Trouble with Torsion box door

1/18/20       
Gary

I am building some 7' X 10' X 1-3/4" flush doors using a torsion box design. 1-1/4" wide X 3/4" poplar grid with 1/4" MDF epoxied to each side. Building them on dead flat stable table. I can't press them due to their size so I am stacking about 1,000 lbs of 8/4 lumber all over and waiting 24 hrs to cure. Huge bow at the stile/edges when I remove from the table. I would have preferred to make them 2-1/4" but that wasn't an option. Other than thickness does anyone see any immediate red flags ?
Thank you

1/18/20       #2: Trouble with Torsion box door ...
BH Davis  Member

Website: http://www.bhdavis.net

The problem is the poplar grid work. Use maple instead and I think the problem will go away.

BH Davis

1/18/20       #3: Trouble with Torsion box door ...
SG

I built a number of large (up to 5.5' x 10') torsion box doors a few years back and used Baltic Birch for the grid and Okoume for the skins and they did very well, but they were also 2.25" thick. The BB grid was less stiff than I would have liked, but they were pocket doors, so it wasn't a structural concern. I question that you'd get any solid wood to lie flat enough, esp. at your 1.75" thickness - that was my primary impetus for going to plywood.

1/18/20       #4: Trouble with Torsion box door ...
Adam

Yea. What that guy said

It amazes me that people try to use poplar for projects that require stability. Poplar is renowned for being unstable. It warps, it twists. Other than interior trim, occasional face frames. Maybe a couple of cabinet doors if you ran out of soft maple.

1/19/20       #5: Trouble with Torsion box door ...
David R Sochar Member

Change the gridwork species as noted. Decrease its thickness so the weight does not become an issue. 1/2" or 3/8" is fine. Increase to 2-1/4".

Epoxy does not require lots of (any?) pressure. Placing one piece on top of another bonds as well as clamping the bejeezus out of the two parts. I think the MDF is OK

Now for the quiz:

Are you able to pin/staple thru the MDF into the grid?

How much is "huge bow at stile and edged..." 1/2"? 3"?

Is the bow across the width or length or both - bowl like?

Were all the materials stored in the same shop, same environment for a week or more before using?

Has the structure changed over time? How much in how long? If it still exists, that is.

1/19/20       #6: Trouble with Torsion box door ...
D Brown

To all of you torsion box builders, to me the boxes are similar to a hollow core door, I was taught to cut an air relief somewhere on the frame under the skins .Not sure if this has anything to do with the bowing ? Good luck

1/19/20       #7: Trouble with Torsion box door ...
Gary

Thank you David; Here are some answers and some changes I have made:
The bow is about 1/4"-3/8"the length of the stile. The bott & top rails are straight.
I can nail into the grid but did not. I wondered if my half-lap joints might be too snug and introducing a warp & weft to the grid so I made my half-lap sloppy so everything can move around a bit. I also added an LVL to each leading edge. I also changed to a 1/2" plywood grid.
This produced another door with one very straight stile and one stile with an 1/8" bow.
The materials were NOT stored in the same place for a week or more. The first door I made now has about a 1/2" bow in it. I cut it up for the garbage.

1/19/20       #8: Trouble with Torsion box door ...
MarkB Member

My guess is gravity is getting you and the skins are causing the bow especially given the ply core being less but still bowed.

1/20/20       #9: Trouble with Torsion box door ...
David R Sochar Member

Loose lap joints is good. I don't know anything about LVL's, but I would refrain from adding more and disparate materials.

KISS ain't the band, as they say.

Materials coming in from suppliers or other environments put with materials that are shop conditioned will exchange MC to reach an equilibrium. This will cause things to move.

I have seen tight Plastic laminate seams open to .090" when put onto particle board, The P L came in a truck from an unheated warehouse (high MC), and the PB was shop conditioned, had been in there for a month or more (lower MC than the P Lam).

1/20/20       #10: Trouble with Torsion box door ...
Adam

Is your dead flat table still flat after loading the 1000lbs of wood on top?

1/20/20       #11: Trouble with Torsion box door ...
Keith Newton

Virtually any shop vac will pull -2 psi, or 288# psf, As has already been pointed out, epoxy doesn't need a lot of pressure, only that both sides meet. But just in case your interested, your door would have 20,160 perfectly even pounds of pressure from all sides.
Any clear plastic sheeting can be turned into a vacuum bag with nothing more than a $3 tube of Butyl caulk.

Epoxy doesn't contain any water to change the MC of the wood.. If your shop is somewhere that is cool now, you can take as long as you like spreading epoxy and putting it all together, getting the bag sealed, then pull the vacuum and turn on the heat to get it to cure.

1/31/20       #12: Trouble with Torsion box door ...
anthony

I designed some tortion panels awhile back for a tall cabinet project, the sides had to be 16' tall and 3" thick. your grid material should be 3/4" 9 ply or greater straight as hell and standing on edge. cut notchs so your grid members can overlap each other and fit tightly together. the grid cannot be attached to the face in any way as in nails or anything during the glueing process. the grid has to be able to float while its drying. if your unable to pull it off or require ultra lite panels you can always use the company called sing core and have the made to spec


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory
    Sponsors

    Become a Sponsor today!