Need Help With T&G Pattern Gate

4/25/19       
loringdesign Member

Hello All, I am hoping I could get some input as to best way to fabricate the paneled chevron-like pattern part of this gate. it is a 3'x7' split door. set in a entry courtyard wall. Location is the hills of Los Angeles where i estimated the MC will be .08 - .14 on average. I took a stab at predicting the max expansion in the multi directions and from what i read in the the knowledge Base here thought the 2.25" should be T&G on all three sides and only glued in small sections to keep the little pieces intact. Could be way off here..
Very fortunate to have access to Spessart quarter sawn oak. the styles and rails mills to 1-7/8" x 5" and the t&g will be 7/8"x 2-1/4". I read up on stave core, ladder core which sounded like it may be more solid but i would have to rip the paneling too thin unless i laminated the S&Rs thicker and trying to stay in the solid lumber mode. Also since the doors are really only 36" x 42" thought the 1-7/8" with tenon joints would hold up well. all pieces will be sealed before putting together and both top and bottom will have copper caps for the rainy season.
i have some finish cabinetry experience but little knowledge and although i did a fair amount of research here and elsewhere some of the terminology is new as im sure some of you may find obvious. Any corrections or suggestions would be greatly appreciated. should be able to read the sketch if zoomed in.
thanks

Click the link below to download the file included with this post.

Gate_Details.pdf

4/25/19       #3: Need Help With T&G Pattern Gate ...
Keith Newton

I'm afraid that if I understand you correctly, that when the wind blows causing the gate to slam, that all those parts will be laying in a pile on the ground behind it.

I'd be tempted to re-saw your face lumber down to 1/16" veneer, make up your parquetry, then glue it on both sides of a weather proof substrate with epoxy.

If you do this, you could deepen your groove, and bond the panel in with thickened epoxy to strengthen everything else. I don't think much of dowel joints, and would do M&T instead.

4/26/19       #4: Need Help With T&G Pattern Gate ...
loringdesign Member

i appreciate the input and will pursue the approach you suggest. I do have 2 follow up questions:
1) is milling the 2.25" material down to 1/16" to reduce expan/contrac of would it be ok to go with 1/4" thickness?
Im not familiar with the epoxy glue , do you have any more info or a brand?
thank you much

4/29/19       #6: Need Help With T&G Pattern Gate ...
David R Sochar Member

Mr Newton offers good advice, and his solution is one way. A good way.

Another good way is to builds a ladder core with additional horizontal rails. They can be narrow. The ladder core should be mortise and tenon. Then mill all your parts to a tongue and groove pattern on sides and ends. Make up your face onto the ladder core, leaving a small gap between each piece. About .030". Glue and clamp the parts. You don't need to slather on the glue, nor do you need to be skimpy and worry about which piece will move where. The gap you leave is for each part to expand and shrink.

Both methods will work. I would go with the one that most closely matches your experience.

What is a 'split' door?

5/1/19       #7: Need Help With T&G Pattern Gate ...
Cajun Craftsman Member

I've had great success with this glue on boats. It's not cheap, but you don't need much to create a good bond, yet it allows for wood movement. It is great for oily woods and requires no need to wipe them down with solvent before applying the adhesive. Smith's also has a "MultiWoodPrime" for sealing the wood before applying a finish. http://www.multiwoodprime.com/cart/about.html


View larger image

Smith's Oak & Teak Glue

5/1/19       #8: Need Help With T&G Pattern Gate ...
loringdesign Member

To David R Sochar:
thank you for your comments
Ive reattached the drawing of my project for reference. By "split door" im referring to a dutch door where a full size door is cut in half horizontally. My original message has two attached files but only the reference image of the door used as wall art is open in the message. this might be confusing and some reviewers may not click the link of the cad drawing as a pdf file.
Is the approach you suggest using a ladder core still applicable with the stile/rail frame design i am attempting?

Click the link below to download the file included with this post.

Gate_Details_2.pdf

5/3/19       #9: Need Help With T&G Pattern Gate ...
David R Sochar Member

Well, that is a bit different. Ladder core makes thickness of about 2-1/4" - too thick for a gate panel.
So.... You could do the 3/16" solid, then a stable core and more 3/16" on the other side, and then you have it. Just bond the whole thing to the core, in a vacuum bag or similar.
Or.... do it with solids that have a tight T&G fit. Tap, hammer and bang the parts - 3/4" thick for sake of conversation - together. Leave about .030" at the bottom of the groove to the tongue when in place. Or use v-joint, drive it tight, and let its designed in 'crush zone' do it for you. Once the panel is made up, set it into a plow in the frame with a bead of glue, and you have it .

5/3/19       #10: Need Help With T&G Pattern Gate ...
loringdesign Member

what do you think about using 1" thick Extira as a core and epoxy both sides with 1/4" oak stock. then set it as a panel in the stile/rail frame but not glue the panel to the frame for movement with should be minimal

5/8/19       #11: Need Help With T&G Pattern Gate ...
Keith Newton

You need to give up the idea that making the face thicker is somehow better. If you make it too thick, seasonal change will make it stronger than the glueline. Thinner than about 1/10" allows the epoxy to prevent the expansion and contraction. Extira should be fine as a substrate.

5/10/19       #12: Need Help With T&G Pattern Gate ...
loringdesign Member

Got it. thank you very much


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory