Customer claiming termites

11/29/16       
Doug

I would appreciate some opinions on how to deal with this scenario. In 2012 when business was harder to to come by we did some residential work that involved refacing an island and adding three cabinets to the back side. Cabinets were made from import pre-finished maple plywood. The total project might have been $3k. The customer is now telling us that those 3 cabinets have termites in the shelves and sides and the pest control company is saying verbally that they had to have been in the shelves when they were installed as there is no evidence of termites anywhere in the house. The pest control report only states that they found them in the shelves but does not indicate the origin. Customer is asking us to pay the $1000 that they paid to have the island fumigated. While we want to maintain a good name in our community we certainly do not want to give away money because some guy in a white hat and coveralls voiced his opinion but would not put that opinion in writing. How do they or we really know if we are responsible for this? We are concerned that if we pay the $1000 just because we are good people it could set a precedence and open up liability if termites are found other places in the house. Has anyone else had a scenario like this? What would others do?

11/29/16       #2: Customer claiming termites ...
D Brown

Perhaps you should hire your own inspector to go out to the house and take a look for the source if not the cabinets .

11/29/16       #3: Customer claiming termites ...
Jerry Cunningham

There is absolutely no way you are responsible for this. They're trying to be cute and pass the buck along to someone else to take responsibility for their misfortune. Termites are an act of God, tell them to send the bill to him if they want. If your island indeed did have termites it wouldn't have taken 3 years to be noticed.

11/29/16       #4: Customer claiming termites ...
Chris

Termites need an active water source to survive. While it doesn't need to be completely saturated, moisture would have to be present.Plywood would not create a sufficient food source for them to survive 3days let alone 3 years. The glue holding it together would also deter them. It's a very far fetched scam they are pulling here.

11/29/16       #5: Customer claiming termites ...
Gary

Are they sure it is termites? I had a powder post beetle incident years ago. They came out of air dried ash I used for unseen, internal parts of a cabinet. After a little research I learned that the larva were dormant for possibly years in the ash and emerged as beetles when conditions were right. I also learned that they would not reinfest the wood as it was now too dry for their liking and had been finished also. The customer agreed to wait and see and all turned out well.

Your customer may have wasted their money on fumigation.

11/29/16       #6: Customer claiming termites ...
Pete D Member

This came up before in a thread not too long ago, although I think it pertained to 'dry termites'. Prof Wengert added a few comments.

If the client never contacted you before the house was fumigated to discuss the situation and instead made these claims after contracting with the pest company that sounds like complete BS. I'm not familiar with the legal aspects, but I would assume you should be given the right to hire your own expert and get a second opinion.

11/29/16       #7: Customer claiming termites ...
rich c.

As mentioned, it's happened before. http://www.woodweb.com/knowledge_base/Powder_Post_Beetles_in_Plywood.html

If the problem goes away for $1,000, make sure everyone signs a release of further responsibility and that then seems cheap to me.

11/30/16       #8: Customer claiming termites ...
Tim G

I had this happen with some made in china ply that was mistakenly sent to my shop. I was on a deadline and used it for shelves.The culprit was PPB. Supplier admitted it in writing , I replaced the shelves in time, and lucked out as they didn't spread.Lesson learned, no more china ply,period!

11/30/16       #9: Customer claiming termites ...
james e mcgrew

Start by requireing a bonded document for insurance and legal review. probably will stop there. if not the ansers are already in this thread

11/30/16       #10: Customer claiming termites ...
james e mcgrew

"certified bonded document with supporting evidence",, " for your insurance company and legal review" Pest control companies are far more regulated than one would think, a good one will not risk their license or bond any more than we would.

11/30/16       #11: Customer claiming termites ...
Robert Member

Termites are not tax deductible.

11/30/16       #12: Customer claiming termites ...
Alan F.

Whoever imported that material had to file a declaration with customs (plant and product declaration). I seriously doubt the termites in came in with the wood, and skids or crates have to be baked for use in international shipping.

I don't know if a $1,000 argument is worth winning, first thing I would do is call the vendor who supplied the materials and tell them it must have come from them. Let them disprove it, in the end they would be the one of the responsible parties if it went to court (which it won't).

A-

1/1/17       #13: Customer claiming termites ...
Gene Wengert-Wood Doc

There is no way that this has active termites. They need water, as already mentioned.

Further, if it was termite infested, you would have seen it in manufacturing and discarded the wood, etc.

Where are you located? I might be able to suggest a good inspector. As a first step, contact your county extension office, as some have expertise in this area or can arrange for someone.

When you see the damage, also look around for antique furniture that they might have bought recently--last few years. This is a common source of the PPB. It would be nice if all incoming foreign plywood was fumigated properly, but it does not happen. So, it is likely that this has PPB and not termites. Fumigation of a cabinet or one room in a house cannot be done. The gas used in fumigation of wood is highly toxic or poisonous to humans; it kills, even a small amount. So, fumigation involves moving out of the house, putting a tent over the house, gassing for a day or two, and then waiting a day for the gas to leave...this should sound like an expensive operation, and it is. Removal of the offending wood is often more reasonable. The PPB in a dry place is only in hardwoods, and cannot infect wood with a finish, so seldom can spread within the house. Then every 6 onths or so, inspect for any new damage.

4/6/19       #15: Customer claiming termites ...
David Koenig Member

Termites are very harmful insects that can damage the wooden structure within a month and we need to stop them. There are various methods to exterminate termites out of which some are cheaper and others expensive. One of the best way to kill the termites quickly is by hiring some pest exterminator who will do it for you, and they will also be able to show you the best way of eradicating them.

Pest Exterminator


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)