Chad  Member

Website: http://www.adamsarch.com

We have been resistant at building double doors over the years due to the gap that often forms between the door & astragal of the semi-active door.

This issue is made worse by the fact that we fabricate our doors at 2-1/4" thick, while most thresholds on the market are designed for 1-3/4" doors. We’ve experimented with adjusting the door position within the jamb—both forward and backward—but none of these adjustments have resolved the problem. We've even attempted to modify Pemko’s wood-top aluminum adjustable thresholds by adding wood to the interior side, but the results have been inconsistent.

Has anyone found an effective way to reduce or eliminate this gap between double doors, particularly at the threshold? We’d appreciate any insights or solutions.

Thanks,
Chad

6/2/25       #3: Gap between double doors and the th ...
Leo G Member

Make your own threshold designed for 2 1/4"

6/3/25       #4: Gap between double doors and the th ...
Chad  Member

Website: http://www.adamsarch.com

I have thought about it. We can make a wood threshold but it is not adjustable and they get beat up from walking over it. Maybe I just need your feedback to keep moving forward on finding an aluminum extruder to fabricate one for me. This could be side hustle. Thanks - Chad

6/3/25       #5: Gap between double doors and the th ...
Leo G Member

Are you using White Oak for the thresholds? They hold up much better than Red Oak.

Maybe talk with Pemko, they may have a solution for you.

The 142 series is a hook type waterproofing method and it work well. I've never used this threshold but I have installed a similar smaller brass threshold on top of my white oak sill that hooks in to prevent water and air infiltration.

Pemko Threshold.

6/12/25       #6: Gap between double doors and the th ...
Monica Chou Member

Website: https://www.zonledoors.com/

We’ve faced a similar challenge with thicker doors. One solution that worked for us was custom-fabricating a wider astragal combined with a modified threshold ramp to match the 2-1/4" thickness. It required some precise milling, but it helped minimize the gap without compromising function. Also, consider using magnetic or brush seals on the meeting edge as an additional barrier. Hope this helps!

6/22/25       #7: Gap between double doors and the th ...
David R Sochar

Chad - We resolved this several years ago as we moved primarily to 2-1/4" doors. One could write a book....
I feel we discussed this over the years, with your resistance to relying upon craft, hoping for a kerf in, cut to length fix. Understandable, but not available. My solutions are workable, but not easy. They rely upon top materials and skilled execution.

Please do not use 'head and foot bolts' as made for the mass market. Use good quality (not Chinese) extension bolts as these will work on doors up to 12' or more. Steer away from those gawd awful aluminum sills, especially if you use the mill finish, or worse yet, the brassy ones. Remember, we are trying to make attractive, tasteful objects that often represent the best craft to be found in the house.

If your customer insists on a tinny sounding, dentable and scratchable aluminum sill, then remove the inner hardwood strip and replace it with a wider White Oak Strip. Rebate the inner edge to receive flooring if you like. Make your jig to locate good quality extension bolts so they will throw into the center of the marginal riser on the Pemko sill. T-Astragals can retain 1/2" blades, with the bevel to just under 3/8".

But being woodworkers, I am sure you prefer making your own White Oak sills. We tipped them for a 5 degree slant, with a 2" wide flat at the top, under your paired doors. We used a bronze sill cap on the sill and planned for 1/2" from the meat of the door to the sill. The bronze sill cap was located on the sill to accept the extension bolt. This bore needs to be filed wider to accommodate the seasonal movement of two stiles. Do not just oversize, as it is this point is the start of the whole seal program. We rabbeted the doors leaving 3/8" to cover the gap when the doors were closed (inswing). This left a nice 1/8" reveal between the door bottoms to the sill, same as what was normally seen on the other sides of the door. The gap between the fixed bronze sill cap and the epoxied door bottom was sealed with the brass leaf nailed to the door bottom - later. The bronze sill cap needs a thin bead of silicone full length, both legs at final fitting. Then close the passive door, and locate the brass leaf tight to the sill cap and mark it. This fit is what makes the system draft and wet proof. Take the door down (I know....), and nail the leaf in place, springing it out so when it closes it rubs the top of the sill cap then closes the gap. I often thought of this part as making a door stop for the bottom of the door. And done properly, it works that way.
If after all your efforts, rain still gets in, there is a 1/8" diameter silicone tube that can have a very small bead of silicone run the length, then set into the leaf all the way to make an even more effective seal.
As you can see, some of this can ber done in the shop, and the rest in the field. If your people are setting the doors, you will have no trouble. If others, get drawings and clear instructions and get ready to send out someone to hold hands. You will also find carpenters that modified it all to suit themselves.
This is highly skilled craft with a bit of everything in there - as well as taking large doors down and back up again. Training your people is paramount - support them with tools, carts, space and help so they can do their best every time.
Once a pair is up, with the little fuzzies in place at the center bottom, doors sealed up like this are worth what they cost, and perform very well. Cut any corner, and the whole will be compromised.
And, of course, this is all in my book on Custom Wood Doors. Perhaps you have worn out your copy and need a new one?

9/18/25       #8: Gap between double doors and the th ...
rempredo Member

A solution that often works well in such situations is to use height-adjustable thresholds that have rubber or brush seals. These thresholds can be precisely adjusted to the thickness and position of the door, significantly reducing the gap and preventing drafts. Alternatively, installing draft stop-type seals on the door edges or on the threshold helps fill the free spaces, improving insulation and tightness.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!