Old Handrail Joining Hardware

4/1/15       
Leo G

I have a railing that someone has brought to me to tidy up and make whole once again. So I'm squaring up ends, tuning things up and installing new hardware for the joining of the railing parts.

I had to take out some metal bolts that someone cut with a hacksaw, they came out easy with an easy out. They are odd. So I went and got some furniture bolts and drilled the hole and found that there is already metal threads inside.

I have one of the bolts and "nuts" that is whole. Anyone ever seen these, the thread size is odd and doesn't match up to any normal thread size. So I either find some of these or I'll need to tear into the railing to remove the threaded nut so I can stick an modern furniture bolt into them (screw on one end, machine thread on the other).

Here's a few pics.

pictures

4/1/15       #2: Old Handrail Joining Hardware ...
Leo G

Hmm, that didn't work.


View larger image

4/1/15       #3: Old Handrail Joining Hardware ...
Leo G

Guess you need to put it in the picture box not the link...duh...

And another


View larger image

4/1/15       #4: Old Handrail Joining Hardware ...
JT

I have one very similar, came out of the second oldest building in our state, 1878. I believe it was handmade by a local blacksmith, you could literally see the file marks in the grooves of the nuts on the one I have. Probably just really old.

4/1/15       #5: Old Handrail Joining Hardware ...
Leo G

Was informed it was from 1845. I just used a holesaw and cut the nut out of the railing. Put a plug in there with some epoxy. I'll just use the modern hardware to join them.

4/2/15       #6: Old Handrail Joining Hardware ...
David R Sochar Member

I think it was Henry Ford that first standardized threads and thread sizes for interchangeable parts on his auto lines in the 1900's. Prior to that, each machine shop had their standards and "thread chasers" were an important part of every shop.

Seems hard to believe now, but each shop thought that their threads were what set them apart from the others, as an asset.

4/2/15       #7: Old Handrail Joining Hardware ...
Leo G

Well, either way. I had to remove the old hardware that was inside the railings so I could use the modern furniture bolts to join them. Used a 1" holesaw to drill the buried nut out of the railing and then a 1 1/8" holesaw to make a plug. Used West System Epoxy to put everything back together.

This is before I cleaned things up.

The original hole was about 5/16". I bored it out to 3/8" and then put a dowel drilling sleeve into the hole before I used the holesaw. The sleeve guided me down the original hole so I could keep center. I made the plugs and used a 1/4" steel rod to keep them in the original hole at the bottom of the holesaw hole. Then after the epoxy was hard I used a pair of vice grips to spin the steel rod out. Now I have a plug with the holes predrilled in the correct spot.


View larger image

4/3/15       #8: Old Handrail Joining Hardware ...
Jim Baldwin

This is an early handrail bolt of course and specifically invented for the purpose of joining the new butt-jointed handrail. This was part of the emerging practice of curved handrail formation by the "tangent method" which provided patterns for butt joints. This method replaced the former cylindrical and geometric methods where plumb joints were the common practice. The rail bolt was a technological breakthrough then and remains (in various forms) the best means of joining handrail.

An original bolts like yours, usually had a star nut on one end and a square nut on the other. Sometimes with swelled centers which wedged the bolt tight in the hole. The bottom of the railings were slotted for the nuts and a special "chaser" tool levered the star nut tight. The mortice-slot was plugged.

The proper method of dis-assembly would have involved removing the rectangular plug to access the star nut and knocking it loose with a punch. Usually there are dowels which break.

Looks like you're doing a good job. I receive parts like this on occasion which must be replicated and it's always interesting to see how things went together and how well things were usually done.

4/3/15       #9: Old Handrail Joining Hardware ...
Leo G

I only found 2 joints with the square nut. The other 2 had the star nuts on both sides.

Today I put the new furniture bolts and holes in the railings. The tangent twist to straight 90 was the toughest. I put the bolt in the tangent and the hole in the flat curve.

The whole railing system is as follows. A 2' and 6' section that was hacked at the joint this is the section that travels up the stairs. I ended up taking out 7/8" of material and will have to put the section back together with reclaimed mahogany. I'll glue this solid into an 8' section. Then a 4' section that joins to the 8' section. The 4' section ends with the 90 degree tangent to the left. It joins with a flat 90 degree section that goes flat so that it swings back 180 degrees. It ends on a square joint that mates with another flat 90 that is about 4' long and terminates to the wall.


View larger image

4/3/15       #10: Old Handrail Joining Hardware ...
Leo G

Pix


View larger image

4/3/15       #11: Old Handrail Joining Hardware ...
Leo G

Pix


View larger image

4/3/15       #12: Old Handrail Joining Hardware ...
Leo G

Pix


View larger image

4/3/15       #13: Old Handrail Joining Hardware ...
Leo G

Some of the joints will need sanding it. Not sure if they were never the same or they have swelled of time. The owner will be stripping everything down and new stain and finish will be applied. I'm just waiting for him to send me some reclaimed mahogany so I can make that joint in the 2' and 6' section. After that he can pick it up and have all the fun of installing it.

Oh, I guess I have to make the hole plugs too.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory