Floating Bartop Construction

1/9/19       
Ron Member

I have been asked to bid on a "floating" or "cantilevered" bartop in a cocktail lounge. This is part of a larger cabinetry job. I have no experience with bar tops. I don't want to sub because I'm getting more commercial bar/lounge/restaurant work.

The proposed 18' long x approx. 15" depth bar is to be installed across a few tall windows in a historic brick building, second floor, overlooking Main St. It will be likely be supported by custom fabricated architectural brackets lagged screwed into the brick wall. All cabinets and millwork will be Mahogany and finished in Red Mahogany.

My question(s) is the construction of the bar top. Initial thoughts are laminating 2pcs 3/4" Mahogany plywood into two separate 9" sections with a scarf joints where necessary on the top lamination. Maybe a 5" backsplash and hardwood edging for easy cleanup.

Would it make sense to prefinish offsite and join them onsite and maybe use some kind of decorative seam cover?

If I joined them onsite, I would think it's necessary to finish onsite as well to cover the seam. This could be an issue as this location and the first floor is active.

Finally, as far as finish, most of the bar top finish postings are older and technology has changed. Barrier coat? 2K Poly? Epoxy? Over the stained red Mahogany.

Thanks in advance

1/9/19       #2: Floating Bartop Construction ...
Paul Miller

Website: http://MCCWOODWORKING.COM

There are so many unknowns in your post that it is difficult to give an opinion. But, there is no way I would do a bar top in plywood or veneer. I would use only hardwood.

18' is not really a big deal. You should be able to get that into the space in one piece and do the fabrication and finish in your shop. Even if you have to have someone with a Boom truck raise it up and bring it in through a window, this would be better and cheaper that finishing on site. I have taken long pieces up through the stairway. It takes a few guys and just pass it up.

I would do a test drilling for the anchoring of the supports into old grout. I did some work at an old historic barn and the grout there just crumbled when we touched it with a drill.

Anyway, this really does sound like a fun job, You might have to have some steel supports fabricated and powder coated. People will be leaning on the bar. This could and probably will be a focal point.

Good luck.

1/9/19       #3: Floating Bartop Construction ...
rich c.

The design, construction, and installation of the bar is not spelled out by a designer or architect? I agree with Paul Miller's comments. Old brick can be a disaster. Drill in a hole for a red head anchor and you can get everything from it not holding, to broken brick. Bar tops can stay wet for long periods, and then be sanitized with any number of products. Plywood won't last, and any seams will also be a disaster with liquids seeping in to them. I have no personal experience with the finish schedule, but I do have bar attendance experience.

1/9/19       #4: Floating Bartop Construction ...
Larry

I also agree with Paul Millers comments. No way would I do plywood. We only build a few bar tops a year. Always in laminated solids, avoid seams at all cost. Always prefinished, top/bottom, usually with epoxy.
Attaching to old brickwork. As stated before, much of the interior brickwork is very poor and attaching to it may require experience beyond what most cabinet makers have. The epoxy sleeves sold for hanging pipes are pretty effective.

1/9/19       #5: Floating Bartop Construction ...
TonyF

Ron:

In addition to agreeing with Paul Miller about a one piece bar out of solid wood, I would also add that since installation of steel supports on masonry is not really in the cabinetmakers realm, that whoever the general contractor is should furnish and install any supports for the bar, fabricated in such a way that your installation is only to place the bar on the supports, and secure the bar to the supports. No sense taking on more liability than you need to, and it would be one less thing to worry about. Old brick is a bitch.

As Larry suggested, definitely solid wood, laminated pieces into one continuous length, with an epoxy finish. Don't forget the underside of the bar. I'm sure your finish supplier will set you up with the necessary "space age" materials and a finish schedule. What I have done in the past for drip rails is a Corian drip rail/edge, screwed to the bottom of the bar with a continuous piece of metal under the Corian where the screws are, so that the Corian does not snap off at the screws. I don't think the health inspector would question that, but a small bead of silicone may be needed to seal the drip rail/bar seam, in order to make the inspector happy.

The first floor may be active, but it is probably not active 24/7, so that delivery, if the bar can go in that way, can be arranged during off hours.

You will probably regret using plywood and playing with field seams. You will definitely regret field finishing of a bar.

Hope this helps. Good luck.
TonyF

1/9/19       #6: Floating Bartop Construction ...
Ron Member

Thanks a bunch guys! Very helpful and insightful. I will rethink these issues before proceeding with this part of the bid.

1/10/19       #7: Floating Bartop Construction ...
HarryProdigy Member

Thanks for the valuable tips, fellas! Would definitely take note of these.

1/10/19       #8: Floating Bartop Construction ...
the google

we do this type of work.

18' long is likely too long to get into the building as one piece (especially on the second floor). a simple butt-joint with mechanical fasteners (draw bolts) should be adequate. i'd suggest putting both pieces together in your shop and level sanding the joint before taking it apart to finish and reassemble. you can achieve a very nice joint this way and it beats finding 19'-20' sticks of lumber.

finish-wise, epoxy, depending on the brand, can be tricky to work with and scratch easily. we spray 2k poly (with the proper protective equipment for our finisher) and i would recommend this for this application. it is expensive vs. other cabinet finishes but performs very well for this type of application. you'll need to coat all sides equally in order to balance the piece.

we do this work for other shops around the country so send me a message if you decide to sub it out. tops like this are pretty straightforward but there are advantages to sending this work to a shop that specializes in this work.

good luck.

1/11/19       #9: Floating Bartop Construction ...
David R Sochar Member

Time for a little field research.

Rich - I'll meet you at the bar. Everyone else is encouraged to join us. I've got the first round.

We should be able to reach a consensus before too long, eh?

1/12/19       #10: Floating Bartop Construction ...
rich c.

Not too soon I hope!


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory