff that it prevents the wood from ever flexing. They make kayaks with carbon and kevlar which take a huge amount of twisting force. The epoxy resin on every surface stabilizes the wood so it is no longer effected by the humidity.

Another problem to consider is the UV attacking the wood.

Carbon fiber is expensive and you need some experience with it to make it worth your time and money.

Very interesting project.

11/10/14       #6: Wood over steel in a brutal climate ...
Craig Caughlan Member

"My thinking on the birch ply is that with all the plies it would restrict the movement from the steel heating and expanding."

Yeah, that isn't what I meant to say. I know the steel is ± stable. My thoughts were that the birch ply would provide a barrier and stable base for the veneer.

My intuition tells me that CF is the way to go. I've limited experience in laminating plys; 3 x 2mm for a final 1/4" and the result is incredibly strong - more than steel in the bending moment.

I messed up with the weight; we're back to 930 lbs at the 12' end.

Questions:
1. Would a Prepeg Twill weave do?
2. Do you think only one layer of CF between the box beam and the veneer is sufficient, or would I laminate the box beam with CF?

It would appear that this is something that could be bagged pretty easily. at least for the 'branches'.

11/10/14       #7: Wood over steel in a brutal climate ...
Adam

You might be able to build the entire thing out of cedar box beam, then skin it with layers of biax carbon and epoxy(pre preg is only good for sticking to itself not wood). The carbon wrapping the joints wood make it very stiff. After its all cured. Trim the outside with the nice looking stuff.

I have no idea how many layers of carbon. It will be surprisingly stiff over the cedar.

11/10/14       #8: Wood over steel in a brutal climate ...
mark

Really, Larry's got the only good suggestions here. Look at the rendering: it's artistically mechanical, and overtly geometric. Make the structure out of coreten, make the honeycomb out of aluminum, and make the octogonal panels out of ply, plastic, glass, fabric, whatever.
Or, come on: just plant a tree if the point is just mimicry.

11/12/14       #9: Wood over steel in a brutal climate ...
lou

Make it our of steel and have an artist faux finish the wood grain.

11/13/14       #10: Wood over steel in a brutal climate ...
Brad Member

Maybe I'm missing something here... If you slotted the holes where plywood meets steel to allow movement between steel and wood, AND built is so that no plane is dependent on the other, why would this not work? No you would not have a tight joint between surfaces, but you mention a 1/8 gap anyways.

11/14/14       #11: Wood over steel in a brutal climate ...
Craig Caughlan

That was one of my thoughts and the reason the corners on the veneer (in my first drawing) are half lap and not mitre.

We've told the architects we couldn't guarantee, so we're exploring solid, laminated wood, and possibly carbon fiber. Thanks for the input everyone.

11/14/14       #12: Wood over steel in a brutal climate ...
John Costin

This reminds me of some classic jokes, but here goes: To me the biggest problem here is the use of 1/4" "veneer" glued to the plywood (or whatever substrate is used).

1/4" thick wood is lumber in my world, not veneer. By this I mean it behaves more like lumber, because at the glue line the forces from wood movement are ten times greater than the forces from a true veneer face (at around 1/40" thick, which is on the thick side for plywood anyway).

I can't evaluate the ideas about how to make the plywood skins stable because I don't know anything about carbon fiber. But when the 1/4" lumber faces start to move they could shear the glueline no matter what type of adhesive you use and no matter what gaps you use.

(FWIW, aesthetically I like it!)

My $0.02.

John Costin
Veneer Services Unlimited
vsu@gwi.net
207-985-7221
Custom Veneered Components for the Woodworking Industry


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory