GaryE Member

I have to make two large French doors each door is 2 1/4 x 42 x 103. The stiles will be 4 1/2, top rail is 6", and the bottom rail is 9". there will be simulated mullions on both side and one side will be removable the other side will be fixed to framing. stiles and rails will be doweled with 14mm x 140 mm domino's. with a 1/4 safety glass panel. My question is do these specifications seem adequate for the these doors

12/16/14       #2: Large French doors ...
David R Sochar Member

I have no experience with dominoes other than watching them fall. However, you have 4 corners and need all the joint surface you can get.

I would make these with double 1/2" thick tenons, haunched, about 3 to 3-1/2" long, and as wide as I could - 1/2" less that the net rail width, for the haunch. Your top rail would have about 92 square inches of surface area on the tenons at one end, same on the mortises - quite a bit. The lower rail will have about 50% more than that. What do the Dominoes work out to be?

My purist view tells me that 'loose tenons' (misnomer applied to Domino type joinery) have twice the potential for failure. If all the gluing is perfect, then perhaps all is as well as it can be. Do the Dominoes have continuous grain from one end to the other? Or are they a composite wood product?


View higher quality, full size image (1944 X 2592)

12/16/14       #3: Large French doors ...
Joe Calhoon

Should be fine with the Domino XL. We use one for curved and angle joints that are otherwise time-consuming to do with tenons and dowels.

Double tenons would be the strongest but pretty expensive to set up for if you only build a few doors.

If this is exterior be sure to use the Sipo tenons. You could also do a double row of 10 or 12mm thick Dominos.

Dave,
These are well engineered and the fit of the Dominos is very snug and unique with the waffle pattern. I recommend them for starting door builders or shops that do not make a lot of doors.
Joe


View higher quality, full size image (1296 X 968)

12/16/14       #4: Large French doors ...
Gary E

Joe I feel pretty good with the domino's. But after I saw Dave's post I thought the same thing two rows would be better than just the one. These will be interior doors and will be made of poplar finger jointed stave core with poplar outer skins.

Dave I agree that would be the strongest joint . I don't have the machinery to haunch out that would have to be done all by hand.

My main concern is will the 4 1/2 stiles and 6" top rail and 9" bottom rail be enough for this size door

12/17/14       #5: Large French doors ...
David R Sochar Member

I can't answer your question directly since I just don't know the materials.

I do know that I would have no qualms at all sending a 42 x 107 door, with divided light insulated glass (much heavier than a laminated pane) out into the world with the double tenons as I described. Overkill though it may be, I have never had a joint failure.

Also, the equipment I used 25 years ago to produce double tenons was a table saw, a mid-size shaper, a hollow chisel mortiser and a router. Fairly basic stuff, just used in somewhat different ways. Today, we can set up and make a double mortise and tenon in less than 15 minutes. Not as fast as I'd like, but certainly adequate for the 2-3 doors like that we do in a year. And I bet lunch (at a moderately -priced establishment) it is faster than the Domino set-up unless the machine is rigged as dedicated to that particular joint.

12/17/14       #6: Large French doors ...
Gary E

Dave- I will give it a try I'm sure I can figure it out. It looks like there are two panel grooves on you stile and rail what is that for. Is there two panels with an air space between?

12/17/14       #7: Large French doors ...
David R Sochar Member

That photo/joint is from a door that had a complex 4" wide bolection molding on both sides, so the grooves are to locate a mock panel ledge for the moldings to register against. They lined up nicely with the tenons and short haunches.

If you have profiled stiles and rails, they can be mitered or coped. I like 1/2" thick tenons, 1/2" apart for doubles on 2-1/4" thick doors. Good practice says 1/3 the thickness should be tenon, and that would dictate 3/8" thick tenons in 2-1/4". No problems with that, I just like the 1/2".

By the way, when you get this set up, make a couple of extra parts in short stock and clean them up for pass-arounds at a prospective job meeting. Nothing will convey your ability better than a well-made mortise and tenon joint. Just make sure the people handling them know to keep fingers out of the way - they can get pinched.

12/25/14       #8: Large French doors ...
Tom Hogan

Website: http://www.oldworldmill.net

My recommendation would be for stile width to be more like 5 1/2 to 6 1/2" wide, top rail matches. Bottom rail 10-11 1/2". Another consideration would be the door lock and hardware might have a wide plate that needs more stile width than 4 1/2" allows to accommodate the width of the hardware mounting plate. This picture shows a set of doors with 6 1/2" stiles and top rail. It might be a little wide because of the applied moulding but with the added weight of the glass and wrought iron on both inside and outside of the doors, the stiles needed to have a pretty good width to help structurally. These doors measure 41" x 113". Hope this helps.


View higher quality, full size image (2048 X 1530)


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory